daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Influence of Calcination Temperature on Nb_2O_5 Physical Property AITranslate

Zhuzhou Cemented Carbide Factory Tantalum Niobium Division
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Study is made of the variation mechanism of Nb 2O 5,main physical properties,ie grain shape,crystalline structure,average particle size,specific surface area and bulk density under calcination temperature.The law of the variation with the temperature variation is found out.Investigation is made on the reasons for the variation.Analysis is made of the relationship between Nb 2O 5 average particle size,specific surface area and bulk density so that the average particle size and specific surface area can be quickly calculated out by measuring the bulk density.

KeyWords AITranslate

Nb 2O 5 calcination temperaturce physical property

1王肇信.钽铌冶金学[M].稀有金属冶金学会、钽铌冶金专业委员会,1998..

2李树棠.晶体X射线学基础[M].北京:冶金工业出版社,1990..

3株洲硬质合金厂.Nb2O5分析测试方法标准[M].湖南省株洲市:株洲硬质合金厂,1996..

1胡胜利,李辉.影响五氧化二铌粒径因素的研究[J].科技资讯,2007,5(35):233-233. 被引量:1

2晏慧娟.传统工艺制备Nb_2O_5粉末物性指标控制技术浅谈[J].稀有金属与硬质合金,2015,43(3):5-8.

3刘肖,滕曼,蔡亚岐,牟世芬.离子色谱法测定五氧化二铌和五氧化二钽中痕量氟氯和硫酸根离子的前处理方法[J].岩矿测试,2006,25(4):319-322. 被引量:7

4王伟,李辉,郑培生.低品位钽铌原料的湿法冶金新工艺研究[J].稀有金属快报,2008,27(4):31-36. 被引量:10

5曹七林,姚卫东.陶瓷电容器用Nb_2O_5的制备[J].稀有金属与硬质合金,2008,36(3):43-44. 被引量:2

6刘自喜,石金根.Nb_2O_5粒度的工艺控制研究[J].稀有金属与硬质合金,2016,44(4):11-13.

7丁明建,冯毅龙,钟建平,刘福扩.Nb_2O_5陶瓷的电化学注氢研究[J].广州化工,2017,45(15):117-119. 被引量:1

8傅小明,杨在志,孙虎.空气中热分解草酸铌制备多孔结构Nb_2O_5试验研究[J].湿法冶金,2017,36(6):507-510. 被引量:3

9章斐,赵博涵.热重联用技术探析铌酸铵草酸盐水合物分解逸出气二次反应[J].分析仪器,2018(4):154-158. 被引量:1

10刘迪,蔡卫滨,韩雪,李奕,王永刚.直接沉淀法制备五氧化二铌超细粉体[J].无机盐工业,2018,50(7):48-50. 被引量:2

1黄秋硕.高性能氧化铌粉体制备工艺研究[J].冶金管理,2020(15):70-71.

2晏慧娟.传统工艺制备Nb_2O_5粉末物性指标控制技术浅谈[J].稀有金属与硬质合金,2015,43(3):5-8.

3胡根火.钽铌湿法冶金分离方法评述[J].稀有金属与硬质合金,2015,43(1):29-32. 被引量:4

4韩建设,周勇.钽铌萃取分离工艺与设备进展[J].稀有金属与硬质合金,2004,32(2):15-20. 被引量:16

5邓小芬,王才明.降低Nb_2O_5中氟含量的研究[J].稀有金属与硬质合金,2005,33(1):11-13. 被引量:2

6郑典模,王振希,全水清,蒋柏泉,庄叶凯.萃取法制备高纯低氟氧化铌的研究[J].南昌大学学报:工科版,2005,27(2):71-73. 被引量:1

7韩建设,赵明智,王才明,张劲,周勇.钽铌湿法冶炼的“三废”综合治理工艺探讨[J].稀有金属与硬质合金,2006,34(4):40-44. 被引量:12

8王伟,李辉,郑培生.低品位钽铌原料的湿法冶金新工艺研究[J].稀有金属快报,2008,27(4):31-36. 被引量:10

9蒋柏泉,黄庆荣,郑典模,全水清,曾庆芳.溶剂浸取法制备低氟高纯氧化钽研究[J].南昌大学学报:工科版,2008,30(2):120-122. 被引量:1

10曹七林,姚卫东.陶瓷电容器用Nb_2O_5的制备[J].稀有金属与硬质合金,2008,36(3):43-44. 被引量:2

1余国峰,毛成枝,孙江安.工艺对铌片机械性能的影响[J].江西有色金属,1991,5(2):9-10.

2丁明.选好焦炭平均粒度降低75%硅铁电耗[J].铁合金,1993(6):19-24. 被引量:4

3胡友明.改善低SiO_2烧结矿性能[J].烧结球团,1995,20(1):12-15.

4刘颖晓,杜建民,王兆利,杜超玲.高炉渣控样的研制与应用[J].河南冶金,2007,15(4):21-22.

5赖志贤.CaO在高碳铬铁熔池中的行为探讨[J].铁合金,2000,31(5):12-15. 被引量:2

6宋修明,周俊.金隆闪速炉炉况变化及稳定对策[J].有色冶炼,1998,27(5):29-33.

712月韩国废钢进口量环比增加[J].不锈:市场与信息,2009(24):7-7.

8王海龙,吴玉程,王德宝,王文芳,宗跃,郑治祥.烧结工艺对Cu-Cr复合材料性能的影响[J].热处理,2009,24(2):36-38. 被引量:3

9陈艳梅,赵俊学.电渣冶金过程炉渣成分变化及其影响研究[J].工业加热,2014,43(3):23-25. 被引量:9

10刘贵德.铟电解精炼中电解液酸度的影响与控制[J].有色矿冶,2010,26(3):41-42. 被引量:4

Basic Information:

DOI:

Chinese Library Classification Number:TF841.6[冶金工程—有色金属冶金]

Citation Information:

Study is made of the variation mechanism of Nb 2O 5,main physical properties,ie grain shape,crystalline structure,average particle size,specific surface area and bulk density under calcination temperature.The law of the variation with the temperature variation is found out.Investigation is made on the reasons for the variation.Analysis is made of the relationship between Nb 2O 5 average particle size,specific surface area and bulk density so that the average particle size and specific surface area can be quickly calculated out by measuring the bulk density.

quote

GB/T 7714-2015 [1] WAN Ming-yuan. Influence of Calcination Temperature on Nb_2O_5 Physical Property[J]. Rare Metals and Cemented Carbides, 2002(1): 19-23.
MLA [1] WAN Ming-yuan. "Influence of Calcination Temperature on Nb_2O_5 Physical Property." Rare Metals and Cemented Carbides, no. 1, 2002, pp. 19-23.
APA [1] WAN Ming-yuan. (2002). Influence of Calcination Temperature on Nb_2O_5 Physical Property. Rare Metals and Cemented Carbides(1), 19-23.
IEEE [1] WAN Ming-yuan, "Influence of Calcination Temperature on Nb_2O_5 Physical Property," Rare Metals and Cemented Carbides, no. 1, pp. 19-23, 2002. keywords: {Nb 2O 5;calcination temperaturce;physical property}