Investigation on Separation of Trace Vanadium by Extraction from Vanadium-containing Ammonium Tungstate Solution AITranslate
Abstract AITranslate
Alkaline extraction method with quaternary ammonium salt was proposed for deep removal of va- nadium from vanadium-containing ammonium tungstate solution and experimental research was carried out. The effects of organic phase composition and equilibrium aqueous pH on extraction were investigated as well as the effect of O/A ratio on stripping. Isotherms of extraction and stripping were plotted and the simulated multi-stage countercurrent extraction and stripping experiments were conducted. The results show that the concentration of vanadium in the aqueous phase drops below 10 mg/L and tungsten loss is below 5% after six-stage countercurrent extraction under the following conditions: organic phase composi- tion (volume fraction) of 1% N263, 5% 2-octanol and sulfonated kerosene,feed pH of 8.7 (by evaporation deamination pretreatment) ,phase ratio (O/A) of 1.25 : 1 and 25 ℃. Vanadium in the loaded organic phase can be completely stripped with 2 mol/L NaOH solution,and the stripped organic phase can be returned to the extraction process for recycle.
KeyWords AITranslate
1肖连生.中国钨提取冶金技术的进步与展望[J].有色金属科学与工程,2013,4(5):6-10. 被引量:20
2张贵清,张启修.一种钨湿法冶金清洁生产工艺[J].稀有金属,2003,27(2):254-257. 被引量:21
3林德海,宋宝华,王中原.废弃SCR脱硝催化剂资源回收[J].山东化工,2013,42(4):8-10. 被引量:13
4罗琳,藤田丰久,治进藤.从废弃的钨金属制品中回收钨和钒[J].矿冶,2002(1):50-54. 被引量:12
5陈星宇,肖露萍,赵中伟.钨钼冶炼过程中除钒[J].中国有色金属学报,2014,24(7):1883-1887. 被引量:5
6宋阜,朱宾权.离子交换法分离富集钨酸钠溶液中的钒[J].稀有金属与硬质合金,2006,34(3):5-7. 被引量:14
7张子岩,简椿林.溶剂萃取法在钨湿法冶金中的应用[J].湿法冶金,2006,25(1):1-9. 被引量:18
8张家靓,赵中伟.W(Ⅵ)-V(Ⅴ)-H_2O体系钨钒分离的热力学分析[J].中国有色金属学报,2014,24(6):1656-1662. 被引量:11
1韩桂洪,王旱雨,苏胜鹏,黄艳芳,刘兵兵.溶解态钨钒选择性分离技术研究进展及探讨[J].中国有色金属学报,2021,31(11):3380-3395. 被引量:3
1韩桂洪,王静雯,刘兵兵,孙虎,黄艳芳.湿法炼锌净化钴渣回收钴技术进展及展望[J].贵州大学学报:自然科学版,2022,39(2):1-6. 被引量:1
2贾蓝波,王玲,郭紫璇,熊雨婷,夏亮亮,王龙,聂轶苗,刘淑贤.含钒溶液萃取分离富集钒的研究进展[J].中国有色金属学报,2022,32(11):3489-3504. 被引量:1
3王泽玮,张伟光,梁新星,刘远,喻亮,曹雪娇,蔡震雷,胡磊.拜耳循环母液中钒的选择性吸附性能及机理[J].有色金属科学与工程,2023,14(4):460-466.
1雷国华,刘佳.GE水煤浆气化渣水工段运行问题探讨[J].山东化工,2017,46(16):145-146.
2朱健玲,王瑞祥.接触膜脱氨法处理离子型稀土矿山氨氮废水的工程实践[J].有色金属:冶炼部分,2017(9):58-62. 被引量:13
3邸惠斌.钒钛矿高炉应对原料含钒变化的生产实践[J].河北冶金,2017(9):39-42.
4王雄,刘明言,宋军超.溶剂萃取-树脂吸附联合脱除盐湖老卤中的微量硼[J].化工进展,2017,36(10):3625-3632. 被引量:3
5阳启华,邹潜,汤启明,徐志刚,李凤,季尚军,杨明.从铜铁浸出液中选择性萃取铜试验研究[J].湿法冶金,2017,36(4):293-296. 被引量:3
6王俊娥,张焕然,衷水平,陈杭.从富铼渣中回收铼并制备高铼酸铵[J].有色金属:冶炼部分,2017(10):57-60. 被引量:7
7陈佳文.探究水环境中挥发性有机物的监测方法[J].环境与发展,2017,29(7):152-153. 被引量:2
8江棉生,沈鸣九.米氮平伴用养血清脑颗粒治疗脑卒中后抑郁状态的疗效观察[J].世界最新医学信息文摘,2016,0(63):130-131. 被引量:2
9陈浩,董俊哲,王会永.水萃取法检测纺织品面料甲醛含量分析[J].轻工科技,2017,33(9):96-97. 被引量:1
10张景丽,刘美林,武名麟,温建康.pH值、相比、温度和金属离子对LIX984界面吸附性能的影响[J].稀有金属,2017,41(9):1019-1027. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TF841.3[冶金工程—有色金属冶金]
Citation Information:
Alkaline extraction method with quaternary ammonium salt was proposed for deep removal of va- nadium from vanadium-containing ammonium tungstate solution and experimental research was carried out. The effects of organic phase composition and equilibrium aqueous pH on extraction were investigated as well as the effect of O/A ratio on stripping. Isotherms of extraction and stripping were plotted and the simulated multi-stage countercurrent extraction and stripping experiments were conducted. The results show that the concentration of vanadium in the aqueous phase drops below 10 mg/L and tungsten loss is below 5% after six-stage countercurrent extraction under the following conditions: organic phase composi- tion (volume fraction) of 1% N263, 5% 2-octanol and sulfonated kerosene,feed pH of 8.7 (by evaporation deamination pretreatment) ,phase ratio (O/A) of 1.25 : 1 and 25 ℃. Vanadium in the loaded organic phase can be completely stripped with 2 mol/L NaOH solution,and the stripped organic phase can be returned to the extraction process for recycle.
quote
| GB/T 7714-2015 | [1] WANG Liu-pei, ZHANG Gui-qing, GUAN Wen-juan, et al. Investigation on Separation of Trace Vanadium by Extraction from Vanadium-containing Ammonium Tungstate Solution[J]. Rare Metals and Cemented Carbides, 2017(4): 1-5. |
| MLA | [1] WANG Liu-pei, et al., "Investigation on Separation of Trace Vanadium by Extraction from Vanadium-containing Ammonium Tungstate Solution." Rare Metals and Cemented Carbides, no. 4, 2017, pp. 1-5. |
| APA | [1] WANG Liu-pei, ZHANG Gui-qing, GUAN Wen-juan, ZENG Li, ZHOU Qin, & XIA Yun. (2017). Investigation on Separation of Trace Vanadium by Extraction from Vanadium-containing Ammonium Tungstate Solution. Rare Metals and Cemented Carbides(4), 1-5. |
| IEEE | [1] WANG Liu-pei, ZHANG Gui-qing, GUAN Wen-juan, ZENG Li, ZHOU Qin, and XIA Yun, "Investigation on Separation of Trace Vanadium by Extraction from Vanadium-containing Ammonium Tungstate Solution," Rare Metals and Cemented Carbides, no. 4, pp. 1-5, 2017. keywords: {vanadium- containing ammonium tungstate solution;vanadium removal;quaternary ammonium salt;extraction;stripping;evaporation deamination} |