daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Study on Preparation and Mechanical Properties of Pb-RE Alloy for Copper Electrowinning AITranslate

School of Applied Science, Jiangxi University of Technology;School of Applied Science, Jiangxi University of Technology;School of Applied Science, Jiangxi University of Technology;School of Applied Science, Jiangxi University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The different types (Pb-Pr,Pb-Sm,Pb-Nd) and different RE contents (0.1%、0.5%、1.0%、1.5%、2.0%) of Pb-RE alloys were prepared by two-stage remelting,and the study was made on the influence rule of the content and type of rare earth element on the tensile strength and microstructure of the alloy. The results show that addition of Pr,Sm,Nd can improve the strength of the alloy in different level, and with the increase of content of rare earth elements the strength of the alloy can improve in different degree. The extent of the effect of RE elements on improving the tensile strength of the alloy goes as follows: Pr〉Sm〉Nd. Nd,Sm and Pb generate intermetaliic compound and precipitate on the grain interface,bene- ficial for the alloy strength improvement. Besides generating intermetallic compound,Pr can also refine alloy grains and prevent grain slip, as is also one of the most important factors to improve the tensile strength of the alloy.

KeyWords AITranslate

Pb-RE alloy copper electrowinning two-stage remelting method tensile strength metallographic structure

1袁明华,李德,普仓凤.低品位硫化铜矿的细菌冶金[M].北京:冶金工业出版社,2008:71-75.

2Hrussanova A, Mirkova L, Dobrev T, et al. Influence of temperature and current density on oxygen overpotential and corrosion rate of Pb-Co2 04 ,Pb-Ca-Sn and Pb-Sb an- odes for copper electrowinning: Part I[J].Hydrometal- lurgy,2004,72(3-4) :205-213.

3Hrussanova A, Mirkova L, Dobrev T. Influence of addi- tives on the corrosion rate and oxygen overpotential ofPb-Co3 04 ,Pb-Ca-Sn and Pb-Sb anodes for copper elec- trowinning: Part II [J]. Hydrometallurgy, 2004,72 ( 3- 4) : 215-224.

4杨海涛,陈步明,郭忠诚.铅基合金阳极在有色金属湿法冶炼中的研究与发展[J].中国有色冶金,2012,41(2):20-24. 被引量:13

5杨存龙,杨迪帆,吴寿松,马国哲.板栅常用铅基合金特性概述[J].蓄电池,2007,44(4):180-185. 被引量:17

6李鑫,王涛,魏绪钧,徐秀芝.稀土在铅基合金中的应用[J].有色金属,2003,55(2):15-17. 被引量:16

7Liu Hou-tian,Yang Jiong, Liang Hai-he,et al. Effect of cerium on the anodic corrosion of Pb-Ca-Sn alloy in sul- furic acid solution[J]. Journal of Power Sources, 2001, 93(1-2) :230-233.

8刘芳清,张新华,马敏,柳厚田.镨和钕对硫酸溶液中铅阳极膜阻抗特性的影响[J].复旦学报:自然科学版,2008,47(5):659-662. 被引量:8

9姚靓,周根树,李党国,徐可为.稀土低锑合金的力学和电化学性能研究[J].稀土,2007,28(2):15-19. 被引量:8

10李党国,周根树,姚靓,郑茂盛.铅铈和铅钙锡合金阳极腐蚀膜的性能研究[J].化学学报,2007,65(7):584-588. 被引量:10

1王帅,刘颖,徐东,周向阳.铜电积用3D-Pb-Ca-Sn阳极的电化学性能和微观形貌[J].稀有金属材料与工程,2022,51(6):1986-1992.

1王昆林,田芝瑞,杨崇斌,宋承彬.用激光重熔法提高铝硅合金的耐磨性[J].金属热处理,1994,19(10):1-5. 被引量:6

2王昆林,田芝瑞,杨崇斌,宋承彬.激光重熔法提高铝硅合金的耐磨性[J].中国表面工程,1993(1):21-24.

3朱茂兰,涂弢,朱根松,张丽娜,王瑞祥.钐对铜电积用铅基阳极性能的影响[J].有色金属:冶炼部分,2015(2):45-47.

4孟宪超,王博,魏斌,纪兴华.2024铝合金半固态组织演变及触变成形[J].特种铸造及有色合金,2014(8):808-811.

5齐向前,田旭海,孙忠波,闫青亮.合金元素对T/P91钢焊缝组织及性能的影响[J].热加工工艺,2008,37(23):25-26. 被引量:1

6轩庆庆,龙伟民,张青科,路全彬.稀土对Al-Si-Zn-Cu钎料工艺性能的影响[J].焊接,2017(2):31-36. 被引量:2

7高压熔炼铸造高氮不锈钢[J].金属功能材料,2009,16(6):29-29.

8袁武华,张传阳.稀土元素含量对铝合金显微组织和性能的影响[J].机械工程材料,2014,38(11):54-59. 被引量:2

9Hayak.,H,贾辉章.用真空电弧重熔法生产的钛合金铸件的凝固组织和偏析[J].钒钛,1992(3):22-29.

10王卫国.金宝铜箔公司开发出薄型电解铜箔[J].上海有色金属,2004,25(3):143-143.

Basic Information:

DOI:

Chinese Library Classification Number:TG146.45[金属学及工艺—金属材料]

Citation Information:

The different types (Pb-Pr,Pb-Sm,Pb-Nd) and different RE contents (0.1%、0.5%、1.0%、1.5%、2.0%) of Pb-RE alloys were prepared by two-stage remelting,and the study was made on the influence rule of the content and type of rare earth element on the tensile strength and microstructure of the alloy. The results show that addition of Pr,Sm,Nd can improve the strength of the alloy in different level, and with the increase of content of rare earth elements the strength of the alloy can improve in different degree. The extent of the effect of RE elements on improving the tensile strength of the alloy goes as follows: Pr〉Sm〉Nd. Nd,Sm and Pb generate intermetaliic compound and precipitate on the grain interface,bene- ficial for the alloy strength improvement. Besides generating intermetallic compound,Pr can also refine alloy grains and prevent grain slip, as is also one of the most important factors to improve the tensile strength of the alloy.

quote

GB/T 7714-2015 [1] ZHU Mao-lan, TU Tao, ZHU Gen-song, et al. Study on Preparation and Mechanical Properties of Pb-RE Alloy for Copper Electrowinning[J]. Rare Metals and Cemented Carbides, 2014(4): 46-51.
MLA [1] ZHU Mao-lan, et al., "Study on Preparation and Mechanical Properties of Pb-RE Alloy for Copper Electrowinning." Rare Metals and Cemented Carbides, no. 4, 2014, pp. 46-51.
APA [1] ZHU Mao-lan, TU Tao, ZHU Gen-song, & GUO Huan. (2014). Study on Preparation and Mechanical Properties of Pb-RE Alloy for Copper Electrowinning. Rare Metals and Cemented Carbides(4), 46-51.
IEEE [1] ZHU Mao-lan, TU Tao, ZHU Gen-song, and GUO Huan, "Study on Preparation and Mechanical Properties of Pb-RE Alloy for Copper Electrowinning," Rare Metals and Cemented Carbides, no. 4, pp. 46-51, 2014. keywords: {Pb-RE alloy;copper electrowinning;two-stage remelting method;tensile strength;metallographic structure}