Feature based three axes computer aided manufacturing software for wire arc additive manufacturing dedicated to thin walled components AITranslate

University of Firenze; University of Firenze; University of Firenze; University of Firenze; University of Firenze
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

WAAM (Wire-Arc-Additive-Manufacturing) is a metal additive manufacturing process using arc welding to create large components with high deposition rate. The workpiece quality and the process productivity are strongly dependent both on the process parameters (wire feed speed, voltage and current) and on the selected deposition path. Currently, the CAM (Computer-Aided-Manufacturing) software dedicated to WAAM rely on a multi-pass strategy to create the component layers, i.e. each layer is built overlapping multiple welding passes. However, since WAAM can create wide layers, a single pass strategy can improve the process efficiency when dealing with thin walled components. This paper proposes CAM software dedicated to WAAM, using a single pass strategy. The proposed solution uses a midsurface representation of the workpiece as input, to generate the deposition toolpath. A feature recognition module is proposed, to identify the critical features of the part, such as free end walls, t-crossings, direct-crossings and isolated tubulars. A specific strategy is developed and proposed for each one of the selected features, with the aim of minimizing the geometrical errors and to ensure the required machining allowances for the subsequent finishing operations. The effectiveness of the proposed strategy is verified manufacturing a test case.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.addma.2018.06.013

Chinese Library Classification Number:

Citation Information:

WAAM (Wire-Arc-Additive-Manufacturing) is a metal additive manufacturing process using arc welding to create large components with high deposition rate. The workpiece quality and the process productivity are strongly dependent both on the process parameters (wire feed speed, voltage and current) and on the selected deposition path. Currently, the CAM (Computer-Aided-Manufacturing) software dedicated to WAAM rely on a multi-pass strategy to create the component layers, i.e. each layer is built overlapping multiple welding passes. However, since WAAM can create wide layers, a single pass strategy can improve the process efficiency when dealing with thin walled components. This paper proposes CAM software dedicated to WAAM, using a single pass strategy. The proposed solution uses a midsurface representation of the workpiece as input, to generate the deposition toolpath. A feature recognition module is proposed, to identify the critical features of the part, such as free end walls, t-crossings, direct-crossings and isolated tubulars. A specific strategy is developed and proposed for each one of the selected features, with the aim of minimizing the geometrical errors and to ensure the required machining allowances for the subsequent finishing operations. The effectiveness of the proposed strategy is verified manufacturing a test case.

quote

GB/T 7714-2015 [1] Giuseppe Venturini, Filippo Montevecchi, Francesco Bandini, et al. Additive Manufacturing, 2018(22). DOI:10.1016/j.addma.2018.06.013.
MLA [1] Giuseppe Venturini, et al., Additive Manufacturing, no. 22, 2018, https://doi.org/10.1016/j.addma.2018.06.013.
APA [1] Giuseppe Venturini, Filippo Montevecchi, Francesco Bandini, Antonio Scippa, & Gianni Campatelli. (2018). Additive Manufacturing(22). https://doi.org/10.1016/j.addma.2018.06.013
IEEE [1] Giuseppe Venturini, Filippo Montevecchi, Francesco Bandini, Antonio Scippa, and Gianni Campatelli, Additive Manufacturing, no. 22, 2018, doi: 10.1016/j.addma.2018.06.013.