Reaction Process and Mechanism of Scheelite Synthesis with Wolframite and Calcium Carbonate AITranslate
Abstract AITranslate
The reaction process and mechanism were studied of scheelite synthesis by calcination of wolf- ramite and calcium carbonate. The experimental results show that scheelite begins to form during wolframite calcination at 550 ℃. Wolframite and calcium carbonate can be completely synthesized into scheelite at 800 ℃, and the main products are CaWO4, Fe2O3 and Mn2 O3. Scheelite synthesis reaction in air takes place by two steps. The first step is generation of CaWO4, FeO and MnO, and the second step is oxidization of FeO and MnO into Fe2O3 and Mn2O3.
KeyWords AITranslate
1万林生,邓登飞,赵立夫,李红超,徐国钻,梁勇.钨绿色冶炼工艺研究方向和技术进展[J].有色金属科学与工程,2013,4(5):15-18. 被引量:18
2万林生,赵立夫,李红超.崇义章源钨业APT绿色冶炼的技术进步和发展[J].中国钨业,2012,27(1):47-49. 被引量:13
3万林生,徐国钻,严永海,聂华平,赵立夫,肖学有.中国钨冶炼工艺发展历程及技术进步[J].中国钨业,2009,24(5):63-66. 被引量:20
4万林生,赵立夫,黄泽辉,等.一种铵盐分解白钨矿的方法[P].中国专利:102154547B,2013-01-16.
5范树森.钨酸钙的粒度控制及白钨母液中钨的回收[J].稀有金属与硬质合金,1993,21(2):13-16. 被引量:2
6李裕芳,赖道玉.不同颗粒人造白钨的制取[J].中国钨业,1990(11):11-14. 被引量:2
7李自强,何良惠.沉淀白钨的条件分析[J].稀有金属,1987,(4):249-252.
8路辉,谢刚,俞小花,李荣兴.仲钨酸铵结晶母液处理技术研究进展[J].稀有金属与硬质合金,2009,37(4):44-47. 被引量:5
9王学文,王明玉.一种钨钼酸盐混合溶液分离提取钨钼的方法[P].中国专利:101880780B,2012-11-14.
10林晓,刘晨明,曹宏斌.一种含钨结晶母液和含氨蒸汽的资源化综合利用方法[P].中国专利:103253711A,2013-08-21.
1万林生,潘明然,谌勇明,赵立夫,李红超.黑钨矿与碳酸钙人工合成白钨工艺研究[J].稀有金属与硬质合金,2014,42(6):1-3.
2张平,赵珊,苏仕军,孙维义,丁桑岚.碳酸锰热解—酸洗制备高纯化学二氧化锰试验研究[J].湿法冶金,2019,38(3):239-242. 被引量:3
3杨运光,万林生,龚丹丹.粗钨酸钠溶液深度脱磷工业试验研究[J].稀有金属与硬质合金,2019,47(4):1-6. 被引量:3
1甘永兰,李玉婷,莫燕娇,张帆,杨雄强.一种重质二氧化锰的制备方法[J].河南化工,2021,38(1):17-20.
2赖星任,张龙辉,周加坤,张忠堂.钨酸钠浓料铝盐除氟工艺探讨[J].中国冶金,2021,31(4):118-121. 被引量:3
3邹飞,黄春荣,蹇攀,邵学财,穆远慧,刘丰源,兰苑培.中空球形碳酸锰合成及热分解制备MnO_(x)研究[J].矿冶工程,2021,41(4):156-160. 被引量:1
4龚丹丹,李祖怡,张勇,万林生,任嗣利.钨渣回收利用技术研究现状[J].稀有金属与硬质合金,2021,49(6):1-8. 被引量:2
5袁昊,杨康,周铜,彭贺.活性炭负载碳酸锰协同紫外光降解甲苯的研究[J].上海第二工业大学学报,2022,39(2):105-111. 被引量:3
6李祖怡,张勇,郑彬涛,侯志明,龚丹丹.碱分解钨渣硫酸浸出的正交试验研究[J].稀有金属与硬质合金,2023,51(1):1-4.
1万林生,潘明然,谌勇明,赵立夫,李红超.黑钨矿与碳酸钙人工合成白钨工艺研究[J].稀有金属与硬质合金,2014,42(6):1-3.
2刘永生,徐义.等摩尔法制备粗颗粒人工合成白钨[J].中国钨业,1992(12):18-22.
3刘淑清.中钢3^#高炉配有空气冷却的喷煤枪的开发[J].钢铁钒钛,2003,24(2):28-28.
4廖春发,杨文强,王旭,谢泉文,肖志华.由钨酸盐熔盐电解直接制备钨粉的可行性分析[J].有色金属科学与工程,2011,2(4):4-6. 被引量:5
5李裕芳,赖道玉.不同颗粒人造白钨的制取[J].中国钨业,1990(11):11-14. 被引量:2
6廖春发,王坤,王旭,杨少华,房孟钊.NaCl-CaCl_2-CaWO_4熔盐体系电导率的研究[J].有色金属科学与工程,2013,4(5):19-22. 被引量:2
7文小强,王玉香,周健,袁德林,郭春平.熔盐法合成红色荧光粉CaWO_4∶Eu^(3+)及其发光性能的研究[J].中国钨业,2014,29(5):40-44. 被引量:9
8王延玲,张廷安,杨欢,魏世丞.自蔓延高温还原法制备钨粉的研究[J].稀有金属材料与工程,2001,30(4):310-313. 被引量:17
9冶金技术[J].中国学术期刊文摘,2008,14(4):96-98.
10张国辉,樊统云,刘景春.一高炉热风系统空气预热器节能改造[J].冶金动力,2008(2):44-45.
Basic Information:
DOI:
Chinese Library Classification Number:TF841.1[冶金工程—有色金属冶金]
Citation Information:
The reaction process and mechanism were studied of scheelite synthesis by calcination of wolf- ramite and calcium carbonate. The experimental results show that scheelite begins to form during wolframite calcination at 550 ℃. Wolframite and calcium carbonate can be completely synthesized into scheelite at 800 ℃, and the main products are CaWO4, Fe2O3 and Mn2 O3. Scheelite synthesis reaction in air takes place by two steps. The first step is generation of CaWO4, FeO and MnO, and the second step is oxidization of FeO and MnO into Fe2O3 and Mn2O3.
quote
| GB/T 7714-2015 | [1] WAN Lin-sheng, SHU Liu-fei, ZHAO Li-fu, et al. Reaction Process and Mechanism of Scheelite Synthesis with Wolframite and Calcium Carbonate[J]. Rare Metals and Cemented Carbides, 2014(2): 1-4. |
| MLA | [1] WAN Lin-sheng, et al., "Reaction Process and Mechanism of Scheelite Synthesis with Wolframite and Calcium Carbonate." Rare Metals and Cemented Carbides, no. 2, 2014, pp. 1-4. |
| APA | [1] WAN Lin-sheng, SHU Liu-fei, ZHAO Li-fu, CHEN Yong-ming, & LI Hong-chao. (2014). Reaction Process and Mechanism of Scheelite Synthesis with Wolframite and Calcium Carbonate. Rare Metals and Cemented Carbides(2), 1-4. |
| IEEE | [1] WAN Lin-sheng, SHU Liu-fei, ZHAO Li-fu, CHEN Yong-ming, and LI Hong-chao, "Reaction Process and Mechanism of Scheelite Synthesis with Wolframite and Calcium Carbonate," Rare Metals and Cemented Carbides, no. 2, pp. 1-4, 2014. keywords: {wolframite;calcium carbonate;scheelite;calcination;synthesis;reaction mechanism} |