daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Recyclable and Self-Repairable Epoxy Anticorrosion Coatings with Curing-Controlled Thermoplasticity AITranslate

Sun Yat-sen University; Sun Yat-sen University; Sun Yat-sen University; Sun Yat-sen University; Sun Yat-sen University; Sun Yat-sen University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Affordable self-repairing coatings with robust interfacial adhesion are of great interest in anticorrosion applications. Epoxy (EP) coating is the most widely used commercial anticorrosion coating but suffers from failure once damaged because it cannot be repaired facilely as a thermosetting material. Herein, we develop a thermoreversible epoxy by regulating the curing program within a partial curing window of a commercial epoxy–anhydride system. The as-prepared coatings experience a reversible solid–liquid transition during the heating–cooling cycle. The curing windows for thermoplastic and thermosetting epoxy are investigated as well as the underlying curing mechanism. The photothermal coatings were fabricated by embedding carbon nanoparticles (CNPs) within the epoxy coating, enabling in situ repairing by the near-infrared laser irradiation. Such coatings show moderate surface adhesion to metal surfaces, impressive recycling and repairing abilities, and competitive corrosion resistance.

KeyWords AITranslate

thermoplastic epoxy repairable coating photothermal effect solid−liquid transition anticorrosion
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01487

Chinese Library Classification Number:

Citation Information:

Affordable self-repairing coatings with robust interfacial adhesion are of great interest in anticorrosion applications. Epoxy (EP) coating is the most widely used commercial anticorrosion coating but suffers from failure once damaged because it cannot be repaired facilely as a thermosetting material. Herein, we develop a thermoreversible epoxy by regulating the curing program within a partial curing window of a commercial epoxy–anhydride system. The as-prepared coatings experience a reversible solid–liquid transition during the heating–cooling cycle. The curing windows for thermoplastic and thermosetting epoxy are investigated as well as the underlying curing mechanism. The photothermal coatings were fabricated by embedding carbon nanoparticles (CNPs) within the epoxy coating, enabling in situ repairing by the near-infrared laser irradiation. Such coatings show moderate surface adhesion to metal surfaces, impressive recycling and repairing abilities, and competitive corrosion resistance.

quote

GB/T 7714-2015 [1] Ting Shen, Hongxi Zeng, Zhiwei Chen, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01487.
MLA [1] Ting Shen, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01487.
APA [1] Ting Shen, Hongxi Zeng, Zhiwei Chen, ShuRui Zhao, HaoCheng Yang, & Weihua Li. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01487
IEEE [1] Ting Shen, Hongxi Zeng, Zhiwei Chen, ShuRui Zhao, HaoCheng Yang, and Weihua Li, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01487. keywords: {thermoplastic epoxy;repairable coating;photothermal effect;solid−liquid transition;anticorrosion}