From Scratch Closure to Electrolyte Barrier Restoration in Self-Healing Polyurethane Coatings AITranslate

Delft University of Technology;Croda, Coatings & Polymers business;Croda, Coatings & Polymers business; Delft University of Technology; Delft University of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The effects of the soft block fraction and H-bond state in thermoplastic polyurethanes on autonomous entropy-driven scratch closure and barrier restoration are studied. To this aim, comparable polyurethanes with different segmentation states are applied as organic coatings on plain carbon steel plates, scratched under very well-controlled conditions, and the scratch closure and sealing kinetics are studied in detail. The scratch closure is measured optically, while the barrier restoration is probed by the accelerated cyclic electrochemical technique (ACET). Scratch closure, attributed to entropic elastic recovery (EER), is followed in a marked two-step process by barrier restoration governed by local viscous flow and the state of the interfacial hydrogen bonding. Polyurethanes with a lower soft phase fraction lead to a higher urea/urethane ratio, which in turn influences the healing efficiency of each healing step. Interestingly, softer polyurethanes leading to efficient crack closure were unable to sufficiently restore barrier properties. The present work highlights the critical role of the soft/hard block and urea/urethane H-bond state content on crack closure and barrier restoration of anticorrosive organic coatings and points at design rules for the design of more efficient corrosion-protective self-healing polyurethanes.

KeyWords AITranslate

selfhealing polymer selfhealing coating polyurethane polymer architecture urea ACET
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00323

Chinese Library Classification Number:

Citation Information:

The effects of the soft block fraction and H-bond state in thermoplastic polyurethanes on autonomous entropy-driven scratch closure and barrier restoration are studied. To this aim, comparable polyurethanes with different segmentation states are applied as organic coatings on plain carbon steel plates, scratched under very well-controlled conditions, and the scratch closure and sealing kinetics are studied in detail. The scratch closure is measured optically, while the barrier restoration is probed by the accelerated cyclic electrochemical technique (ACET). Scratch closure, attributed to entropic elastic recovery (EER), is followed in a marked two-step process by barrier restoration governed by local viscous flow and the state of the interfacial hydrogen bonding. Polyurethanes with a lower soft phase fraction lead to a higher urea/urethane ratio, which in turn influences the healing efficiency of each healing step. Interestingly, softer polyurethanes leading to efficient crack closure were unable to sufficiently restore barrier properties. The present work highlights the critical role of the soft/hard block and urea/urethane H-bond state content on crack closure and barrier restoration of anticorrosive organic coatings and points at design rules for the design of more efficient corrosion-protective self-healing polyurethanes.

quote

GB/T 7714-2015 [1] Vincenzo Montano, Wouter Vogel, Angela Smits, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00323.
MLA [1] Vincenzo Montano, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00323.
APA [1] Vincenzo Montano, Wouter Vogel, Angela Smits, Sybrand van der Zwaag, & Santiago J. Garcia. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00323
IEEE [1] Vincenzo Montano, Wouter Vogel, Angela Smits, Sybrand van der Zwaag, and Santiago J. Garcia, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00323. keywords: {selfhealing polymer;selfhealing coating;polyurethane;polymer architecture;urea;ACET}