Effect of Carbon Content on Microstructure and Properties of WC-3Co-3Ni Coarse Grained Cemented Carbide AITranslate

Zhuzhou Cemented Carbide Group Co.,Ltd.;Zhuzhou Cemented Carbide Group Co.,Ltd.;Zhuzhou Cemented Carbide Group Co.,Ltd.;Zhuzhou Cemented Carbide Group Co.,Ltd.;Zhuzhou Cemented Carbide Group Co.,Ltd.;Zhuzhou Cemented Carbide Group Co.,Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In order to explore the effect of carbon content on the microstructure and properties of coarse grained cemented carbide with Co-Ni composite binder phase, the change rules of microstructure and pro-perties of WC-3 Co-3 Ni coarse grained cemented carbides with different carbon contents were studied by optical microscope, Rockwell hardness tester, coercivity tester and cobalt magnetometer.The results show that the coercive force of alloy increases with the increase of ball milling time, and reaches its maximum value when the ball milling time reaches 22 h.With the increase of carbon content, the WC grain morpho-logy is more angular, the dissolution-precipitation process makes WC grains coarser, the bending strength increases and the hardness decreases.When the milling time is prolonged, the increase of hardness caused by the decrease of carbon content is greater than that caused by the increase of carbon content.

KeyWords AITranslate

coarse grained cemented carbide carbon content ball milling time Co-Ni composite binder phase microstructure property

1莫盛秋,程继贵,王华林.真空烧结低钴粗晶硬质合金及其性能的研究[J].合肥工业大学学报:自然科学版,2000,23(2):294-297. 被引量:7

2龙坚战,陆必志,易茂中,陈飞.新型粘结相硬质合金的研究进展[J].硬质合金,2015,32(3):204-212. 被引量:26

3羊求民,羊建高,陈丽勇,陈颢,唐彦渊.硬质合金粘结相研究进展[J].稀有金属与硬质合金,2019,47(2):82-86. 被引量:11

4何平.WC-Co-Ni硬质合金的微观组织和断裂强度[J].粉末冶金技术,1996,14(4):287-290. 被引量:2

5刘寿荣.WC-Co硬质合金的强度[J].硬质合金,2002,19(3):129-135. 被引量:36

6张卫兵.WC、Co质量对超细硬质合金性能影响的研究[J].硬质合金,2003,20(3):157-160. 被引量:35

7张立,孙宝琦,王柏连.WC-11(Co-Ni)硬质合金抗压强度的研究[J].稀有金属与硬质合金,1993,21(2):26-28. 被引量:2

8周新华,王力民,赵声志,肖可俊.碳含量对粗晶硬质合金性能的影响[J].硬质合金,2009,26(2):82-86. 被引量:13

9陈明,吝楠,贺跃辉.碳含量对WC-Co-Ni-Fe-Cr硬质合金组织与性能的影响[J].硬质合金,2019,36(6):434-439. 被引量:4

10董凯林,时凯华,江庆,周科朝.碳含量对WC-6%Ni细晶硬质合金组织结构及性能的影响[J].硬质合金,2013,30(4):190-196. 被引量:10

1陈振磊,喻琛,邵鸣宇.不同粘结相硬质合金的研究进展[J].机械研究与应用,2021,34(5):204-209. 被引量:2

2唐彦渊,钟志强,羊求民,王红云,徐国钻.碳含量对WC-10Co硬质合金微观组织及力学性能的影响[J].稀有金属与硬质合金,2021,49(6):73-78. 被引量:6

3邝宏有,戴炳蔚,吴育藩.WC-11%(Ti,W)(Ta,Nb)C-11%Co合金制取过程中碳量和球磨时间的优化[J].硬质合金,2022,39(2):111-117.

4罗威,杨诚辉,陈邦明,钟志强,唐彦渊.高频燃烧红外吸收法测定碳化钨粉总碳量[J].硬质合金,2022,39(6):490-494.

1倪莹驰,江佳阳,董凯林,时凯华.不同添加剂对(W,Mo)C-6%Ni合金性能的影响[J].硬质合金,2022,39(2):118-126.

2张云龙,牛楚涵,牛广津,张宇民,李启荣,高志杨,张唯一.La_(2)O_(3)掺杂量对WC-12Co硬质合金微观结构和硬度的影响[J].中国钨业,2022,37(2):53-59.

3罗威,杨诚辉,陈邦明,钟志强,唐彦渊.高频燃烧红外吸收法测定碳化钨粉总碳量[J].硬质合金,2022,39(6):490-494.

4孙化鑫,徐淑波,李辉,郑君姿,卢庆亮.Ni含量对WC-Co-Ni硬质合金的力学性能和耐腐蚀性能的影响[J].稀有金属与硬质合金,2022,50(6):77-82.

