Research on Leaching Process of Retired Ternary Lithium Battery Materials AITranslate
Abstract AITranslate
Retired ternary lithium battery materials were leached with sulfuric acid.The influences werestudied of sulfuric acid dosage,stirring rate,reductant dosage,leaching liquid-solid ratio,leaching time,leaching temperature,and leaching potential on the leaching of Ni,Co,Mn and Li,and the optimized leachingtechnical parameters were determined.The results show that under the optimized conditions of sulfuricacid dosage of 110%the theoretical amount,stirring rate of 250 r/min,reductant dosage of 70%the material,liquid-solid ratio of 5:1,leaching time of 4 h,leaching temperature of 85 ℃,and leaching potential of250 mV,the leaching rates of Ni,Co,Mn and Li are higher than 99%.The research on the process providesa scientific basis for the comprehensive utilization of retired ternary lithium battery materials.
KeyWords AITranslate
1程前,郑雅琴.废旧锂离子电池在氨基磺酸溶液中浸出的最优条件研究[J].广东化工,2016,43(18):33-34. 被引量:6
2李勋创,邬霞,张志强,刘永梅.溶剂萃取回收废弃锂离子电池中钴金属的研究[J].广东化工,2012,39(2):12-13. 被引量:4
3黎华玲,陈永珍,宋文吉,冯自平.湿法回收退役三元锂离子电池有价金属的研究进展[J].化工进展,2019,38(2):921-932. 被引量:27
4李强,王杜,陈若葵,唐红辉,乔延超,陈欢.用硫酸从废旧锂电池除铜尾渣中浸出镍、钴动力学[J].湿法冶金,2018,37(6):452-456. 被引量:7
5杨光,张鹏,钟岸,周秀清,何志荣.废旧锂离子动力电池的回收研究进展[J].广东化工,2018,45(5):139-141. 被引量:13
6陈少斌,程来星,邹燕飞,康立武.用硫酸从废锂电池中浸出钴的试验研究[J].湿法冶金,2015,34(1):32-34. 被引量:9
7施丽华,孙水裕,卢创鑫,杨帆,李惠萌.用硫酸-亚硫酸钠从废旧三元锂离子电池材料中浸出镍钴锰锂[J].湿法冶金,2018,37(5):384-387. 被引量:12
8陈亮,唐新村,张阳,瞿毅,王志敏.从废旧锂离子电池中分离回收钴镍锰[J].中国有色金属学报,2011,21(5):1192-1198. 被引量:64
9张笑笑,王鸯鸯,刘媛,吴锋,李丽,陈人杰.废旧锂离子电池回收处理技术与资源化再生技术进展[J].化工进展,2016,35(12):4026-4032. 被引量:31
1俞品华,徐文婷,王镇宗.基于电动汽车能耗优化的汽车悬架设计方法[J].专用汽车,2023(6):33-35.
2侯晓川,包申旭,李政希,唐华英,阮招娣.退役三元锂离子电池材料浸出液除铁工艺研究[J].稀有金属与硬质合金,2023,51(4):28-32.
1任汝龙,莫伟,黄钰华,梁鐥文,何春彦,周隆林.活性白土副产石膏渣中铁、铝的硫酸浸出[J].广西大学学报:自然科学版,2023,48(2):451-458.
2曾颜亮,霍瑞浩,邹建柏,廖春发,刘付朋.铜阳极泥复合浸出渣选择性分离硒过程热力学分析[J].有色金属科学与工程,2023,14(1):1-7. 被引量:1
3安浩,曾曼,余浩然,张文艺,彭明国,毛林强.基于响应曲面法的钠化焙烧-水浸法回收废加氢催化剂中有价金属工艺优化[J].环境工程学报,2023,17(1):259-267.
4第十六届水泥工业科技创新技术交流峰会暨水泥粉磨系统技术装备创新大会隆重开幕江苏省建材行业协会受邀出席[J].江苏建材,2023(2):167-168.
5黎燕.关于循环农业的农作物秸秆资源化利用模式探讨[J].农家科技:理论版,2023(6):179-181.
6姜楠.危废资源化综合利用工艺技术探析[J].清洗世界,2022,38(12):66-68.
7王晓民,刘冰,川刘芳,宋亚丽,何忠兴,康校花.浅析镍羰化合成残渣的湿法冶金处理技术[J].金川科技,2022(3):55-60.
8张敏娜,邓洋,韩慧泽.我国废旧轮胎资源化综合利用技术现状研究[J].资源节约与环保,2023(3):8-11.
9刘晓明[J].中国冶金,2023,33(3):152-152.
10卢岩川,周永强.济源市畜禽养殖粪污资源化利用现状、问题及对策[J].河南畜牧兽医,2023,44(8):51-52.
Basic Information:
DOI:
Chinese Library Classification Number:TF803.21[冶金工程—有色金属冶金]
Citation Information:
Retired ternary lithium battery materials were leached with sulfuric acid.The influences werestudied of sulfuric acid dosage,stirring rate,reductant dosage,leaching liquid-solid ratio,leaching time,leaching temperature,and leaching potential on the leaching of Ni,Co,Mn and Li,and the optimized leachingtechnical parameters were determined.The results show that under the optimized conditions of sulfuricacid dosage of 110%the theoretical amount,stirring rate of 250 r/min,reductant dosage of 70%the material,liquid-solid ratio of 5:1,leaching time of 4 h,leaching temperature of 85 ℃,and leaching potential of250 mV,the leaching rates of Ni,Co,Mn and Li are higher than 99%.The research on the process providesa scientific basis for the comprehensive utilization of retired ternary lithium battery materials.
quote
| GB/T 7714-2015 | [1] HOU Xiao-chuan, BAO Shen-xu, LI Zheng-xi, et al. Research on Leaching Process of Retired Ternary Lithium Battery Materials[J]. Rare Metals and Cemented Carbides, 2023(2): 98-103. |
| MLA | [1] HOU Xiao-chuan, et al., "Research on Leaching Process of Retired Ternary Lithium Battery Materials." Rare Metals and Cemented Carbides, no. 2, 2023, pp. 98-103. |
| APA | [1] HOU Xiao-chuan, BAO Shen-xu, LI Zheng-xi, & TANG Hua-ying. (2023). Research on Leaching Process of Retired Ternary Lithium Battery Materials. Rare Metals and Cemented Carbides(2), 98-103. |
| IEEE | [1] HOU Xiao-chuan, BAO Shen-xu, LI Zheng-xi, and TANG Hua-ying, "Research on Leaching Process of Retired Ternary Lithium Battery Materials," Rare Metals and Cemented Carbides, no. 2, pp. 98-103, 2023. keywords: {retired ternary lithium battery;sulfuric acid leaching;nickel;cobalt;lithium;manganese;sodiummetabisulfite} |