In view of upstream damming widely used in China metallurgical mines for tailings dam construction, description is made of the cause of tailing formation as well as its special physical and mechanical properties. Analysis is made of the effect of tailing discharge method on the depositing law of tailings dam and the dam structure as well as the effect of tailing discharge concentration/flow velocity/flow capacity/ discharge place on the formation of depositional dam. It is pointed out that during design of upstream tailing damming, the relevant factors should be fully taken into account so as to ensure a well-graded accumulation. And the proper concretion of depositional dam body within a short time is a prerequisite for a stable dam by upstream damming with tailings. The shear strength of depositional body can be improved only by proper arrangement of seepage drainage facility and accelerating dewatering concretion of the depositional body. Two examples are given.
KeyWords AITranslate
1VA范诺尼.泥沙工程[M].孙明漳,译.北京:水利出版社,1981.
2松尾新一郎.土质加固方法手册[M].黄河水利委员会水利科学研究所,译.北京:铁道出版社,1983.
1李识博,代俊芳,吴江伟,肖乐乐.考虑粒组分类影响的最小孔隙比分布及模型验证[J].岩土力学,2022,43(S02):193-204.
2袁维,白冰,李小春,汪海滨.透镜体对尾矿坝安全性影响的参数敏感性分析[J].中南大学学报:自然科学版,2013,44(3):1174-1183. 被引量:12
3孟庭威,武治安.上游法高浓度尾矿库的稳定分析[J].岩土工程技术,2014,28(3):117-120.
4欧孝夺,廖有芳,苏建,潘鑫,李结全.湿堆尾矿双向排水大变形固结计算模型[J].水利水电科技进展,2014,34(5):28-34. 被引量:3
5陶东良,梅聪,陆誉婷.白岩尾矿坝土工席垫排渗措施模拟及渗控效果分析[J].水力发电,2015,41(6):69-72. 被引量:5
6梅聪,沈振中,邵国卫,陆誉婷.尾矿坝土工席垫三维有限元模拟及效果分析[J].水电能源科学,2016,34(1):73-76. 被引量:5
7刘瀚和.上游式尾矿堆积坝外坡坡比设计的探讨[J].有色金属:矿山部分,2016,68(2):91-93. 被引量:1
8李长洪,卜磊,陈龙根.尾矿坝致灾机理研究现状及发展态势[J].工程科学学报,2016,38(8):1039-1049. 被引量:24
9李志平,彭振斌,何忠明,袁维.透镜体影响尾矿坝安全性的规律及其简化方法[J].中南大学学报:自然科学版,2017,48(5):1326-1334. 被引量:2
10唐永俊,王光进,许志发,赵怀刚.尾矿库干滩尾矿粒径的淤积特性研究[J].泥沙研究,2018,43(3):50-56. 被引量:3
1刘道涵,罗士新,陈长敬.高密度电阻率法在丹江口水源区尾矿坝监测中的应用[J].物探与化探,2020,0(1):215-219. 被引量:10
2张文浩,褚衍玉,任高峰,张聪瑞,周可.不同扰动作用下尾矿坝稳定性分析[J].武汉理工大学学报,2019(1):63-69. 被引量:1
3努尔哈斯木.穆哈买提汗,余湘娟,李敏,高磊.新疆某水库坝基砂层透镜体物理力学性质试验研究[J].水利与建筑工程学报,2014,12(3):125-129.
