Abstract AITranslate

Optical devices with switchable optical properties have attracted great interest in recent years because of their extensive engineering applications. The dynamic tuning of optical properties can be triggered by various types of external stimuli. In this work, a mechanically induced elastomeric optical transmittance modulator is reported. The design is composed of poly(dimethylsiloxane), a silicone-based rubber transparent at visible wavelengths, with gold nanofilms deposited on the surface. The influence of geometric parameters on the total transmittance is studied utilizing the Rigorous Coupled Wave Analysis model. Taking advantage of the excellent stretching capacity of the elastomer, reversible modulation of both normal and total transmittance is achieved. A 42% rise in the total transmittance is realized under a strain of 80%. Cycle testing illustrates stable structural integrity and optical performance even after repeated strain cycles. This elastomeric optical transmittance modulator opens avenues for practical applications due to its simple design and facile tunability.

KeyWords AITranslate

optical modulator elastomer mechanically induced tunable optical transmittance smart windows
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00764

Chinese Library Classification Number:

Citation Information:

Optical devices with switchable optical properties have attracted great interest in recent years because of their extensive engineering applications. The dynamic tuning of optical properties can be triggered by various types of external stimuli. In this work, a mechanically induced elastomeric optical transmittance modulator is reported. The design is composed of poly(dimethylsiloxane), a silicone-based rubber transparent at visible wavelengths, with gold nanofilms deposited on the surface. The influence of geometric parameters on the total transmittance is studied utilizing the Rigorous Coupled Wave Analysis model. Taking advantage of the excellent stretching capacity of the elastomer, reversible modulation of both normal and total transmittance is achieved. A 42% rise in the total transmittance is realized under a strain of 80%. Cycle testing illustrates stable structural integrity and optical performance even after repeated strain cycles. This elastomeric optical transmittance modulator opens avenues for practical applications due to its simple design and facile tunability.

quote

GB/T 7714-2015 [1] Fangqi Chen, Yanpei Tian, Xiaojie Liu, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00764.
MLA [1] Fangqi Chen, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00764.
APA [1] Fangqi Chen, Yanpei Tian, Xiaojie Liu, Andrew Caratenuto, & Yi Zheng. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00764
IEEE [1] Fangqi Chen, Yanpei Tian, Xiaojie Liu, Andrew Caratenuto, and Yi Zheng, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00764. keywords: {optical modulator;elastomer;mechanically induced;tunable optical transmittance;smart windows}