Dual Role of Ligand for Porphyrin-Based Covalent Organic Framework Exfoliation and Turn-Up Fluorescence Sensing AITranslate
Abstract AITranslate
Covalent organic nanosheets (CONs) have been attracting widespread attention; however, their fabrication remains challenging owing to their uncontrollable thickness, multilayer structure, and low yield. Herein, we report a ligand that simultaneously achieves porphyrin covalent organic framework (COF) exfoliation and “turn-up” fluorescence sensing. By introducing aniline as the axial ligand and coordinating it to porphyrin COF, uniform nanosheets with 6–10 layers were obtained that exhibited 28 times greater fluorescence for aniline than the pristine COF owing to a synergistic effect. This work not only paves the way to utilize COF to realize highly efficient turn-up fluorescent sensing of aniline but also provides a strategy to make thin-layer nanosheets.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.2c01758
Chinese Library Classification Number:
Citation Information:
Covalent organic nanosheets (CONs) have been attracting widespread attention; however, their fabrication remains challenging owing to their uncontrollable thickness, multilayer structure, and low yield. Herein, we report a ligand that simultaneously achieves porphyrin covalent organic framework (COF) exfoliation and “turn-up” fluorescence sensing. By introducing aniline as the axial ligand and coordinating it to porphyrin COF, uniform nanosheets with 6–10 layers were obtained that exhibited 28 times greater fluorescence for aniline than the pristine COF owing to a synergistic effect. This work not only paves the way to utilize COF to realize highly efficient turn-up fluorescent sensing of aniline but also provides a strategy to make thin-layer nanosheets.
quote
| GB/T 7714-2015 | [1] Lihua Li, Yinghu Ma, Haohao Yang, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c01758. |
| MLA | [1] Lihua Li, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c01758. |
| APA | [1] Lihua Li, Yinghu Ma, Haohao Yang, Ning Wu, Liping Peng, & Junjiao Wang. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c01758 |
| IEEE | [1] Lihua Li, Yinghu Ma, Haohao Yang, Ning Wu, Liping Peng, and Junjiao Wang, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c01758. keywords: {covalent organic frameworks (COFs);covalent organic nanosheets (CONs);exfoliation;fluorescence sensor;aniline} |