Highly Efficient Blue Perovskite Quantum Dots Light-Emitting Diodes Based on Ligand-Assisted Anion Exchange Method Highly Efficient Blue Perovskite Quantum Dots Light-Emitting Diodes Based on Ligand-Assisted Anion Exchange Method AITranslate
Abstract AITranslate
High-performance blue perovskite quantum dots (PQDs) are of key importance for electroluminescent light-emitting diodes (LEDs) toward full color display in the future. Here, mixed halogen PQDs CsPb(Brx/Cl1–x)3 with a tunable emission wavelength was obtained through a strategy of ligand-assisted anion exchange assisted by didodecydimethyammonium chloride (DDAC) ligand. Surface Br– vacancies of the PQD are passivated by the halogen atoms in the anchored DDAC ligand, enabling a high efficiency emission of blue light from the PQD. Stable anchoring of the ligand also improves the robustness of the PQD during its purification in weak polar solvents. Well-controlled chlorine stoichiometry of the PQD also allows fine-tuning of its photoluminescence and electroluminescence spectra in the range of 424–514 nm and 453–500 nm. The external quantum efficiency of the fabricated PQDs LED device reaches 10.1% at 495 nm, 6.5% at 484 nm, and 5.1% at 470 nm (NTSC pure blue) under a constant current test. Our work provides a facile method without additional purification or ligand separation to achieve highly efficient blue PQDs with a tunable emission wavelength, promoting the advance of blue PQDs LED.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.3c00396
Chinese Library Classification Number:
Citation Information:
High-performance blue perovskite quantum dots (PQDs) are of key importance for electroluminescent light-emitting diodes (LEDs) toward full color display in the future. Here, mixed halogen PQDs CsPb(Brx/Cl1–x)3 with a tunable emission wavelength was obtained through a strategy of ligand-assisted anion exchange assisted by didodecydimethyammonium chloride (DDAC) ligand. Surface Br– vacancies of the PQD are passivated by the halogen atoms in the anchored DDAC ligand, enabling a high efficiency emission of blue light from the PQD. Stable anchoring of the ligand also improves the robustness of the PQD during its purification in weak polar solvents. Well-controlled chlorine stoichiometry of the PQD also allows fine-tuning of its photoluminescence and electroluminescence spectra in the range of 424–514 nm and 453–500 nm. The external quantum efficiency of the fabricated PQDs LED device reaches 10.1% at 495 nm, 6.5% at 484 nm, and 5.1% at 470 nm (NTSC pure blue) under a constant current test. Our work provides a facile method without additional purification or ligand separation to achieve highly efficient blue PQDs with a tunable emission wavelength, promoting the advance of blue PQDs LED.
quote
| GB/T 7714-2015 | [1] Zhiyong Lei, Min Wang, XiaoDong Zhang, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00396. |
| MLA | [1] Zhiyong Lei, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00396. |
| APA | [1] Zhiyong Lei, Min Wang, XiaoDong Zhang, Kun Cao, Zhaojie Wang, Yanwei Wen, & Rong Chen. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00396 |
| IEEE | [1] Zhiyong Lei, Min Wang, XiaoDong Zhang, Kun Cao, Zhaojie Wang, Yanwei Wen, and Rong Chen, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00396. keywords: {blue perovskite quantum dots lightemitting diodes passivation anion exchange external quantum efficiency tunable emissionShow More} |