5胡启明,廖宇.贫碳WC-12%(Co+Ni)硬质合金微观组织与性能[J].硬质合金,2023,40(1):66-72.

6秦永强,袁健,罗来马,田宇,彭宇强,吴玉程.热处理对Y_(2)O_(3)掺杂WC-Co硬质合金显微组织及性能的影响[J].材料热处理学报,2023,44(4):40-46.

7江佳阳,廖军,顾金宝,梁靖岳.WC粒度、配碳量对WC-9%Ni硬质合金组织与性能的影响[J].硬质合金,2023,40(4):288-295.

1向新,董定乾,顾金宝,杨伟,谌理飞,时凯华,赵易.双尺度结构WC-6%Co硬质合金球磨工艺研究[J].稀有金属与硬质合金,2021,49(2):82-89. 被引量:2

2杨广宇,陈靖海,刘楠,杨坤,贾亮,贾文鹏,王建,汤慧萍.基于预合金粉末原料的粉床型电子束增材制造W-Ni-Fe-Co合金研究[J].稀有金属材料与工程,2020,49(11):3865-3869. 被引量:1

3赵超,曲召波.新疆东昆仑玉苏普阿勒克塔格地区航磁异常特征及成矿潜力分析[J].世界有色金属,2021(4):177-178.

4羌俊杰,许宏宇,倪鸿,余斌,汪振华.基于TiAl-xCo-Mo-Ni复合粘结相的WC基超细晶硬质合金微观组织和力学性能研究[J].稀有金属与硬质合金,2021,49(2):69-75. 被引量:2

5杨海欧,张书亚,林鑫,胡云龙,黄卫东.工艺参数对激光立体成形Inconel 625合金沉积特征的影响[J].中南大学学报:英文版,2021,28(4):1003-1014. 被引量:1

6卢金德,韦春贝,林松盛,张佳平,李浩宇,李助军,刘怡飞,代明江,李风,刘敏.磁控溅射NiCrAlY/MoS_(2)复合薄膜结构与性能研究[J].表面技术,2021,50(5):198-207. 被引量:2

7于娟,陆政,鲁原,熊艳才,李国爱,冯朝辉,郝时嘉.中间形变热处理对2A97铝锂合金组织和性能的影响[J].材料工程,2021,49(5):130-136. 被引量:4

Basic Information:

DOI:

Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程]

Citation Information:

In order to explore the effect of carbon content on the microstructure and properties of coarse grained cemented carbide with Co-Ni composite binder phase, the change rules of microstructure and pro-perties of WC-3 Co-3 Ni coarse grained cemented carbides with different carbon contents were studied by optical microscope, Rockwell hardness tester, coercivity tester and cobalt magnetometer.The results show that the coercive force of alloy increases with the increase of ball milling time, and reaches its maximum value when the ball milling time reaches 22 h.With the increase of carbon content, the WC grain morpho-logy is more angular, the dissolution-precipitation process makes WC grains coarser, the bending strength increases and the hardness decreases.When the milling time is prolonged, the increase of hardness caused by the decrease of carbon content is greater than that caused by the increase of carbon content.

quote

GB/T 7714-2015 [1] MENG Xiang-jun, TANG Jun, LONG Jian-zhan, et al. Effect of Carbon Content on Microstructure and Properties of WC-3Co-3Ni Coarse Grained Cemented Carbide[J]. Rare Metals and Cemented Carbides, 2021(2): 63-68.
MLA [1] MENG Xiang-jun, et al., "Effect of Carbon Content on Microstructure and Properties of WC-3Co-3Ni Coarse Grained Cemented Carbide." Rare Metals and Cemented Carbides, no. 2, 2021, pp. 63-68.
APA [1] MENG Xiang-jun, TANG Jun, LONG Jian-zhan, LU Bi-zhi, GUO Zhong-wei, & ZHOU Xin-hua. (2021). Effect of Carbon Content on Microstructure and Properties of WC-3Co-3Ni Coarse Grained Cemented Carbide. Rare Metals and Cemented Carbides(2), 63-68.
IEEE [1] MENG Xiang-jun, TANG Jun, LONG Jian-zhan, LU Bi-zhi, GUO Zhong-wei, and ZHOU Xin-hua, "Effect of Carbon Content on Microstructure and Properties of WC-3Co-3Ni Coarse Grained Cemented Carbide," Rare Metals and Cemented Carbides, no. 2, pp. 63-68, 2021. keywords: {coarse grained cemented carbide;carbon content;ball milling time;Co-Ni composite binder phase;microstructure;property}