Revealing the Anisotropy in Protonation-Induced Electronic Phase Transitions of Rare-Earth Nickelates within a Marine Environment AITranslate
Abstract AITranslate
Although the discovery of the electrochemical protonation-induced electronic phase transition of rare-earth nickelates (ReNiO3) enables potential application in sensing the ocean electric field that simulates the working principle of the ampullary organ of marine animals, whether such a functionality is anisotropic is previously overlooked. Herein, we demonstrate the anisotropy in the protonation-induced electronic phase transition in ReNiO3 (Re = Sm, Nd, and Eu) thin films as electrochemically triggered in an ocean environment. A larger elevation in the material resistivity triggered by an electric field within an ocean environment is observed for ReNiO3/LaAlO3(110), compared to ReNiO3/LaAlO3(001) and ReNiO3/LaAlO3(111). This is attributed to the orientation-related in-plane oxygen atomic density that results in more effective in-plane proton diffusion along the adjacent oxygen position, as further confirmed by the electrochemical cyclic voltammetry characterization. In addition, the larger activation energy associated to the anisotropic in-plane electronic structures of ReNiO3/LaAlO3(110) is also expected to promote the formation of electron-localized orbital configurations upon hydrogenation. As demonstrated, anisotropy sheds light on another possibility that can be further introduced to regulate the protonation-induced electronic phase transition properties of ReNiO3 for its potential applications such as ocean electric field sensing or biosensing.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.2c00804
Chinese Library Classification Number:
Citation Information:
Although the discovery of the electrochemical protonation-induced electronic phase transition of rare-earth nickelates (ReNiO3) enables potential application in sensing the ocean electric field that simulates the working principle of the ampullary organ of marine animals, whether such a functionality is anisotropic is previously overlooked. Herein, we demonstrate the anisotropy in the protonation-induced electronic phase transition in ReNiO3 (Re = Sm, Nd, and Eu) thin films as electrochemically triggered in an ocean environment. A larger elevation in the material resistivity triggered by an electric field within an ocean environment is observed for ReNiO3/LaAlO3(110), compared to ReNiO3/LaAlO3(001) and ReNiO3/LaAlO3(111). This is attributed to the orientation-related in-plane oxygen atomic density that results in more effective in-plane proton diffusion along the adjacent oxygen position, as further confirmed by the electrochemical cyclic voltammetry characterization. In addition, the larger activation energy associated to the anisotropic in-plane electronic structures of ReNiO3/LaAlO3(110) is also expected to promote the formation of electron-localized orbital configurations upon hydrogenation. As demonstrated, anisotropy sheds light on another possibility that can be further introduced to regulate the protonation-induced electronic phase transition properties of ReNiO3 for its potential applications such as ocean electric field sensing or biosensing.
quote
| GB/T 7714-2015 | [1] Haifan Li, Yuzhao Wang, Haiyan Li, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00804. |
| MLA | [1] Haifan Li, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00804. |
| APA | [1] Haifan Li, Yuzhao Wang, Haiyan Li, Fengbo Yan, Binghui Ge, Jie Zhang, Nuofu Chen, & Jikun Chen. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00804 |
| IEEE | [1] Haifan Li, Yuzhao Wang, Haiyan Li, Fengbo Yan, Binghui Ge, Jie Zhang, Nuofu Chen, and Jikun Chen, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c00804. keywords: {perovskite oxide electronic correlation protonation thin film anisotropy electronic phase transition rareearth nickelates} |