Hardener Isomerism and Content of Dynamic Disulfide Bond Effect on Chemical Recycling of Epoxy Networks AITranslate
Abstract AITranslate
Nowadays, there is an important concern in the scientific community related to the end-of-life products derived from polymeric matrix composites. In this regard, covalent adaptable networks and, more specifically, the disulfide bond-based ones are a promising approach to develop composite parts able to be dissolved in a specific solvent, thus regaining the continuous fiber reinforcement. In this work, the effect of hardener isomerism, using 2-aminophenyl disulfide (2-AFD) and 4-aminophenyl disulfide (4-AFD), and amine/epoxy ratio (1.0–1.2) was studied to optimize the chemical recycling capabilities at different temperatures. Results confirmed the need for using hardener excesses for dissolving these vitrimers. Networks based on 2-AFD were dissolved in considerably lower times than the 4-AFD ones, which is interesting since the latter one is quite more used for this purpose and currently way more expensive. In this context, a composite laminate, reinforced with six layers of carbon fiber fabric, was manufactured as the proof-of-concept.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.2c00598
Chinese Library Classification Number:
Citation Information:
Nowadays, there is an important concern in the scientific community related to the end-of-life products derived from polymeric matrix composites. In this regard, covalent adaptable networks and, more specifically, the disulfide bond-based ones are a promising approach to develop composite parts able to be dissolved in a specific solvent, thus regaining the continuous fiber reinforcement. In this work, the effect of hardener isomerism, using 2-aminophenyl disulfide (2-AFD) and 4-aminophenyl disulfide (4-AFD), and amine/epoxy ratio (1.0–1.2) was studied to optimize the chemical recycling capabilities at different temperatures. Results confirmed the need for using hardener excesses for dissolving these vitrimers. Networks based on 2-AFD were dissolved in considerably lower times than the 4-AFD ones, which is interesting since the latter one is quite more used for this purpose and currently way more expensive. In this context, a composite laminate, reinforced with six layers of carbon fiber fabric, was manufactured as the proof-of-concept.
quote
| GB/T 7714-2015 | [1] David MartinezDiaz, Alejandro Cortés, Alberto JiménezSuárez, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00598. |
| MLA | [1] David MartinezDiaz, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00598. |
| APA | [1] David MartinezDiaz, Alejandro Cortés, Alberto JiménezSuárez, & Silvia G. Prolongo. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00598 |