daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Optimization Study of Lanthanum Determination in High-Purity Cerium Oxide by ICP-MSYUAN AITranslate

China Rare Earth Group(Liangshan)Co.,Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

High-purity cerium oxide is widely used in high-end sectors such as electronics and optics.There-fore,the accurate determination of its lanthanum content is essential for ensuring product quality control and improving the efficiency of comprehensive resource utilization.To address the issue of insufficient pre-cision in the determination of lanthanum content in high-purity cerium oxide by inductively coupled plasma mass spectrometry(ICP-MS),this paper systematically analyzes the primary influencing factors,including the complexity of the sample composition,environmental interferences(temperature and relative humidi-ty),and the settings of instrumental parameters(RF power and carrier gas flow rate).Based on this analy-sis,corresponding optimization strategies are proposed:Sample pretreatment using ion exchange chroma-tography or extraction to reduce impurity interference and enrich lanthanum,the application of an environ-mental variable correction model to mitigate the effects of temperature and relative humidity fluctuations on the determination results,controlling the experimental environmental conditions within a temperature range of 20~25℃and relative humidity of 40%~60%,and optimizing the ICP-MS instrument operating parameters with an RF power of 1350~1400 W and a carrier gas flow rate of 0.8~1.0 L/min.Under the optimal conditions(ambient temperature of 20℃,relative humidity of 40%,RF power of 1400 W,and carrier gas flow rate of 1.0 L/min),the detection limit for lanthanum in the high-purity cerium oxide ma-trix solution reaches as low as 0.01μg/L,and the relative standard deviation(RSD)is reduced to 1.65%.This significantly enhances the accuracy and reliability of the measurement results,meeting the require-ments for the precise determination of trace lanthanum in high-purity cerium oxide.

KeyWords AITranslate

high-purity cerium oxide lanthanum content ICP-MS influencing factor pretreatment working parameter accurate measurement
No data

Basic Information:

DOI:

Chinese Library Classification Number:O657.63[理学—分析化学];TQ133.3[理学—化学]

Citation Information:

High-purity cerium oxide is widely used in high-end sectors such as electronics and optics.There-fore,the accurate determination of its lanthanum content is essential for ensuring product quality control and improving the efficiency of comprehensive resource utilization.To address the issue of insufficient pre-cision in the determination of lanthanum content in high-purity cerium oxide by inductively coupled plasma mass spectrometry(ICP-MS),this paper systematically analyzes the primary influencing factors,including the complexity of the sample composition,environmental interferences(temperature and relative humidi-ty),and the settings of instrumental parameters(RF power and carrier gas flow rate).Based on this analy-sis,corresponding optimization strategies are proposed:Sample pretreatment using ion exchange chroma-tography or extraction to reduce impurity interference and enrich lanthanum,the application of an environ-mental variable correction model to mitigate the effects of temperature and relative humidity fluctuations on the determination results,controlling the experimental environmental conditions within a temperature range of 20~25℃and relative humidity of 40%~60%,and optimizing the ICP-MS instrument operating parameters with an RF power of 1350~1400 W and a carrier gas flow rate of 0.8~1.0 L/min.Under the optimal conditions(ambient temperature of 20℃,relative humidity of 40%,RF power of 1400 W,and carrier gas flow rate of 1.0 L/min),the detection limit for lanthanum in the high-purity cerium oxide ma-trix solution reaches as low as 0.01μg/L,and the relative standard deviation(RSD)is reduced to 1.65%.This significantly enhances the accuracy and reliability of the measurement results,meeting the require-ments for the precise determination of trace lanthanum in high-purity cerium oxide.

quote

GB/T 7714-2015 [1] Hong-xia. Optimization Study of Lanthanum Determination in High-Purity Cerium Oxide by ICP-MSYUAN[J]. Rare Metals and Cemented Carbides, 2026(2): 11-15.
MLA [1] Hong-xia. "Optimization Study of Lanthanum Determination in High-Purity Cerium Oxide by ICP-MSYUAN." Rare Metals and Cemented Carbides, no. 2, 2026, pp. 11-15.
APA [1] Hong-xia. (2026). Optimization Study of Lanthanum Determination in High-Purity Cerium Oxide by ICP-MSYUAN. Rare Metals and Cemented Carbides(2), 11-15.
IEEE [1] Hong-xia, "Optimization Study of Lanthanum Determination in High-Purity Cerium Oxide by ICP-MSYUAN," Rare Metals and Cemented Carbides, no. 2, pp. 11-15, 2026. keywords: {high-purity cerium oxide;lanthanum content;ICP-MS;influencing factor;pretreatment;working parameter;accurate measurement}