Enhancement of Columbic Efficiency and Capacity of Li-Ion Batteries using a Boron Nitride Nanotubes-Dispersed-Electrolyte with High Ionic Conductivity AITranslate

R&D Center, NAiEEL Technology;R&D Center, NAiEEL Technology; Chungnam National University;R&D Center, NAiEEL Technology;R&D Center, NAiEEL Technology;R&D Center, NAiEEL Technology;R&D Center, NAiEEL Technology; Chungnam National University; Chungnam National University; Korea Institute of Energy Technology;R&D Center, NAiEEL Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Carbon nanotubes (CNT) are currently used as conductive additives for the electrodes to enhance the capacity of the lithium-ion batteries (LIBs), and we herein for the first time demonstrate the feasibility of boron nitride nanotubes (BNNT) as an electrolyte additive for lithium ion batteries (LIBs). The 0.9 wt % BNNT electrolyte yielded enhanced Li-ion conductivity up to 30% (∼0.87 mS/cm) and a much higher Li-ion transference number (∼0.73) compared to electrolytes without BNNT. The BNNT dispersed electrolyte (1 M LiPF6 in ethylene carbonate/dimethyl carbonate) prepared via sonication serves as a new electrolyte formulation, together with the NCM622//graphite full cell, and exhibits the highest reversible capacities of 153 mAh/g at 1 C and excellent cyclic retention over 500 cycles at high 10 C with a specific capacity of 71.5 mAh/g and a Coulombic efficiency of 99.6% compared to 125.3 mAh/g at 1 C and 40 mAh/g at 10 C with only 97.5% Coulombic efficiency without BNNT, respectively. Overall, we suggest BNNT as a new class of functional electrolyte material that resolves the major limitations of conventional carbonate-based electrolytes and is compatible for different electrolytes/electrode materials aimed at practical implementations for current as well as advanced LIBs.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.3c00538

Chinese Library Classification Number:

Citation Information:

Carbon nanotubes (CNT) are currently used as conductive additives for the electrodes to enhance the capacity of the lithium-ion batteries (LIBs), and we herein for the first time demonstrate the feasibility of boron nitride nanotubes (BNNT) as an electrolyte additive for lithium ion batteries (LIBs). The 0.9 wt % BNNT electrolyte yielded enhanced Li-ion conductivity up to 30% (∼0.87 mS/cm) and a much higher Li-ion transference number (∼0.73) compared to electrolytes without BNNT. The BNNT dispersed electrolyte (1 M LiPF6 in ethylene carbonate/dimethyl carbonate) prepared via sonication serves as a new electrolyte formulation, together with the NCM622//graphite full cell, and exhibits the highest reversible capacities of 153 mAh/g at 1 C and excellent cyclic retention over 500 cycles at high 10 C with a specific capacity of 71.5 mAh/g and a Coulombic efficiency of 99.6% compared to 125.3 mAh/g at 1 C and 40 mAh/g at 10 C with only 97.5% Coulombic efficiency without BNNT, respectively. Overall, we suggest BNNT as a new class of functional electrolyte material that resolves the major limitations of conventional carbonate-based electrolytes and is compatible for different electrolytes/electrode materials aimed at practical implementations for current as well as advanced LIBs.

quote

GB/T 7714-2015 [1] Dolly Yadav, JungHwan Jung, Yurim Lee, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.3c00538.
MLA [1] Dolly Yadav, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.3c00538.
APA [1] Dolly Yadav, JungHwan Jung, Yurim Lee, Thomas YouSeok Kim, Eunkwang Park, KiIn Choi, Jungho Cha, WooJin Song, JaeHak Choi, Seokgwang Doo, & Jaewoo Kim. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.3c00538
IEEE [1] Dolly Yadav, JungHwan Jung, Yurim Lee, Thomas YouSeok Kim, Eunkwang Park, KiIn Choi, Jungho Cha, WooJin Song, JaeHak Choi, Seokgwang Doo, and Jaewoo Kim, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.3c00538.