Wettability Gradient-Structured Bicomponent Polylactic Acid–Viscose Composite Fabrics with Enhanced Asymmetric Water Penetration Characteristics AITranslate

Tiangong University; Zhongyuan University of Technology; Zhongyuan University of Technology;Henan Key Laboratory of Medical Polymer Materials Technology and Application;Henan Key Laboratory of Medical Polymer Materials Technology and Application; Tiangong University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Fabrics with asymmetric water penetration characteristics play an important role in our daily lives because they are often used in hygiene and medical applications. However, the existing materials have serious limitations, such as low durability and complex manufacturing processes. Herein, we report a bicomponent polylactic acid–viscose (PLA-VIS) composite fabric with a wettability gradient. The fabric can be manufactured industrially by a simple process that combines two compatible methods: needle punching and through air bonding. Five-layer cross-laid fibrous webs with various mass ratios of VIS fiber distribution were laminated in the thickness direction to produce a wettability gradient. Owing to its wettability gradient index (Rv) and porosity, the resulting composite fabric had enhanced asymmetric water penetration characteristics. Its accumulative one-way transport index (AOTI) increased from 77.8 to 165.6% as the Rv value increased from 0 to 1.5; its saturated water adsorption rate increased by 14.1 times and its water retention rate increased by 11.6 times as the porosity increased from 90 to 96%. Moreover, its water wicking performance clearly demonstrated that there was a large difference in water wetting capacity between the two sides of the fabric. The PLA-VIS composite fabric described herein has potential for use in hygiene and medical applications.

KeyWords AITranslate

wettability gradient asymmetric penetration nonwovens needle punching chemicalfree bicomponent polylactic acid Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00249

Chinese Library Classification Number:

Citation Information:

Fabrics with asymmetric water penetration characteristics play an important role in our daily lives because they are often used in hygiene and medical applications. However, the existing materials have serious limitations, such as low durability and complex manufacturing processes. Herein, we report a bicomponent polylactic acid–viscose (PLA-VIS) composite fabric with a wettability gradient. The fabric can be manufactured industrially by a simple process that combines two compatible methods: needle punching and through air bonding. Five-layer cross-laid fibrous webs with various mass ratios of VIS fiber distribution were laminated in the thickness direction to produce a wettability gradient. Owing to its wettability gradient index (Rv) and porosity, the resulting composite fabric had enhanced asymmetric water penetration characteristics. Its accumulative one-way transport index (AOTI) increased from 77.8 to 165.6% as the Rv value increased from 0 to 1.5; its saturated water adsorption rate increased by 14.1 times and its water retention rate increased by 11.6 times as the porosity increased from 90 to 96%. Moreover, its water wicking performance clearly demonstrated that there was a large difference in water wetting capacity between the two sides of the fabric. The PLA-VIS composite fabric described herein has potential for use in hygiene and medical applications.

quote

GB/T 7714-2015 [1] Qi Zhen, Heng Zhang, He Li, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00249.
MLA [1] Qi Zhen, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00249.
APA [1] Qi Zhen, Heng Zhang, He Li, JingQiang Cui, Jie Cheng, & Yong Liu. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00249
IEEE [1] Qi Zhen, Heng Zhang, He Li, JingQiang Cui, Jie Cheng, and Yong Liu, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00249. keywords: {wettability gradient;asymmetric penetration;nonwovens;needle punching;chemicalfree;bicomponent polylactic acid;Show More}