daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Design of a Boron-Containing PTHF-Based Solid Polymer Electrolyte for Sodium-Ion Conduction with High Na+ Mobility and Salt Dissociation AITranslate

Syracuse University; Syracuse University; Syracuse University; Syracuse University; Syracuse University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Solid polymer electrolytes based on semi-interpenetrating polymer networks (semi-IPNs) were developed for sodium-ion conduction using a boron-centered moiety with polytetrahydrofuran (PTHF) chains. The resulting solid polymer electrolytes (SPEs) combined the anion-trapping properties of the boron with the weakly coordinating PTHF to achieve enhanced salt dissociation and transference number. The structure of the polymer was confirmed by 1H NMR, 13C NMR, and 11B NMR, and the cross-linking reaction with hexamethylene diisocyanate (HMDI) was confirmed by Fourier transform infrared (FTIR) spectroscopy. The mechanical and thermal stabilities of the samples were evaluated, and FTIR spectroscopic analysis showed the efficiency of the boron centers in complexing with ClO4–. Dielectric studies also indicated the predominance of free Na+ in samples. The highest room-temperature ionic conductivity was delivered by boron-containing electrolytes with O/Na: 5, 7.54 × 10–5 S cm–1, and O/Na: 10, 1.13 × 10–5 S cm–1. Linear sweep voltammetry (LSV) revealed suitable electrochemical stability against Na metal, and the measured transference number was 0.88, confirming that electrolytes benefit from the looser coordination of Na+ ions with PTHF chains combined with the anion-trapping performance of boron moieties, indicating a potential direction in polymer electrolyte design.

KeyWords AITranslate

solid polymer electrolyte sodium lithium alternatives boron polytetrahydrofuran electrochemistry
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01276

Chinese Library Classification Number:

Citation Information:

Solid polymer electrolytes based on semi-interpenetrating polymer networks (semi-IPNs) were developed for sodium-ion conduction using a boron-centered moiety with polytetrahydrofuran (PTHF) chains. The resulting solid polymer electrolytes (SPEs) combined the anion-trapping properties of the boron with the weakly coordinating PTHF to achieve enhanced salt dissociation and transference number. The structure of the polymer was confirmed by 1H NMR, 13C NMR, and 11B NMR, and the cross-linking reaction with hexamethylene diisocyanate (HMDI) was confirmed by Fourier transform infrared (FTIR) spectroscopy. The mechanical and thermal stabilities of the samples were evaluated, and FTIR spectroscopic analysis showed the efficiency of the boron centers in complexing with ClO4–. Dielectric studies also indicated the predominance of free Na+ in samples. The highest room-temperature ionic conductivity was delivered by boron-containing electrolytes with O/Na: 5, 7.54 × 10–5 S cm–1, and O/Na: 10, 1.13 × 10–5 S cm–1. Linear sweep voltammetry (LSV) revealed suitable electrochemical stability against Na metal, and the measured transference number was 0.88, confirming that electrolytes benefit from the looser coordination of Na+ ions with PTHF chains combined with the anion-trapping performance of boron moieties, indicating a potential direction in polymer electrolyte design.

quote

GB/T 7714-2015 [1] Francielli Silva Genier, Shreyas Pathreeker, Paige Olufunmilayo Adebo, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c01276.
MLA [1] Francielli Silva Genier, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c01276.
APA [1] Francielli Silva Genier, Shreyas Pathreeker, Paige Olufunmilayo Adebo, Paul Chando, & Ian Dean Hosein. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c01276
IEEE [1] Francielli Silva Genier, Shreyas Pathreeker, Paige Olufunmilayo Adebo, Paul Chando, and Ian Dean Hosein, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c01276. keywords: {solid polymer electrolyte;sodium;lithium alternatives;boron;polytetrahydrofuran;electrochemistry}