4欧孝夺,苏建,钟一和,吴光航,江杰.逐级堆排尾矿泥浆排水固结规律试验[J].金属矿山,2018,47(11):18-24. 被引量:3
5万露,辛保泉,郭明东,李迪.基于模型相似理论的尾矿库溃坝试验研究[J].矿业研究与开发,2018,38(12):66-71. 被引量:8
6张圣,李同春,周桂云,晁阳.赵家沟尾矿坝稳定安全系数预测研究[J].矿业研究与开发,2019,39(1):72-76. 被引量:2
7史冬梅,杨风暴,王肖霞.尾矿坝风险评估中指标相关性权重的确定[J].金属矿山,2014,43(11):143-146. 被引量:3
8唐葭,邓宗伟,高乾丰,蒋建清.湖相软土动力特性影响因素敏感性分析[J].重庆大学学报:自然科学版,2014,37(8):59-66. 被引量:2
9张钦礼,陈宇,王新民,杨伟,薛希龙.改进突变理论在井下排水方案优选中的应用[J].安全与环境学报,2015,15(3):48-52. 被引量:3
10邓红卫,叶茂,吴彦霖.基于GMS和Slide的透镜体数值模拟和敏感性研究[J].安全与环境学报,2016,16(1):91-94. 被引量:3
1雷云生.上游法尾矿堆积坝工程勘察应注意的几个问题[J].铜业工程,2001(1):53-54.
2李跃强,李瑞鸿.某尾矿库上游法加高扩容方案研究[J].现代矿业,2016,0(10):152-154.
3徐骏.改变浓缩机底流的排放方式[J].选煤技术,1990(5):24-26.
4刘瑞.改变浓缩机底流排放方式的实践[J].选煤技术,1991(4):10-11.
5陶德宁.尾矿堆对环境的长期影响[J].铀矿冶,2007,26(2):89-89.
6张学义,吴冲龙.影响煤矿生产的一种新的地质因素——泥石流[J].阜新矿业学院学报,1989,8(4):49-53. 被引量:1
7郭英杰.排渗设施在尾矿坝设计中的应用[J].工程设计与研究(长沙),1994(4):37-39. 被引量:2
8利用细菌氧化从尾矿堆中回收贱金属[J].有色金属再生与利用,2005(7):41-41.
9何国益,侯文炯.煤层巷道锚杆支护设计探讨[J].陕西煤炭技术,1995(3):28-30.
10张汉泉,付金涛,黄成林,路漫漫,张泽强.新疆某选铜尾矿中铁回收试验[J].中国矿业,2015,24(1):131-134.
Basic Information:
DOI:
Chinese Library Classification Number:TD926.4[矿业工程—选矿]
Citation Information:
In view of upstream damming widely used in China metallurgical mines for tailings dam construction, description is made of the cause of tailing formation as well as its special physical and mechanical properties. Analysis is made of the effect of tailing discharge method on the depositing law of tailings dam and the dam structure as well as the effect of tailing discharge concentration/flow velocity/flow capacity/ discharge place on the formation of depositional dam. It is pointed out that during design of upstream tailing damming, the relevant factors should be fully taken into account so as to ensure a well-graded accumulation. And the proper concretion of depositional dam body within a short time is a prerequisite for a stable dam by upstream damming with tailings. The shear strength of depositional body can be improved only by proper arrangement of seepage drainage facility and accelerating dewatering concretion of the depositional body. Two examples are given.
quote
| GB/T 7714-2015 | [1] YAN Xue-jun. Investigation on the Depositing Law of Tailings Dam by Upstream Damming[J]. Rare Metals and Cemented Carbides, 2008(2): 54-58. |
| MLA | [1] YAN Xue-jun. "Investigation on the Depositing Law of Tailings Dam by Upstream Damming." Rare Metals and Cemented Carbides, no. 2, 2008, pp. 54-58. |
| APA | [1] YAN Xue-jun. (2008). Investigation on the Depositing Law of Tailings Dam by Upstream Damming. Rare Metals and Cemented Carbides(2), 54-58. |
| IEEE | [1] YAN Xue-jun, "Investigation on the Depositing Law of Tailings Dam by Upstream Damming," Rare Metals and Cemented Carbides, no. 2, pp. 54-58, 2008. keywords: {upstream damming with tailings;dam body deposition;depositional dam;dewatering concretion;dam stability} |