Experimental Study on Phase Transformation of Ilmenite Ore during High Temperature Carbon Thermal Reduction AITranslate

Beijing University of Science and Technology of Science and Technology of Science and Technology;Beijing University of Science and Technology of Science and Technology of Science and Technology;Beijing University of Science and Technology of Science and Technology of Science and Technology;Beijing University of Science and Technology of Science and Technology of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Using coal powder as reducing agent, carbon thermal reduction of ilmenite with 61.85 % TiO2 was performed at 1 573-1 873 K,and the phase transformation and microstructure of reaction products were studied by XRD and SEM. The results show that when carbon-oxygen ratio of carbon to all oxides in ilmenite is higher than 1 : 1,all the reduction products are TiC and Fe. So the TiC/Fe composites can be obtained from ilmenite by carbon thermal reduction, providing reference for the comprehensive utilization of Fe and Ti in ilmenite ore.

KeyWords AITranslate

ilmenite carbon thermal reduction TiC phase analysis carbon addition reduction temperature

1余伟.用钛精矿冶炼钛渣的工业试验研究[J].稀有金属与硬质合金,2004,32(4):29-32. 被引量:4

2蒋伟,蒋训雄,汪胜东,范艳青,刘巍,张登高.钛铁矿制备人造金红石半工业试验[J].有色金属:冶炼部分,2014(11):28-30. 被引量:4

3郑子恩,赵婷,袁仕华.我国钛工业的技术现状及展望[J].稀有金属与硬质合金,2012,40(4):35-39. 被引量:5

4王震,李坚,华一新,张志,张远,柯平超.钛制取工艺研究进展[J].稀有金属,2014,38(5):915-927. 被引量:27

5白天蛟,丁伟中,尚兴付,谈定生,郭曙强.攀枝花钛精矿还原锈蚀法研究[J].钢铁钒钛,2016,37(4):8-13. 被引量:7

6吴恩辉,朱荣,杨绍利,李宏,李军,侯静.空气气氛下钒钛铁精矿碳热还原制备Fe-Ti(C,N)复合粉末[J].钢铁钒钛,2016,37(1):46-50. 被引量:4

7张建良,杨广庆,国宏伟,邵久刚,李健,文永才.含钒钛铁矿球团还原过程中微观结构变化[J].北京科技大学学报,2013,35(1):41-48. 被引量:13

8刘阳,曾令可,胡晓力,王慧,程小苏,张明,史琳林.碳化钛的合成及其应用研究进展[J].中国陶瓷,2002,38(5):7-10. 被引量:26

1喻连香,汤优优,刘军,陈雄.含难分离赤铁矿的钛铁粗精矿选冶提质工艺研究[J].金属矿山,2020(5):185-190. 被引量:3

2尹国亮,李仕超,徐慎颖,张丹,金成国,张嫒馨.还原钛制备富钛料工艺现状及应用前景分析[J].铁合金,2022,53(3):34-37. 被引量:3

1刘超,洪秋阳,陈志强,刘勇,刘牡丹,吕昊子.国外某钒钛铁矿工艺矿物学与磁选回收技术研究[J].矿物学报,2021,41(3):277-286. 被引量:1

2刘超,刘勇,刘牡丹,陈志强,吕建芳,吕昊子.选冶联合回收风化型钒钛铁矿试验研究[J].矿冶工程,2022,42(3):51-54. 被引量:1

3胡厚勤,罗荣飞,吴雪红.钛铁矿浮选精矿选矿提质试验研究[J].矿冶,2022,31(4):19-24.

4李珍珍.富钛料制备中不同亚熔盐反应介质及工艺参数的影响研究[J].山西冶金,2023,46(3):21-23.

5农胜英,王祥丁,覃辉平,方敢,黄翔,杨阳,李潇咏,张鹏鹏,黄春雷.人造金红石的生产技术及应用研究[J].大众科技,2023,25(8):62-65.

6吕津辉.氯化法钛白粉生产工艺研究进展[J].中国粉体工业,2023(4):9-13.

