The blank roasting process and kinetics of power generation ash from vanadium phosphate ore were studied.The results show that in the ash,vanadium mainly exists in the form of vanadium mica,predominately in the V3+.The optimum process parameters for the blank roasting of the ash are as follows:grinding 90%of the ash to a fineness of-0.074 mm before roasting and then roasting the ash at 880~900℃for 16 h,the leaching rate of V2O_5 reaches approximately 71%.The blank roasting of the ash is controlled by interfacial chemical reaction,with an apparent activation energy of 89.75 kJ/mol and a kinetic equation of 1-(1-x)1/3=114.47exp[-89750/(RT)]t.
KeyWords AITranslate
1侯帅,田颖,李运刚.金属钒制备方法的研究进展[J].稀有金属与硬质合金,2022,50(6):22-26. 被引量:5
2崔文婧.我国钒矿资源开发利用现状及建议[J].合作经济与科技,2019,0(11):54-56. 被引量:20
3曾凌云.我国钒矿资源开采形势分析与建议[J].世界有色金属,2020,45(16):80-81. 被引量:4
4李丽洁,石美莲,华骏,颜文斌,高峰,黄超.二氧化锰氧化浸出石煤钒矿动力学研究[J].稀有金属与硬质合金,2020,48(6):24-29. 被引量:3
5李龙涛,曾伟强,施正伦,蒋啸,祝培旺.高碳石煤循环流化床焙烧灰渣酸浸提钒试验研究[J].稀有金属,2014,38(1):123-129. 被引量:8
6朱军,刘欢,齐建云,卫琛浩.某低热值石煤钒矿配煤燃烧灰渣酸浸提钒的研究[J].稀有金属与硬质合金,2015,43(1):10-14. 被引量:3
7郑祥明,田学达,张小云,石华,邓益强.湿法提取石煤中钒的新工艺研究[J].湘潭大学自然科学学报,2003,25(1):43-45. 被引量:40
8李龙涛,祝培旺,施正伦,蒋啸,曾伟强.云母型含钒石煤灰渣空白焙烧提钒试验研究[J].稀有金属,2014,38(3):480-486. 被引量:12
1王淼,温建康,李文娟,杨鑫龙,赖永传,杨洪英.选冶联合回收石煤中伴生战略金属钒镍钼的研究进展[J].稀有金属,2023,47(6):881-892. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TF841.3[冶金工程—有色金属冶金]
Citation Information:
The blank roasting process and kinetics of power generation ash from vanadium phosphate ore were studied.The results show that in the ash,vanadium mainly exists in the form of vanadium mica,predominately in the V3+.The optimum process parameters for the blank roasting of the ash are as follows:grinding 90%of the ash to a fineness of-0.074 mm before roasting and then roasting the ash at 880~900℃for 16 h,the leaching rate of V2O_5 reaches approximately 71%.The blank roasting of the ash is controlled by interfacial chemical reaction,with an apparent activation energy of 89.75 kJ/mol and a kinetic equation of 1-(1-x)1/3=114.47exp[-89750/(RT)]t.
quote
| GB/T 7714-2015 | [1] GUO Shuan-quan, NIU Fang-yin, KANG Min, et al. Study on Blank Roasting Process and Kinetics of Power Generation Ash from Vanadium Phosphate Ore[J]. Rare Metals and Cemented Carbides, 2024(2): 6-10. |
| MLA | [1] GUO Shuan-quan, et al., "Study on Blank Roasting Process and Kinetics of Power Generation Ash from Vanadium Phosphate Ore." Rare Metals and Cemented Carbides, no. 2, 2024, pp. 6-10. |
| APA | [1] GUO Shuan-quan, NIU Fang-yin, KANG Min, GUO Mei, NING Xin-xia, & XING Xiang-dong. (2024). Study on Blank Roasting Process and Kinetics of Power Generation Ash from Vanadium Phosphate Ore. Rare Metals and Cemented Carbides(2), 6-10. |
| IEEE | [1] GUO Shuan-quan, NIU Fang-yin, KANG Min, GUO Mei, NING Xin-xia, and XING Xiang-dong, "Study on Blank Roasting Process and Kinetics of Power Generation Ash from Vanadium Phosphate Ore," Rare Metals and Cemented Carbides, no. 2, pp. 6-10, 2024. keywords: {vanadium phosphate ore;power generation ash;blank roasting;vanadium leaching;apparent reac-tiona ctivation energy;kinetic equation} |