daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Study of Deep Separation of Tungsten from Molybdate Solution AITranslate

School of Metallurgical Science and Engineering, Central South University;School of Metallurgical Science and Engineering, Central South University;School of Metallurgical Science and Engineering, Central South University;School of Metallurgical Science and Engineering, Central South University;School of Metallurgical Science and Engineering, Central South University;School of Metallurgical Science and Engineering, Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Deep separation of tungsten from molybdate solution is a problem in the field of metallurgy.According to the different properties between tungsten compound and molybdenum compound,using the theory and method of molecular design,a new reagent is used to enlarge the differences between tungsten compound and molybdenum compound.A new adsorbent is used to remove tungsten from molybdate solution.After removing tungsten,the ammonium molybdate contained WO3<0.05% is obtained by ion exchange and crystallization fro...

KeyWords AITranslate

molybdate solution Mo/W separation deep removal of impurity separation coefficient

1[1]李洪桂,莫似浩,钟海云,等.有色金属提取手册--稀有高熔点金属(上)[M].北京:冶金工业出版社,1999.118.

2冶金过程强化学科组.“选择性沉淀法从钨酸盐溶液中除钼、砷、锡、锑”专利技术的新进展[J].中国钨业,2000,15(4):29-30. 被引量:7

3肖连生,张启修,龚柏藩,黄芍英.密实移动床——流化床离子交换除钼技术在工业上的应用[J].中国钨业,2001,16(2):26-29. 被引量:21

4霍广生,孙培梅,李洪桂,李运姣,赵中伟,苏鹏抟.离子浮选法从钨酸盐溶液中分离钨钼[J].中国钨业,1999,14(3):35-36. 被引量:12

5范薇,黄普选,姚莉,康定学.氨浸法生产钼酸铵中钨的分离[J].无机盐工业,2001,33(5):3-4. 被引量:8

6吕莹,孙放.Fe(OH)_3吸附法从高钨钼酸钠溶液中分离钨钼的研究[J].稀有金属与硬质合金,2005,33(3):1-3. 被引量:19

7梁起,康定学.MoO_4^(2-)、WO_4^(2-)在Al_2O_3上的吸附与分离[J].河南大学学报:自然科学版,1994,24(2):51-54. 被引量:2

8李洪桂,孙培梅,李运姣,起中伟,苏鹏抟,刘茂盛.选择性沉淀法从钨酸盐溶液中除钼、砷、锑、锡等杂质的研究[J].中国钨业,1998,13(4):17-19. 被引量:19

1张亨.钼酸铵的生产研究综述[J].杭州化工,2012,42(2):11-15. 被引量:3

2张亨.钼酸铵的生产研究进展[J].中国钼业,2013,37(2):49-54. 被引量:5

3张金莲,张要军,黄进献.钼酸铵溶液中两种除钨方法比较研究[J].资源导刊:地球科技版,2015,0(2):60-61.

4杨伟,易建,刘锦锐.超低钾低钨二钼酸铵制备工艺研究[J].福建冶金,2023,52(3):44-47.

1刘燕,李来平,蒋丽娟.钼酸铵制备技术研究现状[J].中国钼业,2018,42(4):1-5. 被引量:3

2王晓亮,沈裕军,彭俊,刘强,周小舟.采用硫酸酸沉法从高硫钼酸铵溶液中回收钼的工艺研究[J].矿冶工程,2018,38(6):124-126. 被引量:3

3徐志昌,张萍.模块化合成化学在制备系列钼酸铵工艺中的应用[J].中国钼业,2019,43(6):38-43. 被引量:2

4李彦龙,李银丽,李守荣,鲁兴武,陈一博,焦晓斌,牛永胜.用钼精矿制备钼酸铵试验研究[J].湿法冶金,2020,39(1):30-33. 被引量:1

5孙聪,郭持皓,余群波.钼焙砂的浸出试验研究[J].中国资源综合利用,2021,39(1):8-10.

6周小舟,沈裕军,彭俊,刘强.采用萃取法从高硫钼酸铵溶液中回收钼的研究[J].稀有金属与硬质合金,2021,49(2):1-4. 被引量:2

7刘蕾.二钼酸铵中钙含量控制的研究[J].四川化工,2022,25(2):17-19.

1肖超,肖连生,曹佐英.从钼酸盐溶液中分离微量钨的机理研究[J].中国钼业,2011,35(2):29-32. 被引量:4

2J.Khler,侯文澜.从钼酸盐溶液中萃取铼[J].湿法冶金,1989(2):52-58.

3郭金亮,马高峰,白宏斌,王伟,李伟,谢亚宁,王子川,冯宝奇.从大量钼酸盐溶液中分离微量钨的研究[J].中国钼业,2012,36(4):32-35. 被引量:1

4刘能生,朱薇,肖连生.从钼酸盐溶液中分离微量钨的研究进展[J].中国钼业,2008,32(2):20-24. 被引量:2

5魏宗武,陈建华,艾光华,刘智林.生物浸出——萃取法分离彩钼铅矿的研究[J].有色矿冶,2007,23(1):22-24. 被引量:4

6梁妹.从废弃炉渣中分离回收钴、镍[J].湿法冶金,2007,26(3):157-162. 被引量:13

7胡健,王学文,肖连生,宋松如.钼酸盐溶液离子交换钼钒分离机理[J].中国有色金属学报,2008,18(E01):112-116. 被引量:2

8唐瑜钟,陈志传,萧作平,童张法.二氯二氨锌的制备及性质[J].有色金属:冶炼部分,2011(8):52-55. 被引量:2

9李运姣,李洪桂,孙培梅,苏鹏抟,赵中伟,霍广生,刘茂盛.选择性沉淀法从钨酸钠溶液中除钼[J].稀有金属,2000,24(5):356-359. 被引量:6

10林江顺,蒋开喜.钴锰渣除杂提钴工艺研究[J].有色金属,2002,54(3):36-38. 被引量:9

Basic Information:

DOI:

Chinese Library Classification Number:TF803.23[冶金工程—有色金属冶金]

Citation Information:

Deep separation of tungsten from molybdate solution is a problem in the field of metallurgy.According to the different properties between tungsten compound and molybdenum compound,using the theory and method of molecular design,a new reagent is used to enlarge the differences between tungsten compound and molybdenum compound.A new adsorbent is used to remove tungsten from molybdate solution.After removing tungsten,the ammonium molybdate contained WO3<0.05% is obtained by ion exchange and crystallization fro...

quote

GB/T 7714-2015 [1] ZHAO Zhong-wei, LI Jiang-tao, CAO Cai-fang, et al. Study of Deep Separation of Tungsten from Molybdate Solution[J]. Rare Metals and Cemented Carbides, 2008(1): 1-4.
MLA [1] ZHAO Zhong-wei, et al., "Study of Deep Separation of Tungsten from Molybdate Solution." Rare Metals and Cemented Carbides, no. 1, 2008, pp. 1-4.
APA [1] ZHAO Zhong-wei, LI Jiang-tao, CAO Cai-fang, HUO Guang-sheng, CHEN Ai-liang, & LI Hong-gui. (2008). Study of Deep Separation of Tungsten from Molybdate Solution. Rare Metals and Cemented Carbides(1), 1-4.
IEEE [1] ZHAO Zhong-wei, LI Jiang-tao, CAO Cai-fang, HUO Guang-sheng, CHEN Ai-liang, and LI Hong-gui, "Study of Deep Separation of Tungsten from Molybdate Solution," Rare Metals and Cemented Carbides, no. 1, pp. 1-4, 2008. keywords: {molybdate solution;Mo/W separation;deep removal of impurity;separation coefficient}