Giant Photoluminescence Enhancement in CsPbCl3 Perovskite Nanocrystals by Simultaneous Dual-Surface Passivation AITranslate

King Abdullah University of Science and Technology (KAUST); King Abdullah University of Science and Technology (KAUST); King Abdullah University of Science and Technology (KAUST); King Abdullah University of Science and Technology (KAUST); King Abdullah University of Science and Technology (KAUST); King Abdullah University of Science and Technology (KAUST); King Abdullah University of Science and Technology (KAUST); King Abdullah University of Science and Technology (KAUST); King Abdullah University of Science and Technology (KAUST); King Abdullah University of Science and Technology (KAUST)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The presence of localized trap states on the surface of CsPbCl3 perovskite nanocrystals (NCs) is one of the greatest challenges precluding the development of optoelectronic applications of these NCs. Passivation of these defect sites provides a promising pathway to remediating their electronic and optical properties, such as the photoluminescence quantum yield (PLQY). Herein, we demonstrate a postsynthetic dual-surface treatment using trivalent metal ion salts, i.e., YCl3, as a new passivation approach that enhances the PLQY up to 60% while preserving the NC size and crystal structure. Such remarkable enhancement of the PLQY along with prolongation of the average PL lifetimes of treated NCs samples indicates effective passivation of the surface defects and subsequent suppression of the formation of surface nonradiative recombination centers. As a segue toward optoelectronic applications, we probed the photoelectric performance of the NCs using ultraflexible devices; we found that YCl3-treated CsPbCl3 NC films exhibit an order of magnitude larger photocurrent compared to their nontreated counterparts. Our experimental and theoretical results provide an insightful understanding of the effective passivating roles of Y3+ and Cl– ions on the surface of CsPbCl3 NCs, as well as offering a new path to synthesize high-quality NCs for UV light conversion applications.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b01441

Chinese Library Classification Number:

Citation Information:

The presence of localized trap states on the surface of CsPbCl3 perovskite nanocrystals (NCs) is one of the greatest challenges precluding the development of optoelectronic applications of these NCs. Passivation of these defect sites provides a promising pathway to remediating their electronic and optical properties, such as the photoluminescence quantum yield (PLQY). Herein, we demonstrate a postsynthetic dual-surface treatment using trivalent metal ion salts, i.e., YCl3, as a new passivation approach that enhances the PLQY up to 60% while preserving the NC size and crystal structure. Such remarkable enhancement of the PLQY along with prolongation of the average PL lifetimes of treated NCs samples indicates effective passivation of the surface defects and subsequent suppression of the formation of surface nonradiative recombination centers. As a segue toward optoelectronic applications, we probed the photoelectric performance of the NCs using ultraflexible devices; we found that YCl3-treated CsPbCl3 NC films exhibit an order of magnitude larger photocurrent compared to their nontreated counterparts. Our experimental and theoretical results provide an insightful understanding of the effective passivating roles of Y3+ and Cl– ions on the surface of CsPbCl3 NCs, as well as offering a new path to synthesize high-quality NCs for UV light conversion applications.

quote

GB/T 7714-2015 [1] Ghada H. Ahmed, Jehad K. ElDemellawi, Jun Yin, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b01441.
MLA [1] Ghada H. Ahmed, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b01441.
APA [1] Ghada H. Ahmed, Jehad K. ElDemellawi, Jun Yin, Jun Pan, Dhinesh Babu Velusamy, Mohamed Nejib Hedhili, Erkki Alarousu, Osman M. Bakr, Husam N. Alshareef, & Omar F. Mohammed. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b01441
IEEE [1] Ghada H. Ahmed, Jehad K. ElDemellawi, Jun Yin, Jun Pan, Dhinesh Babu Velusamy, Mohamed Nejib Hedhili, Erkki Alarousu, Osman M. Bakr, Husam N. Alshareef, and Omar F. Mohammed, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b01441.