Preparation and Raman Spectroscopic Study of Flower-like Micro-nanostructures of TeO_2 AITranslate

School of Opto-electronic Information Science and Technology,Yantai University;School of Opto-electronic Information Science and Technology,Yantai University;School of Opto-electronic Information Science and Technology,Yantai University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Using Bi2Te3 powder as raw material,TeO2 micro-nanostructures were successfully prepared by thermal evaporation.The morphology of the synthesized products was characterized by scanning electron microscopy (SEM).The results illustrate that the miero-nanostructures of the synthesized products are flower-like clusters formed by stacking a large number of micro-nanosheets.It was found by EDS that the sample consisted of two elements of Te and O.The Raman spectra of synthesized products were characterized by eonfocal laser Raman spectroscopy.The results show that the spectra of the synthesized products are consistent with those of TeO2 crystals.Also with the increase of thermal evaporation temperature,the higher the intensity of the Raman peak is,the sharper the characteristic peak is,and the better the crystallinity of the product prepared on Si substrate is.

KeyWords AITranslate

TeO2 micro-nanostructure thermal evaporation method Raman spectroscopy

1朱勇,岳世海,王威,殷学技,葛增伟.二氧化碲晶体及其在红外器件中的应用研究进展[J].无机材料学报,2015,30(8):802-808. 被引量:3

2季小红,桑文斌,刘冬华,李冬梅,钱永彪,史伟民,闵嘉华.声光晶体TeO_2的生长及缺陷研究[J].人工晶体学报,2001,30(1):93-98. 被引量:5

3沈岩柏,魏德洲,马嘉伟,张宝庆.TeO_2纳米线的制备及其室温NO_2气敏特性[J].东北大学学报:自然科学版,2014,35(7):1019-1022. 被引量:4

4储耀卿,葛增伟,吴国庆,殷学技,唐林耀.大尺寸优质声光晶体TeO_2的生长[J].人工晶体学报,2004,33(5):810-812. 被引量:3

5刘晓静,仇怀利,王爱华,殷绍唐,尤静林,蒋国昌.二氧化碲(TeO_2)晶体的Raman光谱研究[J].光谱学与光谱分析,2003,23(3):484-486. 被引量:8

1孙逗.那花[J].章回小说:上旬刊(文学版),2018(33):19-34.

2田甜,崔庆芝,雷云,沈志杰,徐家跃.Dy^(3+)掺杂TeO_2单晶的生长及其发光性能研究[J].中国照明电器,2017(9):15-19. 被引量:2

3周树生,刘昌碧.光纤缺陷定位检测用声光偏转器[J].压电与声光,1987,0(4):25-27.

4潘永刚,付秀华,张程.二氧化碲晶体混合低温等离子体表面改性技术制备光学薄膜[J].材料科学,2019,9(1):25-31. 被引量:1

5冒俊霞,王彦,胡祖明,于俊荣,诸静.巯基改性碳纳米管的制备与表征[J].化工新型材料,2019,47(3):88-93. 被引量:3

6刘中.宋人的晚风[J].黄河,2019,0(1):177-181.

7吴婧,李松,王月鑫,郭川洲,封莹莹,蔡可迎.氮掺杂碳催化过硫酸钾降解水中二甲酚橙[J].精细石油化工进展,2018,19(6):11-15. 被引量:1

8张旭,兑宝峰.松塔掌栽培与繁殖[J].中国花卉园艺,2019,0(2):32-32.

9狄保寿.惊天偷渡[J].章回小说:上旬刊(文学版),2018(16):14-29.

10王梓儒,刘铭晖,刘恩凯,董作人,蔡圣闻,殷磊,刘峰.基于极值统计的拉曼光谱信噪比评估方法与应用[J].光谱学与光谱分析,2019,39(4):1080-1085.

Basic Information:

DOI:

Chinese Library Classification Number:O433.4[机械工程—光学工程]

Citation Information:

Using Bi2Te3 powder as raw material,TeO2 micro-nanostructures were successfully prepared by thermal evaporation.The morphology of the synthesized products was characterized by scanning electron microscopy (SEM).The results illustrate that the miero-nanostructures of the synthesized products are flower-like clusters formed by stacking a large number of micro-nanosheets.It was found by EDS that the sample consisted of two elements of Te and O.The Raman spectra of synthesized products were characterized by eonfocal laser Raman spectroscopy.The results show that the spectra of the synthesized products are consistent with those of TeO2 crystals.Also with the increase of thermal evaporation temperature,the higher the intensity of the Raman peak is,the sharper the characteristic peak is,and the better the crystallinity of the product prepared on Si substrate is.

quote

GB/T 7714-2015 [1] JIANG Jia-liang, ZHANG Jun, SONG Zhi-chao. Preparation and Raman Spectroscopic Study of Flower-like Micro-nanostructures of TeO_2[J]. Rare Metals and Cemented Carbides, 2019(1): 43-46.
MLA [1] JIANG Jia-liang, et al., "Preparation and Raman Spectroscopic Study of Flower-like Micro-nanostructures of TeO_2." Rare Metals and Cemented Carbides, no. 1, 2019, pp. 43-46.
APA [1] JIANG Jia-liang, ZHANG Jun, & SONG Zhi-chao. (2019). Preparation and Raman Spectroscopic Study of Flower-like Micro-nanostructures of TeO_2. Rare Metals and Cemented Carbides(1), 43-46.
IEEE [1] JIANG Jia-liang, ZHANG Jun, and SONG Zhi-chao, "Preparation and Raman Spectroscopic Study of Flower-like Micro-nanostructures of TeO_2," Rare Metals and Cemented Carbides, no. 1, pp. 43-46, 2019. keywords: {TeO2;micro-nanostructure;thermal evaporation method;Raman spectroscopy}