Hybridization of a Polymer inside the Pores of Activated Carbon and Pore Structural Characterization AITranslate
Abstract AITranslate
A polymer, polydicyclopentadiene (PDCPD), is hybridized within the pores of activated carbon (AC) that has micropores and mesopores of ∼4 nm. The hybridization is performed via gas-phase adsorption of dicyclopentadiene (DCPD) on AC and subsequent thermal polymerization. It is confirmed from a variety of analytical techniques, such as scanning and transmittance electron microscopies, a nitrogen adsorption–desorption analysis, and electrochemical measurements, that there is little PDCPD on the particle surfaces of AC. The nitrogen adsorption–desorption measurement of the resulting AC/PDCPD hybrids reveals that the micropore and mesopore volumes decrease with the increasing amount of the hybridized PDCPD. Moreover, the electric double-layer capacitance decreases and the diffusion resistance increases with the increasing amount of the hybridized PDCPD. These results cannot be explained by a micropore filling model where micropores are first filled with PDCPD. Our experimental results reveal that PDCPD does not exist as layers covering the pore walls of AC but exists as agglomerates uniformly distributing inside both micropores and mesopores.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c00498
Chinese Library Classification Number:
Citation Information:
A polymer, polydicyclopentadiene (PDCPD), is hybridized within the pores of activated carbon (AC) that has micropores and mesopores of ∼4 nm. The hybridization is performed via gas-phase adsorption of dicyclopentadiene (DCPD) on AC and subsequent thermal polymerization. It is confirmed from a variety of analytical techniques, such as scanning and transmittance electron microscopies, a nitrogen adsorption–desorption analysis, and electrochemical measurements, that there is little PDCPD on the particle surfaces of AC. The nitrogen adsorption–desorption measurement of the resulting AC/PDCPD hybrids reveals that the micropore and mesopore volumes decrease with the increasing amount of the hybridized PDCPD. Moreover, the electric double-layer capacitance decreases and the diffusion resistance increases with the increasing amount of the hybridized PDCPD. These results cannot be explained by a micropore filling model where micropores are first filled with PDCPD. Our experimental results reveal that PDCPD does not exist as layers covering the pore walls of AC but exists as agglomerates uniformly distributing inside both micropores and mesopores.
quote
| GB/T 7714-2015 | [1] Hiroyuki Itoi, Ryutaro Suzuki, Masahiro Miyaji, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00498. |
| MLA | [1] Hiroyuki Itoi, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00498. |
| APA | [1] Hiroyuki Itoi, Ryutaro Suzuki, Masahiro Miyaji, Miku Matsuura, Kazuki Takagi, Yuichiro Tanabe, Yuka Goto, Satoshi Kameoka, Shinichi Kugimiya, Hiroyuki Iwata, & Yoshimi Ohzawa. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00498 |
| IEEE | [1] Hiroyuki Itoi, Ryutaro Suzuki, Masahiro Miyaji, Miku Matsuura, Kazuki Takagi, Yuichiro Tanabe, Yuka Goto, Satoshi Kameoka, Shinichi Kugimiya, Hiroyuki Iwata, and Yoshimi Ohzawa, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00498. keywords: {activated carbon;dicyclopentadiene;polydicyclopentadiene;hybridization;electric doublelayer capacitors} |