Study on Effect of Ce on the Thermoplasticity of Copper-containing Arsenic Steel AITranslate
Abstract AITranslate
The effect of Ce on improving the thermoplasticity of copper-containing arsenic steel was investigated by Gleeble—3800 thermal/force simulation test machine.The results of thermoplastic curve analysis and fracture and microstructure observation show that adding 0.005 8% Ce can reduce the temperature range of the thermoplastic groove of copper-containing arsenic steel, and improve the thermoplasticity of the steel at 957~1 100 ℃ to a certain extent.The addition of 0.005 8%Ce can reduce the temperature to 1 000 ℃ at which the hot tensile fracture of copper-containing arsenic steel is completely transformed into dimple fracture, and at the same time, the temperature at which copper-containing arsenic steel enters the austenite single-phase region can be reduced to 800 ℃.There are no arsenious rare earth inclusions in the copper-containing arsenic steel with 0.005 8%Ce, while the solid solution Ce in the steel segregates prefe-rentially at the grain boundary, reducing the As content at the grain boundary, and thereby improving the thermoplasticity of copper-containing arsenic steel.
KeyWords AITranslate
1陆明希,张浩.国内电炉钢发展现状与应用前景[J].再生资源与循环经济,2012,5(1):37-39. 被引量:4
2李士琦,陈煜,刘润藻,季淑娟.现代电弧炉炼钢技术进展[J].中国冶金,2005,15(6):8-13. 被引量:13
3张胤彦.残余元素对工艺及性能的影响[J].中国金属通报,2021(7):247-248. 被引量:1
4王绚,唐雪萍,杨接明,雷旻.钢中主要杂质元素的特性及影响[J].特钢技术,2011,17(1):13-15. 被引量:17
5贺景春,弓文生,任新建.钢中残余有害元素的影响及其控制[J].包钢科技,2007,33(S2):1-4. 被引量:13
6罗林根,王建军,彭家庆,林银河,陈正宗,李正邦.钢中残余元素铜的去除方法研究现状[J].铸造技术,2015,36(6):1490-1494. 被引量:2
7杜显彬,魏泽华,杜传治,赵培林,方金林.残余元素砷、铜对耐低温热轧型钢表面质量的影响[J].连铸,2017,42(3):34-38. 被引量:6
1曾重阳,黄宏锋,陈元,姜迈,韦莉莉,刘淑辉.室温多向模锻道次对Al-5Mg-0.3Mn合金组织与性能的影响[J].锻压技术,2022,47(5):5-11.
2习小慧,陈柏潼,刘永乐,彭晓柏,王金亮.塑性变形与调质处理耦合作用对40Cr钢锭焊接接头疲劳性能的影响研究[J].广州化工,2022,50(13):156-158. 被引量:2
3马钰,唐海燕,刘颜彬,刘锦文,江野,张家泉.稀土铈对55SiCr高应力弹簧钢夹杂物的改性作用[J].钢铁,2022,57(6):57-71. 被引量:6
4刘明,白佳,王鲁,房璐璐,丁乔峰.某火电机组三连杆恒力弹簧支吊架弹簧拉杆断裂原因[J].机械工程材料,2022,46(3):89-94. 被引量:2
5马江,王峰,薛永盛,李勇.某Q345R钢制压力容器超声测厚异常原因[J].理化检验:物理分册,2022,58(3):31-32.
6梁燕燕,刘少先,杨冬冬.某热镀纯锌卷大锌花和发亮缺陷产生原因及改善措施[J].理化检验:物理分册,2022,58(3):75-78.
7许永春,周杰,沈鹏,孙晓军,张钦莹,朱鹏飞.TC4钛合金高锁螺栓发生异常双剪断裂原因[J].理化检验:物理分册,2022,58(3):66-69.
8汪勇,姜亚雄,郑仁军,刘志斌,高起方,庄世明,王德毛.某高砷微细粒难处理金矿石选冶试验研究[J].黄金,2022,43(7):60-66. 被引量:1
9王之香,南海,张锦文.国产高铁齿轮用材料的韧脆转变温度研究[J].山西冶金,2022,45(3):1-3.
10张特,马绍斌.氧化锌烟尘浸出液加压氧化中和脱砷试验研究[J].有色设备,2022,36(3):23-26.
Basic Information:
DOI:
Chinese Library Classification Number:TG142.33[金属学及工艺—金属材料]
Citation Information:
The effect of Ce on improving the thermoplasticity of copper-containing arsenic steel was investigated by Gleeble—3800 thermal/force simulation test machine.The results of thermoplastic curve analysis and fracture and microstructure observation show that adding 0.005 8% Ce can reduce the temperature range of the thermoplastic groove of copper-containing arsenic steel, and improve the thermoplasticity of the steel at 957~1 100 ℃ to a certain extent.The addition of 0.005 8%Ce can reduce the temperature to 1 000 ℃ at which the hot tensile fracture of copper-containing arsenic steel is completely transformed into dimple fracture, and at the same time, the temperature at which copper-containing arsenic steel enters the austenite single-phase region can be reduced to 800 ℃.There are no arsenious rare earth inclusions in the copper-containing arsenic steel with 0.005 8%Ce, while the solid solution Ce in the steel segregates prefe-rentially at the grain boundary, reducing the As content at the grain boundary, and thereby improving the thermoplasticity of copper-containing arsenic steel.
quote
| GB/T 7714-2015 | [1] CAO Cheng-xiang, LIANG Yu-yu, XIN Wen-bin, et al. Study on Effect of Ce on the Thermoplasticity of Copper-containing Arsenic Steel[J]. Rare Metals and Cemented Carbides, 2022(3): 52-56. |
| MLA | [1] CAO Cheng-xiang, et al., "Study on Effect of Ce on the Thermoplasticity of Copper-containing Arsenic Steel." Rare Metals and Cemented Carbides, no. 3, 2022, pp. 52-56. |
| APA | [1] CAO Cheng-xiang, LIANG Yu-yu, XIN Wen-bin, ZHANG Jing, & MENG Qin-yang. (2022). Study on Effect of Ce on the Thermoplasticity of Copper-containing Arsenic Steel. Rare Metals and Cemented Carbides(3), 52-56. |
| IEEE | [1] CAO Cheng-xiang, LIANG Yu-yu, XIN Wen-bin, ZHANG Jing, and MENG Qin-yang, "Study on Effect of Ce on the Thermoplasticity of Copper-containing Arsenic Steel," Rare Metals and Cemented Carbides, no. 3, pp. 52-56, 2022. keywords: {Ce addition;copper-containing arsenic steel;thermoplasticity;fracture;inclusion;grain boundary segregation} |