daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Atomic Oxygen Resistance Vitrimers with High Strength, Recyclability, and Thermal Stability AITranslate

College of Polymer Science and Engineering at Sichuan University; College of Polymer Science and Engineering at Sichuan University; College of Polymer Science and Engineering at Sichuan University; College of Polymer Science and Engineering at Sichuan University; College of Polymer Science and Engineering at Sichuan University; College of Polymer Science and Engineering at Sichuan University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Vitrimers are a generation of spacecraft materials. However, how to improve the atomic oxygen (AO) resistance of vitrimers remains unexplored although it is critical for extending the lifetime of spacecraft at a low earth orbit. Herein, we fabricate a series of AO resistance epoxy vitrimers with high mechanical properties, recyclability, and thermal stability using glutaric acid to cross-link the mixture of diglycidyl ether of bisphenol F (DGEBF) and polyhedral oligomeric silsesquioxane (POSS) functionalized with epoxy groups. The rigid POSS structure not only imparts the epoxy vitrimers with high mechanical properties (up to 94.4 MPa) and thermal stability (decomposition temperature > 300 °C) but also endows the epoxy vitrimers with excellent AO resistance due to the formation of the SiO2 layer on the surface after AO exposure. Moreover, the reversible ester bonds allow the epoxy vitrimers to be recycled and reprocessed. Therefore, this class of vitrimers hold great promise for application in spacecraft.

KeyWords AITranslate

epoxy resin POSS vitrimer ester bond atomic oxygen
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00659

Chinese Library Classification Number:

Citation Information:

Vitrimers are a generation of spacecraft materials. However, how to improve the atomic oxygen (AO) resistance of vitrimers remains unexplored although it is critical for extending the lifetime of spacecraft at a low earth orbit. Herein, we fabricate a series of AO resistance epoxy vitrimers with high mechanical properties, recyclability, and thermal stability using glutaric acid to cross-link the mixture of diglycidyl ether of bisphenol F (DGEBF) and polyhedral oligomeric silsesquioxane (POSS) functionalized with epoxy groups. The rigid POSS structure not only imparts the epoxy vitrimers with high mechanical properties (up to 94.4 MPa) and thermal stability (decomposition temperature > 300 °C) but also endows the epoxy vitrimers with excellent AO resistance due to the formation of the SiO2 layer on the surface after AO exposure. Moreover, the reversible ester bonds allow the epoxy vitrimers to be recycled and reprocessed. Therefore, this class of vitrimers hold great promise for application in spacecraft.

quote

GB/T 7714-2015 [1] Yao Zhang, Hu Xu, Hao Wang, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00659.
MLA [1] Yao Zhang, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00659.
APA [1] Yao Zhang, Hu Xu, Hao Wang, Rui Wu, Biqiang Jin, & Jinrong Wu. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00659