On Expansion of Ta-W-Y Alloy Bars in the Couse of Moderate Temperature Sintering AITranslate
Abstract AITranslate
Study was made on expansion of Ta-W-Y alloy bar in the couse of moderatetemperature sintering. The paper analyses the source of expansion, relation of expansionrate to sintering temperature and W content,and put forward a 2-stage sintering method tosolve the bar's adhesion problem.
KeyWords AITranslate
1邓伟平,曾兴蒂,池向东.熔盐电解制取镁钇合金和金属钇[J].稀土,1997,18(2):57-60. 被引量:11
2何润德,车蓉,毛小浩,黎志英,张念炳.处理我国铝土矿的两段烧结法研究[J].贵州工业大学学报:自然科学版,2003,32(5):9-12. 被引量:2
3谢明,郑福前,陈长华.Ag-Ni-Y 合金的组织和性能研究[J].昆明理工大学学报:理工版,1997,22(2):83-86. 被引量:7
4毛小浩,车蓉,胡四春,何润德.中低品位铝土矿两段烧结法中一段烧结工艺研究[J].贵州工业大学学报:自然科学版,2003,32(2):11-15. 被引量:2
5何润德,黎志英,张念炳,车蓉,毛小浩.两段烧结法处理中低品位铝土矿[J].有色金属,2005,57(3):55-57. 被引量:4
6上官正,杨重愚.两段烧结工艺中的Ⅰ段赤泥烧结[J].中南工业大学学报,1999,30(1):26-30. 被引量:1
7中金黄金和中国建行总行签订“小金条系列产品委托加工合同”[J].黄金,2005,26(6):47-47.
8郭旭涛,李培杰,曾大本.Mg-Y合金的电子理论研究[J].中国稀土学报,2004,22(2):291-291.
9P.F.索仁参,毛水和.无机酸沉淀法从CIP法洗出液中回收金被贱金属污染的洗出液中金的沉淀[J].黄金,1990,11(2):47-49.
10Jessica Jacks,王永慧.黄 金[J].中国有色冶金,1990,0(1):1-8.
Basic Information:
DOI:
Chinese Library Classification Number:TF123.71[冶金工程—粉末冶金]
Citation Information:
Study was made on expansion of Ta-W-Y alloy bar in the couse of moderatetemperature sintering. The paper analyses the source of expansion, relation of expansionrate to sintering temperature and W content,and put forward a 2-stage sintering method tosolve the bar's adhesion problem.
quote
| GB/T 7714-2015 | [1] YANG Pei-lin. On Expansion of Ta-W-Y Alloy Bars in the Couse of Moderate Temperature Sintering[J]. Rare Metals and Cemented Carbides, 1997(1): 31-33. |
| MLA | [1] YANG Pei-lin. "On Expansion of Ta-W-Y Alloy Bars in the Couse of Moderate Temperature Sintering." Rare Metals and Cemented Carbides, no. 1, 1997, pp. 31-33. |
| APA | [1] YANG Pei-lin. (1997). On Expansion of Ta-W-Y Alloy Bars in the Couse of Moderate Temperature Sintering. Rare Metals and Cemented Carbides(1), 31-33. |
| IEEE | [1] YANG Pei-lin, "On Expansion of Ta-W-Y Alloy Bars in the Couse of Moderate Temperature Sintering," Rare Metals and Cemented Carbides, no. 1, pp. 31-33, 1997. keywords: {Ta-W-Y alloy bar, moderate temperature sintering, expansion, adhesion} |