daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Highly Stretchable Poly(thiocarbonate)/Graphene Oxide Dielectric Composites toward a High Dielectric Constant and Low Dielectric Loss AITranslate

Zhejiang University; Zhejiang University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Dielectric elastomers (DEs) have attracted much attention due to their application prospects in biomimetic actuated devices, it is still a big challenge to prepare DEs with high dielectric constants (ε′) and low dielectric losses (tan δ). This work reports highly stretchable poly(propylene-monothiocarbonate)/graphene oxide (PPMTC/GO) dielectric composites with high ε′ and low tan δ via a simple solution-mixing process. The PPMTC with repeated thiocarbonate units enhances the interfacial polarizations with GO, leading to a high ε′ (up to 12). Meanwhile, the hydrogen bonding interactions of PPMTC and GO improve the dispersion of GO in the polymer matrix and thus decrease tan δ (∼0.07). Interestingly, the PPMTC/GO composites also possess excellent shape-memory performance, especially under large deformations (about 50%), with both the fixing ratio (Rf) and recovery ratio (Rr) more than 90%. In addition, the ultimate tensile strength is about 6.5 MPa for the neat PPMTC and over 7.0 MPa for its composites, and the elongation at break for all the samples is over 700%. Thus, it provides an alternative method to the fabrication of DEs.

KeyWords AITranslate

polythiocarbonate/GO dielectric composites highly stretchable high dielectric constant low dielectric loss shape memory
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00477

Chinese Library Classification Number:

Citation Information:

Dielectric elastomers (DEs) have attracted much attention due to their application prospects in biomimetic actuated devices, it is still a big challenge to prepare DEs with high dielectric constants (ε′) and low dielectric losses (tan δ). This work reports highly stretchable poly(propylene-monothiocarbonate)/graphene oxide (PPMTC/GO) dielectric composites with high ε′ and low tan δ via a simple solution-mixing process. The PPMTC with repeated thiocarbonate units enhances the interfacial polarizations with GO, leading to a high ε′ (up to 12). Meanwhile, the hydrogen bonding interactions of PPMTC and GO improve the dispersion of GO in the polymer matrix and thus decrease tan δ (∼0.07). Interestingly, the PPMTC/GO composites also possess excellent shape-memory performance, especially under large deformations (about 50%), with both the fixing ratio (Rf) and recovery ratio (Rr) more than 90%. In addition, the ultimate tensile strength is about 6.5 MPa for the neat PPMTC and over 7.0 MPa for its composites, and the elongation at break for all the samples is over 700%. Thus, it provides an alternative method to the fabrication of DEs.

quote

GB/T 7714-2015 [1] Zhanbin Feng, XingHong Zhang. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00477.
MLA [1] Zhanbin Feng, and XingHong Zhang. ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00477.
APA [1] Zhanbin Feng, & XingHong Zhang. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00477
IEEE [1] Zhanbin Feng and XingHong Zhang, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00477. keywords: {polythiocarbonate/GO dielectric composites;highly stretchable;high dielectric constant;low dielectric loss;shape memory}