Abstract AITranslate

Liquid phase sintering of mixed W--Cu powders is hampered'by the insolubi lity of tungsten in copper. In this study, the propertiesof the system are significant ly improved by addition of less than lwtqdCo to the starting powder mixture. The effects of process variablessuch as cobalt content, initial homogeneity, copper parcticle size.copper content, green blank density, heating rate, and sintering temperature are invest irated.

KeyWords AITranslate

W--Cu W--Cu--Co composite material liquid phasesintering powder metallurgy

1黄劲松,周继承,刘文胜,黄伯云.钨基高密度合金的烧结[J].粉末冶金材料科学与工程,2003,8(1):34-39. 被引量:7

2程继贵,吴玉程,夏永红,蒋阳,雷纯鹏.纳米W-Cu粉末的热机械化学法制备及其烧结性能研究[J].金属功能材料,2005,12(2):12-15. 被引量:4

3王玉金,宋桂明,周玉,雷廷权.合金元素及第二相对钨的影响[J].宇航材料工艺,1998,28(5):11-18. 被引量:19

4徐凯.钨铜复合材料的现状与发展[J].中国钨业,2010,25(3):30-34. 被引量:19

5范志康,肖鹏,梁淑华,罗启文.钨粉粒径对熔渗法制备的CuW触头材料硬度的影响[J].电工材料,2001(3):5-7. 被引量:5

6黄劲松,周继承,黄伯云.元素及其化合物对钨基高密度合金性能的影响[J].稀有金属材料与工程,2004,33(5):454-458. 被引量:8

1马运柱,黄伯云,刘文胜.钨基合金材料的研究现状及其发展趋势[J].粉末冶金工业,2005,15(5):46-54. 被引量:23

2叶途明,易健宏,李丽娅,彭元东,吕豫湘,胡礼福.高密度钨合金研究的新进展[J].粉末冶金材料科学与工程,2003,8(2):134-140. 被引量:7

3李倩,宋月鹏,高东升,李江涛,孙祥鸣,Kim Hyoungseop.超重力熔铸W/Cu复合材料温度及应力场的仿真[J].材料热处理学报,2013,34(S2):227-232. 被引量:2

4陈德欣,王志法,张行健,张瑾瑾.钨粉粒径对W-15Cu导热性能的影响[J].稀有金属与硬质合金,2005,33(2):16-18. 被引量:9

5晏建武,周继承,鲁世强,陈同彩,郭浩.碳/Me(Co,RE)对W-Ni-Fe高密度合金性能和显微组织的影响[J].南昌航空工业学院学报,2005,19(1):40-44. 被引量:2

6杨林,栾道成,吴小刚.热压烧结法制备钨铜复合材料的工艺研究[J].西华大学学报:自然科学版,2005,24(6):98-101. 被引量:13

7黄冬根,廖世军,党志.钨精矿中杂质元素ICP-MS测定方法的研究[J].稀有金属材料与工程,2006,35(2):333-336. 被引量:9

8张存信,秦丽柏,米文宇,白志国.我国穿甲弹用钨合金研究的最新进展与展望[J].粉末冶金材料科学与工程,2006,11(3):127-132. 被引量:45

9甘乐,张保红.钨粉粒度及预混合原料配比对渗铜方法制备W-Cu合金性能的影响[J].粉末冶金工业,2006,16(4):21-25. 被引量:1

10金永中,刘东亮,孙亚丽,杨晓青,李志翔.稀土元素镧对97W-Ni-Fe合金性能的影响[J].中国钨业,2007,22(2):34-36. 被引量:1

1贾成厂,金雪华,赵军,解子章.用机械活化与化学活化方法制备W-Cu合金[J].粉末冶金技术,2001,19(3):148-152. 被引量:16

2贾成厂,刘小扬,解子章,赵军.用机械活化粉末制备钨合金[J].清华大学学报:自然科学版,1999,39(6):35-38. 被引量:16

3John.,JL,陈安庆.化学活化液相烧结钨—铜合金[J].钨钼材料,1995(1):55-62.

4温树德.钨-铜化学活化液相烧结[J].国外金属热处理,1998,19(4):44-48. 被引量:3

5S.St-Laurent,寸南.温压时钢粉末混合物的若干现象[J].重庆钢研,2000(25):65-69.

6А.,ВВ,张文成.加热TiC—TiNi粉末混合物过程的热分析和热重分析[J].钒钛,1990(1):64-64.

7刘曼朗.专利信息[J].粉末冶金工业,2017,27(2):80-80.

8宋旭艳,韩静云,郜志海.化学活化烟气灰的活性评价及火山灰效应研究[J].材料导报,2010,24(16):76-79. 被引量:2

9住友金属开发新的保护渣 改善亚包晶钢的表面质量[J].涟钢科技与管理,2005(1):35-35.

10许孙曲.用机械化学处理氟碳铈矿提取稀土的非高温工艺[J].稀土信息,1998,4(12):12-12.

Basic Information:

DOI:

Chinese Library Classification Number:TF124.54[冶金工程—粉末冶金]

Citation Information:

Liquid phase sintering of mixed W--Cu powders is hampered'by the insolubi lity of tungsten in copper. In this study, the propertiesof the system are significant ly improved by addition of less than lwtqdCo to the starting powder mixture. The effects of process variablessuch as cobalt content, initial homogeneity, copper parcticle size.copper content, green blank density, heating rate, and sintering temperature are invest irated.

quote

GB/T 7714-2015 [1] HUANG Jin-chang, XU Xiu-ru. Chemically Activated Liquid Phase Sintering of Tungsten-copper[J]. Rare Metals and Cemented Carbides, 1996(4): 59-64.
MLA [1] HUANG Jin-chang, and XU Xiu-ru. "Chemically Activated Liquid Phase Sintering of Tungsten-copper." Rare Metals and Cemented Carbides, no. 4, 1996, pp. 59-64.
APA [1] HUANG Jin-chang, & XU Xiu-ru. (1996). Chemically Activated Liquid Phase Sintering of Tungsten-copper. Rare Metals and Cemented Carbides(4), 59-64.
IEEE [1] HUANG Jin-chang and XU Xiu-ru, "Chemically Activated Liquid Phase Sintering of Tungsten-copper," Rare Metals and Cemented Carbides, no. 4, pp. 59-64, 1996. keywords: {W--Cu, W--Cu--Co, composite material, liquid phasesintering, powder metallurgy}