Multiscale Characterization of Creep and Fatigue Crack Propagation Resistance of Fully Bio-Based Epoxy-Amine Resins AITranslate
Abstract AITranslate
In this study, accelerated creep and dynamic fatigue crack propagation (FCP) measurements were carried out on fully bio-based epoxy-amine thermoset resins. Formulations based on resorcinol diglycidyl ether (RE) were cured with an aliphatic (hexamethylenediamine—HMDA), a cycloaliphatic (diamine-limonene—DA-LIM), or an aromatic (diamine-allyl eugenol—DA-AE) structure. Diglycidyl ether of bisphenol A (DGEBA) cured with HMDA served as a petrosourced benchmark. By considering a multiscale experimental approach combining these experiments with time-domain NMR, it was found that for DGEBA/HMDA, RE/DA-LIM, and RE/DA-AE, their aging properties depend on the resin network structure characterized by the chemical and physical cross-link density. It was demonstrated that the three considered fully bio-based matrices showed better aging resistance compared to DGEBA/HMDA. For RE/HMDA, which possesses a lower experimental cross-link density than expected, physical entanglements probed by NMR act as semihard cross-links conferring a more ductile behavior. This leads to RE/HMDA showing comparable aging properties to those of RE/DA-LIM and RE/DA-AE. This work shows that the studied fully bio-based epoxy-amine resins possess remarkable fatigue crack resistance properties and can be considered as potential candidates for functional applications. Finally, the proposed multiscale approach combining macroscopic mechanical studies with molecular time-domain NMR allowed us to soundly deepen the understanding of the structure–property relationship for such functional materials.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c00894
Chinese Library Classification Number:
Citation Information:
In this study, accelerated creep and dynamic fatigue crack propagation (FCP) measurements were carried out on fully bio-based epoxy-amine thermoset resins. Formulations based on resorcinol diglycidyl ether (RE) were cured with an aliphatic (hexamethylenediamine—HMDA), a cycloaliphatic (diamine-limonene—DA-LIM), or an aromatic (diamine-allyl eugenol—DA-AE) structure. Diglycidyl ether of bisphenol A (DGEBA) cured with HMDA served as a petrosourced benchmark. By considering a multiscale experimental approach combining these experiments with time-domain NMR, it was found that for DGEBA/HMDA, RE/DA-LIM, and RE/DA-AE, their aging properties depend on the resin network structure characterized by the chemical and physical cross-link density. It was demonstrated that the three considered fully bio-based matrices showed better aging resistance compared to DGEBA/HMDA. For RE/HMDA, which possesses a lower experimental cross-link density than expected, physical entanglements probed by NMR act as semihard cross-links conferring a more ductile behavior. This leads to RE/HMDA showing comparable aging properties to those of RE/DA-LIM and RE/DA-AE. This work shows that the studied fully bio-based epoxy-amine resins possess remarkable fatigue crack resistance properties and can be considered as potential candidates for functional applications. Finally, the proposed multiscale approach combining macroscopic mechanical studies with molecular time-domain NMR allowed us to soundly deepen the understanding of the structure–property relationship for such functional materials.
quote
| GB/T 7714-2015 | [1] Nour Mattar, Fabian Hübner, Martin Demleitner, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00894. |
| MLA | [1] Nour Mattar, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00894. |
| APA | [1] Nour Mattar, Fabian Hübner, Martin Demleitner, Alexander Brückner, Valérie Langlois, Estelle Renard, Holger Ruckdäschel, & Agustín Rios de Anda. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00894 |
| IEEE | [1] Nour Mattar, Fabian Hübner, Martin Demleitner, Alexander Brückner, Valérie Langlois, Estelle Renard, Holger Ruckdäschel, and Agustín Rios de Anda, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00894. keywords: {biobased thermosets;creep;fatigue crack propagation;mechanical aging;lifetime resistance} |