Effect of Process Parameters on the Properties of Direct Written Gas-Generating Reactive Layers AITranslate
Abstract AITranslate
A mixture of copper complex and Al/CuO nanothermite, Al/CuO/CuC, represents one of the state-of-the-art gas-generating thermite systems with various pyrotechnic applications due to its tunable gas release rates. The reactivity of reactive inks with various loadings of the poly(vinylpyrrolidone) (PVP) binder mixed with Al/CuO/CuC is characterized using high-speed imaging diagnostics and pressure measurements. For a PVP mass fraction of <7 wt %, the printed materials remain highly reactive and burn at a high velocity (10–54 m/s), which was one of the important goals of this study. At higher PVP contents, the polymer inhibits the reaction. Printing (dropwise and continuously writing) of inks containing 5 wt % PVP and 95 wt % reactive Al/CuO/CuC powder was demonstrated using a volumetrically controlled dispenser and a pneumatically actuated syringe. The pressure development and burning rate of the printed materials are 0.37 MPa (at 46.3% theoretical maximum density (TMD)) and 17 m/s (at 0.24% TMD), respectively, more than 10 times faster than the majority of works dealing with printed energetic formulations.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c00513
Chinese Library Classification Number:
Citation Information:
A mixture of copper complex and Al/CuO nanothermite, Al/CuO/CuC, represents one of the state-of-the-art gas-generating thermite systems with various pyrotechnic applications due to its tunable gas release rates. The reactivity of reactive inks with various loadings of the poly(vinylpyrrolidone) (PVP) binder mixed with Al/CuO/CuC is characterized using high-speed imaging diagnostics and pressure measurements. For a PVP mass fraction of <7 wt %, the printed materials remain highly reactive and burn at a high velocity (10–54 m/s), which was one of the important goals of this study. At higher PVP contents, the polymer inhibits the reaction. Printing (dropwise and continuously writing) of inks containing 5 wt % PVP and 95 wt % reactive Al/CuO/CuC powder was demonstrated using a volumetrically controlled dispenser and a pneumatically actuated syringe. The pressure development and burning rate of the printed materials are 0.37 MPa (at 46.3% theoretical maximum density (TMD)) and 17 m/s (at 0.24% TMD), respectively, more than 10 times faster than the majority of works dealing with printed energetic formulations.
quote
| GB/T 7714-2015 | [1] Florent Sevely, Xuwen Liu, Tao Wu, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00513. |
| MLA | [1] Florent Sevely, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00513. |
| APA | [1] Florent Sevely, Xuwen Liu, Tao Wu, Fabien Mesnilgrente, Bernard Franc, Sandrine AssieSouleille, Xavier Dollat, & Carole Rossi. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00513 |
| IEEE | [1] Florent Sevely, Xuwen Liu, Tao Wu, Fabien Mesnilgrente, Bernard Franc, Sandrine AssieSouleille, Xavier Dollat, and Carole Rossi, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00513. keywords: {reactive material;3D printing;thermite;gas generation;energetic materials;direct writing} |