daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Research Progress of Refractory High-entropy Alloys AITranslate

School of Materials Science and Engineering,Shaanxi University of Technology;School of Materials Science and Engineering,Shaanxi University of Technology;School of Materials Science and Engineering,Shaanxi University of Technology;School of Materials Science and Engineering,Shaanxi University of Technology;School of Materials Science and Engineering,Shaanxi University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Refractory high-entropy alloys have excellent high-temperature properties and have great development potential.The research progress of refractory high-entropy alloys is reviewed from the aspects of preparation process,treatment process,mechanical properties and corrosion resistance,and their application prospects are pointed out.

KeyWords AITranslate

refractory high-entropy alloy preparation process treatment process mechanical property corrosion resistance review

1张娈,董闯,王存山,王清.45钢表面激光熔覆Fe-B-Si铁基非晶复合材料[J].材料热处理学报,2012,33(10):116-123. 被引量:16

2聂洋洋,程兴旺,聂宇坤,刘日平.20Zr-70Ti-6Al-4V合金静动态力学性能研究[J].稀有金属材料与工程,2018,47(4):1210-1215. 被引量:3

3王胜海,杨春成,边秀房.铝基非晶合金的研究进展[J].材料导报,2012,26(1):88-93. 被引量:5

4肖璐,潘复生.挤压态定向凝固镁合金组织及力学性能[J].材料科学与工程学报,2020,38(3):460-465. 被引量:1

5赵宇芳,张金钰,王亚强,吴凯,刘刚,孙军.Cu/NbMoTaW纳米叠层材料具有尺寸效应的力学性能及变形机制(英文)[J].中国科学:材料科学(英文版),2020,63(3):444-452. 被引量:3

6漆陪部,梁秀兵,仝永刚,陈永雄,张志彬.球磨时间对机械合金化制备NbMoTaW高熵合金粉末的影响[J].稀有金属材料与工程,2019,48(8):2623-2629. 被引量:8

7陈刚,罗涛,沈书成,陶韬,唐啸天,薛伟,夏义.基于铝热反应FeCrNiCuAlSn0.5 高熵合金涂层的制备[J].材料导报,2020,34(17):17047-17051. 被引量:5

8张雪,崔洪芝,王明亮,赵玉桥,孙康.Al含量对Al_xCoCrFeNi系高熵合金组织和耐蚀性能的影响[J].材料热处理学报,2018,39(12):29-36. 被引量:9

9张长亮,卢一平.氮元素对Ti2ZrHfV0.5Mo0.2高熵合金组织及力学性能的影响[J].材料导报,2019,33(A01):329-331. 被引量:6

10畅海涛,李万鹏,杨涛,黄志青,武保林,段国升,杜兴蒿.立方晶体结构高熵合金在低温条件下的力学行为研究进展[J].稀有金属材料与工程,2020,49(9):3273-3284. 被引量:8

1孟凡莹,张一凡,杨佳惠,张薇,王琳,武俊霞,李培友.高熵合金催化性能的研究进展[J].材料热处理学报,2023,44(6):20-27.

1李玉成,孙言,朱守宇.玻璃钢构件粘接用环氧胶粘剂性能研究[J].纤维复合材料,2021,38(3):60-64. 被引量:3

2矢部室恒,岡崎賢司,平田茂,王昆(日本冶金工业株式会社技术研究所),Murotsune YABE.耐高氯化物/硫酸腐蚀兼用型7.5Mo镍基合金NAS355N的开发[J].不锈,2021(3):1-9.

Basic Information:

DOI:

Chinese Library Classification Number:TG146.4[金属学及工艺—金属材料]

Citation Information:

Refractory high-entropy alloys have excellent high-temperature properties and have great development potential.The research progress of refractory high-entropy alloys is reviewed from the aspects of preparation process,treatment process,mechanical properties and corrosion resistance,and their application prospects are pointed out.

quote

GB/T 7714-2015 [1] LIU Ya-ling, YANG Jia-hui, WU Jun-xia, et al. Research Progress of Refractory High-entropy Alloys[J]. Rare Metals and Cemented Carbides, 2021(5): 59-64.
MLA [1] LIU Ya-ling, et al., "Research Progress of Refractory High-entropy Alloys." Rare Metals and Cemented Carbides, no. 5, 2021, pp. 59-64.
APA [1] LIU Ya-ling, YANG Jia-hui, WU Jun-xia, DONG Hong-feng, & LI Pei-you. (2021). Research Progress of Refractory High-entropy Alloys. Rare Metals and Cemented Carbides(5), 59-64.
IEEE [1] LIU Ya-ling, YANG Jia-hui, WU Jun-xia, DONG Hong-feng, and LI Pei-you, "Research Progress of Refractory High-entropy Alloys," Rare Metals and Cemented Carbides, no. 5, pp. 59-64, 2021. keywords: {refractory high-entropy alloy;preparation process;treatment process;mechanical property;corrosion resistance;review}