Use of W--Re Thermocouple in High-temperature Sintering Stove of Mo Metallurgy AITranslate
Abstract AITranslate
The present situation of temperature measurement in high--temperature sintering stove of Mo metallurgy was introduced. The adVantage of W--Re thermocouple over traditional optical pyrometer was discussed. The characteristics of several W--Re thermocouples were presen tedl
KeyWords AITranslate
1庄褂哲.对高温烧结的新认识[J].粉末冶金工业,1992(4):30-31.
2WikmanS.钢的高温烧结[J].粉末冶金技术,2003,21(1):55-55.
3鲁淑瑜,李永祚.快速钨铼电偶测温系统...[J].首钢科技,1991(5):23-26.
4刘曼朗.专利信息[J].粉末冶金工业,2014,24(2):60-60.
5张汪年,邓宁,梁伟杰,彭俐俐,王新海.CuO对白云石烧结性能的影响[J].粉末冶金技术,2016,34(4):277-280. 被引量:7
Basic Information:
DOI:
Chinese Library Classification Number:TF841.2[冶金工程—有色金属冶金]
Citation Information:
The present situation of temperature measurement in high--temperature sintering stove of Mo metallurgy was introduced. The adVantage of W--Re thermocouple over traditional optical pyrometer was discussed. The characteristics of several W--Re thermocouples were presen tedl
quote
| GB/T 7714-2015 | [1] GUO Guo-zhou, WEI Qing-shan. Use of W--Re Thermocouple in High-temperature Sintering Stove of Mo Metallurgy[J]. Rare Metals and Cemented Carbides, 1994(2): 58-60. |
| MLA | [1] GUO Guo-zhou, and WEI Qing-shan. "Use of W--Re Thermocouple in High-temperature Sintering Stove of Mo Metallurgy." Rare Metals and Cemented Carbides, no. 2, 1994, pp. 58-60. |
| APA | [1] GUO Guo-zhou, & WEI Qing-shan. (1994). Use of W--Re Thermocouple in High-temperature Sintering Stove of Mo Metallurgy. Rare Metals and Cemented Carbides(2), 58-60. |
| IEEE | [1] GUO Guo-zhou and WEI Qing-shan, "Use of W--Re Thermocouple in High-temperature Sintering Stove of Mo Metallurgy," Rare Metals and Cemented Carbides, no. 2, pp. 58-60, 1994. keywords: {W--Re thermocouple, Mo metallurgy, high--tempera ture Stnteringstove} |