1吴恩辉,侯静,李军,赖奇,杨绍利,柴航,黄平,徐众.钒钛铁精矿盐酸浸出渣碳热还原法制备碳氮化钛复合粉末工艺研究[J].中国有色冶金,2017,46(5):66-71.

2郑涌,周洋,王嘉琪,李鸿宇,李世波,黄振莺,李翠伟,翟洪祥.高体积含量TiC/Fe复合材料的制备及力学性能[J].稀有金属材料与工程,2017,46(9):2673-2678. 被引量:1

3赵福荣.MR诊断对乳腺癌的诊断价值分析[J].实用妇科内分泌电子杂志,2017,4(15):136-136.

4尤登攀.九味熄风颗粒与氟哌啶醇治疗抽动障碍的对照研究[J].疾病监测与控制,2017,11(11):885-886. 被引量:4

5陈如标,王乐,周天亮,李晓艳,罗东,潘桦滟.碳热还原法合成LaSi_3N_5∶Ce^(3+)蓝色荧光粉及其发光性能研究[J].光谱学与光谱分析,2017,37(10):3032-3036. 被引量:1

6李杰,信自成,刘卫星,杨爱民,张玉柱,潘建磊.钒钛烧结矿低温还原粉化性能预测[J].烧结球团,2017,42(5):1-5. 被引量:4

7程辰,周胜利,周军,顾艳.磁共振动态增强联合弥散加权成像对乳腺癌的诊断价值研究[J].医学影像学杂志,2017,27(11):2122-2126. 被引量:35

8何鹏,居殿春,沈朋飞,靳红滨.基于直接还原熔分的赤泥综合利用试验研究[J].冶金能源,2017,36(4):57-60. 被引量:2

9刘丽霞,李文挺,彭军,张磊,安胜利,薛应东,刘伟,李晓明.粉煤灰中锗的赋存状态研究[J].稀有金属与硬质合金,2017,45(5):27-30. 被引量:6

10李明强,樊俊杰,张忠孝,乌晓江.液渣捕捉高碱煤中碱金属特性及机理[J].燃烧科学与技术,2017,23(5):429-435. 被引量:10

Basic Information:

DOI:

Chinese Library Classification Number:TF041[冶金工程—冶金物理化学]

Citation Information:

Using coal powder as reducing agent, carbon thermal reduction of ilmenite with 61.85 % TiO2 was performed at 1 573-1 873 K,and the phase transformation and microstructure of reaction products were studied by XRD and SEM. The results show that when carbon-oxygen ratio of carbon to all oxides in ilmenite is higher than 1 : 1,all the reduction products are TiC and Fe. So the TiC/Fe composites can be obtained from ilmenite by carbon thermal reduction, providing reference for the comprehensive utilization of Fe and Ti in ilmenite ore.

quote

GB/T 7714-2015 [1] GU Jing, XIA De-hong, QI Zhao-dong, et al. Experimental Study on Phase Transformation of Ilmenite Ore during High Temperature Carbon Thermal Reduction[J]. Rare Metals and Cemented Carbides, 2017(5): 17-21.
MLA [1] GU Jing, et al., "Experimental Study on Phase Transformation of Ilmenite Ore during High Temperature Carbon Thermal Reduction." Rare Metals and Cemented Carbides, no. 5, 2017, pp. 17-21.
APA [1] GU Jing, XIA De-hong, QI Zhao-dong, & AO Wen-qing. (2017). Experimental Study on Phase Transformation of Ilmenite Ore during High Temperature Carbon Thermal Reduction. Rare Metals and Cemented Carbides(5), 17-21.
IEEE [1] GU Jing, XIA De-hong, QI Zhao-dong, and AO Wen-qing, "Experimental Study on Phase Transformation of Ilmenite Ore during High Temperature Carbon Thermal Reduction," Rare Metals and Cemented Carbides, no. 5, pp. 17-21, 2017. keywords: {ilmenite;carbon thermal reduction;TiC;phase analysis;carbon addition;reduction temperature}