daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Volumetric Determination of Tellurium in Commercial Metallic Tellurium and Tellurium-enriched Material AITranslate

Department of Biological Engineering and Environmental Science, Changsha College;School of Metallurgy and Environment, Central South University;Liuyang Yaguang High-tech Materials Co., Ltd.;Yongxing County Mayang Nonferrous Metals Co., Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Determination of high-content tellurium in commercial metallic tellurium and low-content tellur- ium in tellurium-enriched material was carried out by volumetric titration with potassium dichromate. The above method is suitable for tellurium determination of the materials containing 1 %-99.5 % tellurium.

KeyWords AITranslate

tellurium determination volumetric method potassium dichromate commercial metallic telluri- um tellurium-enriched material

1《有色金属工业分析丛书》编辑委员会.难熔金属和稀散金属冶金分析[M].北京:冶金工业出版社,1992.83.

2梁培德.硒碲合金中碲的测定[J].理化检验:化学分册,1989,25(2):54-55. 被引量:7

3沈广鑫,卢宏(英文翻译).重铬酸钾滴定法测定中和渣中的碲[J].江西冶金,2008,28(5):32-34. 被引量:9

4王冬珍.阳极泥及碲回收物料中高含量碲的测定[J].岩矿测试,2002,21(2):143-146. 被引量:14

5ГОСТ 9816. 1-84. Теллур технический-Метод опр- еделения теллура[S].

1武明丽.碲料中高含量碲的测定[J].广州化工,2014,42(13):116-117. 被引量:2

2万双,李先和.还原分离–硫酸亚铁铵返滴定法测定碲化铜中碲[J].化学分析计量,2018,27(6):11-15. 被引量:2

3万双,李先和,吕广颖,兰福荫.碲化铜中碲含量测定方法的精密度[J].化学分析计量,2019,28(5):93-98.

4黄兴德,李勇,赵思倩,吴久伟,官国英.氯化亚锡还原-分光光度法测定铅铋合金中痕量碲[J].冶金分析,2021,41(4):81-85. 被引量:1

1万双,李先和.还原分离–硫酸亚铁铵返滴定法测定碲化铜中碲[J].化学分析计量,2018,27(6):11-15. 被引量:2

2万双,李先和,吕广颖,兰福荫.碲化铜中碲含量测定方法的精密度[J].化学分析计量,2019,28(5):93-98.

3徐吉成,蒋艳,徐兵,张涛,邱凤仙.含碲溶液中选择性分离碲的研究进展[J].山东化工,2020,49(24):73-75. 被引量:2

4鲁海妍,谢海东,胡兰基,孔晓彦,刘玉川.湿法消解-电感耦合等离子体质谱法测定多金属矿中碲[J].桂林理工大学学报,2023,43(2):211-217.

1李良发.铜铁金属有机化合物中铜铁的容量测定法[J].理化检验:化学分册,1997,33(4):178-179. 被引量:1

2云作敏,苏丹,张丽娟.重铬酸钾容量法测定铁矿石中全铁的测量不确定度评定[J].长春工程学院学报:自然科学版,2012,13(1):78-79. 被引量:1

3刘璠.锌价难以走出震荡格局——4月份锌市场评述及后市展望[J].中国铅锌锡锑,2010(5):18-25.

4夏清华,黄永东,黄永川,付婷婷,周鑫兰,张伟.土壤有机质重铬酸钾容量法最佳测定条件的探索[J].南方农业,2014,8(6):35-37. 被引量:15

5今年镍价将延续升势[J].金川科技,2014(2):49-49.

6李俊超.重铬酸钾容量法的改进技术研究[J].科技创新导报,2017,14(3):69-70. 被引量:4

7何新锋.重铬酸钾容量法测定矾土中铁的改进[J].理化检验:化学分册,2000,36(7):321-321. 被引量:1

8袁圣华.全铁的测定—重铬酸钾容量法探讨[J].安徽地质,2010,20(1):56-57. 被引量:7

9世界顶级铂生产商[J].中国贵金属,2008(9):49-50.

10俄罗斯削减2009年铜铝镍产量[J].特种铸造及有色合金,2009(7):649-649.

Basic Information:

DOI:

Chinese Library Classification Number:O655.2[理学—分析化学]

Citation Information:

Determination of high-content tellurium in commercial metallic tellurium and low-content tellur- ium in tellurium-enriched material was carried out by volumetric titration with potassium dichromate. The above method is suitable for tellurium determination of the materials containing 1 %-99.5 % tellurium.

quote

GB/T 7714-2015 [1] CAO Dao-jin, ZHAO Hong, HUANG Li, et al. Volumetric Determination of Tellurium in Commercial Metallic Tellurium and Tellurium-enriched Material[J]. Rare Metals and Cemented Carbides, 2013(4): 62-63.
MLA [1] CAO Dao-jin, et al., "Volumetric Determination of Tellurium in Commercial Metallic Tellurium and Tellurium-enriched Material." Rare Metals and Cemented Carbides, no. 4, 2013, pp. 62-63.
APA [1] CAO Dao-jin, ZHAO Hong, HUANG Li, & ZHAO Qin-sheng. (2013). Volumetric Determination of Tellurium in Commercial Metallic Tellurium and Tellurium-enriched Material. Rare Metals and Cemented Carbides(4), 62-63.
IEEE [1] CAO Dao-jin, ZHAO Hong, HUANG Li, and ZHAO Qin-sheng, "Volumetric Determination of Tellurium in Commercial Metallic Tellurium and Tellurium-enriched Material," Rare Metals and Cemented Carbides, no. 4, pp. 62-63, 2013. keywords: {tellurium determination;volumetric method;potassium dichromate;commercial metallic telluri- um;tellurium-enriched material}