Flame-Retardant, Antimicrobial, and UV-Protective Lignin-Based Multilayer Nanocoating AITranslate

Ss. Cyril and Methodius University; Ss. Cyril and Methodius University; University of Belgrade; University of Belgrade; Texas A&M University; Texas A&M University; University of Belgrade; Texas A&M University; Ss. Cyril and Methodius University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Creating multifunctional textiles using chemicals from renewable sources is challenging. In an effort to develop a sustainable and efficient multifunctional cotton treatment, a lignin-based multilayer nanocoating comprising magnesium lignosulfonate, chitosan, and monoammonium phosphate (MAP) was deposited using layer-by-layer assembly. A five bilayer coating adds 15.5 wt % to cotton and imparts fire extinguishing behavior and excellent UV and antimicrobial protection to the fabric. Just a two bilayer coating imparts sufficient self-extinguishing behavior to pass the standard vertical flame test. The combined influence of lignin as a char-forming and UV-protective macromolecule, chitosan as a char-forming biopolymer, and MAP acting as an antimicrobial agent (and a blowing agent and an acid source in an intumescent flame retardant system) results in a very powerful multifunctional textile treatment with very few layers of deposition.

KeyWords AITranslate

cotton layerbylayer assembly lignosulfonate chitosan intumescent monoammonium phosphate
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00520

Chinese Library Classification Number:

Citation Information:

Creating multifunctional textiles using chemicals from renewable sources is challenging. In an effort to develop a sustainable and efficient multifunctional cotton treatment, a lignin-based multilayer nanocoating comprising magnesium lignosulfonate, chitosan, and monoammonium phosphate (MAP) was deposited using layer-by-layer assembly. A five bilayer coating adds 15.5 wt % to cotton and imparts fire extinguishing behavior and excellent UV and antimicrobial protection to the fabric. Just a two bilayer coating imparts sufficient self-extinguishing behavior to pass the standard vertical flame test. The combined influence of lignin as a char-forming and UV-protective macromolecule, chitosan as a char-forming biopolymer, and MAP acting as an antimicrobial agent (and a blowing agent and an acid source in an intumescent flame retardant system) results in a very powerful multifunctional textile treatment with very few layers of deposition.

quote

GB/T 7714-2015 [1] Jovana Petkovska, Nina Mladenovic, Darka Marković, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00520.
MLA [1] Jovana Petkovska, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00520.
APA [1] Jovana Petkovska, Nina Mladenovic, Darka Marković, Marija Radoičić, Natalie A. Vest, Bethany Palen, Maja Radetić, Jaime C. Grunlan, & Igor Jordanov. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00520
IEEE [1] Jovana Petkovska, Nina Mladenovic, Darka Marković, Marija Radoičić, Natalie A. Vest, Bethany Palen, Maja Radetić, Jaime C. Grunlan, and Igor Jordanov, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00520. keywords: {cotton;layerbylayer assembly;lignosulfonate;chitosan;intumescent;monoammonium phosphate}