daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Effect of Nano-La2O3 Doping on Microstructure and Mechanical Properties of Mo2NiB2 Based Cermets AITranslate

School of Materials Science and Engineering,Shaanxi University of Technology;School of Materials Science and Engineering,Shaanxi University of Technology;School of Materials Science and Engineering,Shaanxi University of Technology;School of Materials Science and Engineering,Shaanxi University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Based on the composition of Ni-6 B-53.3 Mo,Mo2NiB2 based cermets with different content of nano-La2O3 particles(0,0.3%,0.6%,0.9%,1.2%)were prepared by vacuum hot pressing sintering technology,and their microstructure and mechanical properties were studied.The results show that doping La2O3 can improve the solubility of hard phase and Ni based binding phase of Mo2NiB2 based cermets,reduce the grain size and make the distribution of Ni based binding phase more uniform.With the increase of La2O3 content,the bending strength,hardness and compressive strength of Mo2NiB2 based cermets increase first and then decrease.The cermet with 0.6%La2O3 has the maximum bending strength and hardness of 603.55 MPa and 902.1 HV,respectively.The cermet with 0.3%La2O3 has the maximum compressive strength of 550 MPa.However,with the increase of La2O3 content,both the fracture toughness and density of Mo2NiB2 based cermets decrease.

KeyWords AITranslate

vacuum hot pressing sintering Mo2NiB2 based cermet La2O3 microstructure mechanical property

1杨林,潘应君,柯德庆,徐源源,王盼.稀土Sm_2O_3对Mo_2NiB_2基金属陶瓷微观组织和力学性能的影响[J].武汉科技大学学报,2017,40(2):105-109. 被引量:9

2易善杰,尹海清,殷小龙,曲选辉,ZHENG Qingjun.Mo_2NiB_2基金属陶瓷的制备与性能[J].工程科学学报,2015,37(4):488-493. 被引量:8

3林启权,龙燕萍.La_2O_3掺杂对金属陶瓷显微结构与性能的影响[J].硅酸盐学报,2014,42(12):1537-1542. 被引量:3

4李炯义,曹顺华,林信平.硬质合金中的晶粒长大抑制剂[J].硬质合金,2004,21(1):56-60. 被引量:23

1王鑫,蒋妍.锂原电池正极MnO2-Ag的制备及放电性能研究[J].湖北工业大学学报,2020,35(5):31-34.

1同艳维,冯成岚,李娜丽,崔旭梅,张雪峰.碳纤维添加量对Ti(C,N)基金属陶瓷材料组织和性能的影响[J].稀有金属与硬质合金,2020,48(3):50-53. 被引量:2

2刘建科,徐亚宁,曹文斌,张瑞婷,宋帆,谢鑫,乔毅楠.La2O3掺杂对Zn–Pr基压敏陶瓷电学特性的影响[J].硅酸盐学报,2020,0(3):337-342. 被引量:3

3冉岚,范冰冰,兰琳琳.硅烷偶联剂改性粉煤灰及其在聚氨酯中的应用[J].热固性树脂,2020(2):21-25. 被引量:6

4鲜勇,刘伟,陈立明,丁义超,王静,刘瑶.界面掺杂石墨烯的Ti-ZrO2双层复合材料制备及性能研究[J].钢铁钒钛,2020(2):38-41. 被引量:1

5冯垚,贺鹤鸣,郝艳,武开鹏,何盈春.Y3+-La3+共掺对MgAl2O4透明玻璃陶瓷结构及光学性能的影响[J].西南科技大学学报,2019,34(4):1-5.

6万帅,许衡,曹伟,谷山强,张瑞,李桂芳.La2O3的掺杂对氧化锌压敏陶瓷电性能的影响[J].压电与声光,2020,42(3):353-356. 被引量:2

7韦胜利.陕钢汉钢超厚料层均质烧结技术工业实践[J].山西冶金,2020,43(3):116-118. 被引量:2

8韩宝帅,万雄,徐严谨,侯红亮,荆涛,马晓光,裴葆青.基于韧脆复合结构的Ti-Al-Ti-Ti2AlNb层状复合材料的组织与力学性能[J].稀有金属材料与工程,2020,49(6):2083-2088. 被引量:1

9秦笑威,盛利文,李双,谢志鹏.振荡压力烧结氮化硅陶瓷微观形貌及其力学性能[J].硅酸盐学报,2020(6):803-809. 被引量:3

Basic Information:

DOI:

Chinese Library Classification Number:TG148[金属学及工艺—金属材料]

Citation Information:

Based on the composition of Ni-6 B-53.3 Mo,Mo2NiB2 based cermets with different content of nano-La2O3 particles(0,0.3%,0.6%,0.9%,1.2%)were prepared by vacuum hot pressing sintering technology,and their microstructure and mechanical properties were studied.The results show that doping La2O3 can improve the solubility of hard phase and Ni based binding phase of Mo2NiB2 based cermets,reduce the grain size and make the distribution of Ni based binding phase more uniform.With the increase of La2O3 content,the bending strength,hardness and compressive strength of Mo2NiB2 based cermets increase first and then decrease.The cermet with 0.6%La2O3 has the maximum bending strength and hardness of 603.55 MPa and 902.1 HV,respectively.The cermet with 0.3%La2O3 has the maximum compressive strength of 550 MPa.However,with the increase of La2O3 content,both the fracture toughness and density of Mo2NiB2 based cermets decrease.

quote

GB/T 7714-2015 [1] ZHOU Pei-de, LI Wen-hu, AI Tao-tao, et al. Effect of Nano-La2O3 Doping on Microstructure and Mechanical Properties of Mo2NiB2 Based Cermets[J]. Rare Metals and Cemented Carbides, 2020(3): 33-37.
MLA [1] ZHOU Pei-de, et al., "Effect of Nano-La2O3 Doping on Microstructure and Mechanical Properties of Mo2NiB2 Based Cermets." Rare Metals and Cemented Carbides, no. 3, 2020, pp. 33-37.
APA [1] ZHOU Pei-de, LI Wen-hu, AI Tao-tao, & DONG Hong-feng. (2020). Effect of Nano-La2O3 Doping on Microstructure and Mechanical Properties of Mo2NiB2 Based Cermets. Rare Metals and Cemented Carbides(3), 33-37.
IEEE [1] ZHOU Pei-de, LI Wen-hu, AI Tao-tao, and DONG Hong-feng, "Effect of Nano-La2O3 Doping on Microstructure and Mechanical Properties of Mo2NiB2 Based Cermets," Rare Metals and Cemented Carbides, no. 3, pp. 33-37, 2020. keywords: {vacuum hot pressing sintering;Mo2NiB2 based cermet;La2O3;microstructure;mechanical property}