Tensile Strength of Tungsten Wires vs their Quality AITranslate
Abstract AITranslate
The paper analyses the tensile strength of tungsten wires during processing vstheir guality, and gives suggestions for wire upgrading, such as optimize the annealing conditions, improve the processing technology to control the wire strength d& and so on.
KeyWords AITranslate
1孟庆乐,黄立峰,卜春阳.粗钼丝空心断裂的成因分析[J].中国钼业,2013,37(3):43-46.
2李世伟,孟庆乐,黄立峰.钼丝抗拉强度控制的探讨[J].中国钼业,2013,37(6):49-51.
1Nagy,G,范荣奎.中间退火对钨灯丝再结晶的影响[J].钨钼材料,1993(4):22-26.
2蔡健,卫敏玲,房振山.提高电缆箔力学性能的工艺措施[J].轻合金加工技术,2000,28(7):14-16. 被引量:1
3张玉章.漆包线柔软度的影响因素讨论[J].电线电缆,2005(6):28-29. 被引量:1
4卢德强.铝箔力学性能的研究[J].轻合金加工技术,1998,26(1):8-11. 被引量:4
5冶专.电池壳体用铝合金板及其制造方法[J].铝加工,2006(3):42-42.
6王金荣.采用铜拉中间退火 减小漆包线回弹角[J].电线电缆,1992(4):64-64.
7刘楚明,张新明,陈志永,周卓平,林林,陈文,李成利.中间退火对高纯铝箔立方织构的影响[J].金属热处理,2001,26(3):28-30. 被引量:8
8韩富生.前置式在线中间退火工艺及其拉丝机[J].电线电缆,2012(5):41-44.
9卢国辉,黄惠平.无氧铜细丝拉丝中间退火工艺与组织性能[J].热加工工艺,2000,29(4):36-37. 被引量:1
10胡汪洋,陈纪昌,刘二微,王均安.中间退火对Ni-7at%W合金基带再结晶织构的影响[J].金属热处理,2014,39(1):89-94. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TM923.04[电气工程—电力电子与电力传动]
Citation Information:
The paper analyses the tensile strength of tungsten wires during processing vstheir guality, and gives suggestions for wire upgrading, such as optimize the annealing conditions, improve the processing technology to control the wire strength d& and so on.
quote
| GB/T 7714-2015 | [1] LI Kui-chu. Tensile Strength of Tungsten Wires vs their Quality[J]. Rare Metals and Cemented Carbides, 1997(1): 38-40. |
| MLA | [1] LI Kui-chu. "Tensile Strength of Tungsten Wires vs their Quality." Rare Metals and Cemented Carbides, no. 1, 1997, pp. 38-40. |
| APA | [1] LI Kui-chu. (1997). Tensile Strength of Tungsten Wires vs their Quality. Rare Metals and Cemented Carbides(1), 38-40. |
| IEEE | [1] LI Kui-chu, "Tensile Strength of Tungsten Wires vs their Quality," Rare Metals and Cemented Carbides, no. 1, pp. 38-40, 1997. keywords: {tungsten wire quality,tensile strength,technological conditions, annealing} |