daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Sandwich-like Structure of Indole and Carbon Dioxide with Efficient CO2 Capture and Conversion AITranslate

Southwest University of Science and Technology; Southwest University of Science and Technology; Southwest University of Science and Technology; Southwest University of Science and Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A hydroxyl-containing and aniline-functionalized indole-based microporous organic polymer (MOP) material poly(hydroxyl indole)-NH2 (PHOIN-NH2) has been successfully designed and synthesized. It was first proven that, due to the electron-rich benzene ring of the aniline group and the electron donor hydroxyl groups donating their electron density to the inner indole ring, the highly electron-rich π indole plane can simultaneously attract two CO2 molecules via the double local dipole-π interactions, thereby forming a “CO2–indole–CO2” sandwich-like structure and endowing this microporous material with a remarkable CO2 adsorption capacity (33 wt %). In addition, due to the classical acid–base interaction between the aniline group in the PHOIN-NH2 aerogel and the CO2 molecule, the resulting material displays excellent gas selectivity (CO2/N2 = 146, CO2/CH4 = 24). Moreover, the phenolic–OH groups in the PHOIN-NH2 aerogel provide an abundance of sites for anchoring Zn2+ via metal-coordination interactions for effective conversion of CO2 into propylene carbonate.

KeyWords AITranslate

double local dipoleπ acid−base metalcoordination CO2 adsorption selectivity conversion
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00808

Chinese Library Classification Number:

Citation Information:

A hydroxyl-containing and aniline-functionalized indole-based microporous organic polymer (MOP) material poly(hydroxyl indole)-NH2 (PHOIN-NH2) has been successfully designed and synthesized. It was first proven that, due to the electron-rich benzene ring of the aniline group and the electron donor hydroxyl groups donating their electron density to the inner indole ring, the highly electron-rich π indole plane can simultaneously attract two CO2 molecules via the double local dipole-π interactions, thereby forming a “CO2–indole–CO2” sandwich-like structure and endowing this microporous material with a remarkable CO2 adsorption capacity (33 wt %). In addition, due to the classical acid–base interaction between the aniline group in the PHOIN-NH2 aerogel and the CO2 molecule, the resulting material displays excellent gas selectivity (CO2/N2 = 146, CO2/CH4 = 24). Moreover, the phenolic–OH groups in the PHOIN-NH2 aerogel provide an abundance of sites for anchoring Zn2+ via metal-coordination interactions for effective conversion of CO2 into propylene carbonate.

quote

GB/T 7714-2015 [1] Yewei Xu, Cheng Wang, Li Yang, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00808.
MLA [1] Yewei Xu, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00808.
APA [1] Yewei Xu, Cheng Wang, Li Yang, & Guanjun Chang. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00808
IEEE [1] Yewei Xu, Cheng Wang, Li Yang, and Guanjun Chang, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00808. keywords: {double local dipoleπ;acid−base;metalcoordination;CO2 adsorption;selectivity;conversion}