Experimental Research on Stainless Steel Drilling with Ultrafine-grained Cemented Carbide Micro-drill AITranslate
Abstract AITranslate
Two kinds of ultrafine-grained WC-Co cemented carbides were chosen to fabricate micro-drills,and then 0Cr18Ni9 stainless steel was drilled with the fabricated micro-drills.The wear of micro-drills was observed and analyzed,and their working life was measured.The results show that for the micro-drills,the finer WC grains,the slower wear speed and the longer working life.Grain refinement is helpful for reducing chipping and breakage of the micro-drills during micro-drilling.
KeyWords AITranslate
1徐兰英,叶邦彦,伍强,王伟文,梁忠伟.奥氏体不锈钢小孔钻削机理研究(英文)[J].科学技术与工程,2008,8(23):6344-6348. 被引量:4
2李宁,龙坚战,周永贵,张勇.超细WC-Co硬质合金的组织与性能特征[J].硬质合金,2005,22(2):107-111. 被引量:10
3梁洁萍,周知进.微小孔加工与微细钻头[J].湘潭师范学院学报:自然科学版,2004,26(4):56-58. 被引量:11
4Xiaoguang Sun,You Wang,D.Y. Li.Mechanical properties and erosion resistance of ceria nano-particle-doped ultrafine WC–12Co composite prepared by spark plasma sintering[J]. Wear . 2013 (1-2)
5C Lin,S Kang,,K F.Helical micro—drill point design and grinding. Manufacturing Science and Engineering ASKE . 1995
1于启勋.现代刀具材料系列讲座(五)——新型硬质合金──细晶粒与超细晶粒硬质合金和Ti(C,N)与TiC基硬质合金[J].机械工程师,2001(5):58-60. 被引量:2
2硬质合金刀具在加工合金钢中的应用[J].模具工程,2006(10):53-53. 被引量:1
3凌平.超细晶粒硬质合金的钎焊方法[J].硬质合金,1997,14(4):240-241. 被引量:8
4杜.加工小直径端面的微型切槽刀[J].工具展望,2005(1):24-24.
5И.В.科比茨科依,唐丹,李沐山.添加难熔金属(Cr和V)碳化物的WC—Co类超细晶粒硬质合金的研究[J].国外难熔金属与硬质材料,1999,15(1):19-21. 被引量:3
6王文光.超细晶粒硬质合金的特点及用途[J].工具展望,1998(4):8-10. 被引量:1
7刘战强,万熠,周军.高速切削刀具材料及其应用[J].机械工程材料,2006,30(5):1-4. 被引量:30
8佘建芳.德国维迪阿公司超细硬质合金的发展[J].稀有金属与硬质合金,2002,30(2):55-58. 被引量:6
9陶小平.超细晶粒硬质合金生产工艺条件探讨[J].江西冶金,1990,10(6):9-11. 被引量:2
10邱健,詹友基,贾敏忠.陶瓷结合剂金刚石砂轮磨削超细晶粒硬质合金的表面粗糙度研究[J].工具技术,2014,48(9):20-24. 被引量:10
Basic Information:
DOI:
Chinese Library Classification Number:TG52[金属学及工艺—金属切削加工及机床]
Citation Information:
Two kinds of ultrafine-grained WC-Co cemented carbides were chosen to fabricate micro-drills,and then 0Cr18Ni9 stainless steel was drilled with the fabricated micro-drills.The wear of micro-drills was observed and analyzed,and their working life was measured.The results show that for the micro-drills,the finer WC grains,the slower wear speed and the longer working life.Grain refinement is helpful for reducing chipping and breakage of the micro-drills during micro-drilling.
quote
| GB/T 7714-2015 | [1] ZHANG Hao-qiang, WANG Xi-bin, PANG Si-qin, et al. Experimental Research on Stainless Steel Drilling with Ultrafine-grained Cemented Carbide Micro-drill[J]. Rare Metals and Cemented Carbides, 2015(3): 63-66. |
| MLA | [1] ZHANG Hao-qiang, et al., "Experimental Research on Stainless Steel Drilling with Ultrafine-grained Cemented Carbide Micro-drill." Rare Metals and Cemented Carbides, no. 3, 2015, pp. 63-66. |
| APA | [1] ZHANG Hao-qiang, WANG Xi-bin, PANG Si-qin, LI Shen-wang, & CHENG Jian-bing. (2015). Experimental Research on Stainless Steel Drilling with Ultrafine-grained Cemented Carbide Micro-drill. Rare Metals and Cemented Carbides(3), 63-66. |
| IEEE | [1] ZHANG Hao-qiang, WANG Xi-bin, PANG Si-qin, LI Shen-wang, and CHENG Jian-bing, "Experimental Research on Stainless Steel Drilling with Ultrafine-grained Cemented Carbide Micro-drill," Rare Metals and Cemented Carbides, no. 3, pp. 63-66, 2015. keywords: {ultrafine-grained cemented carbide;mechanical property;micro-drilling;stainless steel} |