Non-Covalent Free-Standing Monolayer Nanoarchitectonics of Heterocoronene-Based Discotic Liquid Crystal Molecules Non-Covalent Free-Standing Monolayer Nanoarchitectonics of Heterocoronene-Based Discotic Liquid Crystal Molecules AITranslate

Indian Institute of Technology (IIT) Patna; Indian Institute of Technology (IIT) Patna; Indian Institute of Technology (IIT) Patna; Indian Institute of Technology (IIT) Patna; Indian Institute of Technology (IIT) Patna; Indian Institute of Science Education and Research (IISER) Mohali; Indian Institute of Science Education and Research (IISER) Mohali; Central University of South Bihar; Indian Institute of Technology (IIT) Patna
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

With excellent charge carrier mobility, tendency to form long-range assembly with self-healing ability, and remarkable chemical and mechanical stability, highly conjugated discotic molecules constitute an important class of materials for electronic applications. Here, we report formation of the stable free-standing molecular film of heterocoronene-based discotic liquid crystal (DLC) molecules, held solely by supra-molecular non-covalent interactions. The films of monolayer thickness (∼4 nm) were lifted from Langmuir trough directly onto a circular ring of diameter up to 2 mm as well as onto TEM grids. Films remain free-standing up to a macroscopic length scale, as revealed by optical and secondary electron microscopy, presumably due to the synergistic effect of intermolecular π–π interactions and the dispersion forces between the peripheral alkyl chains as well as their interdigitation. The monolayer is more than 97% transparent in the visible range. Further, resistive switching measurements carried out on the monolayer DLC film transferred on a silver substrate revealed electrochemical metallization to be the governing process. The switching time was found to decrease exponentially with voltage indicating nucleation to be a possible rate-limiting step. We anticipate that the method presented here will facilitate utilization of such non-covalent free-standing films in flexible memristor and nano-electromechanical systems.

KeyWords AITranslate

heterocoronene discotic liquid crystal freestanding monolayer nanoarchitectonics selfassembly resistive switchingShow More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c00225

Chinese Library Classification Number:

Citation Information:

With excellent charge carrier mobility, tendency to form long-range assembly with self-healing ability, and remarkable chemical and mechanical stability, highly conjugated discotic molecules constitute an important class of materials for electronic applications. Here, we report formation of the stable free-standing molecular film of heterocoronene-based discotic liquid crystal (DLC) molecules, held solely by supra-molecular non-covalent interactions. The films of monolayer thickness (∼4 nm) were lifted from Langmuir trough directly onto a circular ring of diameter up to 2 mm as well as onto TEM grids. Films remain free-standing up to a macroscopic length scale, as revealed by optical and secondary electron microscopy, presumably due to the synergistic effect of intermolecular π–π interactions and the dispersion forces between the peripheral alkyl chains as well as their interdigitation. The monolayer is more than 97% transparent in the visible range. Further, resistive switching measurements carried out on the monolayer DLC film transferred on a silver substrate revealed electrochemical metallization to be the governing process. The switching time was found to decrease exponentially with voltage indicating nucleation to be a possible rate-limiting step. We anticipate that the method presented here will facilitate utilization of such non-covalent free-standing films in flexible memristor and nano-electromechanical systems.

quote

GB/T 7714-2015 [1] Nishant Kumar, Anwesha Mahapatra, Himangshu Paul, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00225.
MLA [1] Nishant Kumar, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00225.
APA [1] Nishant Kumar, Anwesha Mahapatra, Himangshu Paul, Priyanka Priyadarshani Samal, Itishree Pradhan, Joydip De, Santanu Kumar Pal, Puneet Mishra, & Alpana Nayak. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00225
IEEE [1] Nishant Kumar, Anwesha Mahapatra, Himangshu Paul, Priyanka Priyadarshani Samal, Itishree Pradhan, Joydip De, Santanu Kumar Pal, Puneet Mishra, and Alpana Nayak, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00225. keywords: {heterocoronene discotic liquid crystal freestanding monolayer nanoarchitectonics selfassembly resistive switchingShow More}