daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Poly(ethylene oxide)-Based Electrolytes for Solid-State Potassium Metal Batteries with a Prussian Blue Positive Electrode AITranslate

Karlsruhe Institute of Technology (KIT); Skolkovo Institute of Science and Technology; Karlsruhe Institute of Technology (KIT); Karlsruhe Institute of Technology (KIT); Karlsruhe Institute of Technology (KIT); Karlsruhe Institute of Technology (KIT); Skolkovo Institute of Science and Technology; Karlsruhe Institute of Technology (KIT)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Potassium-ion batteries are an emerging post-lithium technology that are considered ecologically and economically benign in terms of raw materials’ abundance and cost. Conventional cell configurations employ flammable liquid electrolytes that impose safety concerns, as well as considerable degrees of irreversible side reactions at the reactive electrode interfaces (especially against potassium metal), resulting in a rapid capacity fade. While being inherently safer, solid polymer electrolytes may present a solution to capacity losses owing to their broad electrochemical stability window. Herein, we present for the first time a stable solid-state potassium battery composed of a potassium metal negative electrode, a Prussian blue analogue K2Fe[Fe(CN)6] positive electrode, and a poly(ethylene oxide)-potassium bis(trifluoromethanesulfonyl)imide polymer electrolyte. At an elevated operating temperature of 55 °C, the solid-state battery achieved a superior capacity retention of 90% over 50 cycles in direct comparison to a conventional carbonate-based liquid electrolyte operated at ambient temperature with a capacity retention of only 66% over the same cycle number interval.

KeyWords AITranslate

potassium battery solid polymer electrolytes SPEs polyethylene oxide PEO KTFSI Prussian blue analogue PBA
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00014

Chinese Library Classification Number:

Citation Information:

Potassium-ion batteries are an emerging post-lithium technology that are considered ecologically and economically benign in terms of raw materials’ abundance and cost. Conventional cell configurations employ flammable liquid electrolytes that impose safety concerns, as well as considerable degrees of irreversible side reactions at the reactive electrode interfaces (especially against potassium metal), resulting in a rapid capacity fade. While being inherently safer, solid polymer electrolytes may present a solution to capacity losses owing to their broad electrochemical stability window. Herein, we present for the first time a stable solid-state potassium battery composed of a potassium metal negative electrode, a Prussian blue analogue K2Fe[Fe(CN)6] positive electrode, and a poly(ethylene oxide)-potassium bis(trifluoromethanesulfonyl)imide polymer electrolyte. At an elevated operating temperature of 55 °C, the solid-state battery achieved a superior capacity retention of 90% over 50 cycles in direct comparison to a conventional carbonate-based liquid electrolyte operated at ambient temperature with a capacity retention of only 66% over the same cycle number interval.

quote

GB/T 7714-2015 [1] Anna D. Khudyshkina, Polina A. Morozova, Andreas J. Butzelaar, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00014.
MLA [1] Anna D. Khudyshkina, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00014.
APA [1] Anna D. Khudyshkina, Polina A. Morozova, Andreas J. Butzelaar, Maxi Hoffmann, Manfred Wilhelm, Patrick Theato, Stanislav S. Fedotov, & Fabian Jeschull. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00014
IEEE [1] Anna D. Khudyshkina, Polina A. Morozova, Andreas J. Butzelaar, Maxi Hoffmann, Manfred Wilhelm, Patrick Theato, Stanislav S. Fedotov, and Fabian Jeschull, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00014. keywords: {potassium battery;solid polymer electrolytes;SPEs;polyethylene oxide;PEO;KTFSI;Prussian blue analogue;PBA}