Study on Occurrence State of Germanium in the Coal Ash AITranslate
Abstract AITranslate
The germanium content in the coal ash containing germanium was measured with titration meth- od,and other chemical components were tested by ICP. The phase composition of the coal ash containing germanium was studied by ore microscope,XRD and SEM-EDS. The results show that the content of SiO2 and iron oxide are the highest, followed by Al2O3 ,CaO and MgO, the carbon content greatly fluctuates, and arsenic content is also high. Before carbon removal,germanium dispersedly exists in various phases of the coal ash containing germanium. Germanium content is relatively higher in the phases with high SiO2 and iron oxide content, and lower in carbon particles. After carbon removal, germanium-rich phase appears in coal ash containing germanium, mainly existing in the form of Mg3 Fe3 GeO3 complex oxide and inlaid in oxides such as SiO2 and CaO.
KeyWords AITranslate
1桑永亮,康凯.云南锗业:资源技术铸就锗业龙头[J].中国金属通报,2010(21):34-35. 被引量:2
2孟祥东,曲晓慧,于兆亮,胡悦,孙萌.硅锗光子晶体复合电极对非晶硅电池性能的影响[J].吉林师范大学学报:自然科学版,2016,37(3):36-40. 被引量:3
3郑能瑞.锗的应用与市场分析[J].广东微量元素科学,1998,5(2):12-18. 被引量:15
4胡瑞忠,苏文超,戚华文,毕献武.锗的地球化学、赋存状态和成矿作用[J].矿物岩石地球化学通报,2000,19(4):215-217. 被引量:81
5李余华.临沧锗矿床地质特征[J].云南地质,2000,19(3):263-269. 被引量:11
6胡瑞忠,毕献武,叶造军,苏文超,漆亮.临沧锗矿床成因初探[J].矿物学报,1996,16(2):97-102. 被引量:41
7王兰明.内蒙古锡林郭勒盟乌兰图嘎锗矿地质特征及勘查工作简介[J].内蒙古地质,1999(3):16-20. 被引量:29
8张家敏,雷霆,张玉林,冯林永.从含锗褐煤中干馏提锗和制取焦炭的试验研究[J].稀有金属,2007,31(3):371-376. 被引量:18
1黄根,王宾,徐宏祥,邓久帅.粉煤灰综合利用与提质技术研究进展[J].矿产保护与利用,2019,39(4):32-37. 被引量:17
2刘俊杰,刘丽霞,彭军,柴轶凡,李文挺,安胜利.高温二次火法富集粉煤灰中锗的工艺优化[J].稀有金属与硬质合金,2020,48(2):5-9. 被引量:2
3刘丽霞,宋波,彭军,安胜利.SiO2对锗尘高温富集-盐酸浸出蒸馏中Ge提取的影响[J].稀有金属与硬质合金,2020,48(4):6-11. 被引量:2
4王丽萍,李超,李世春.粉煤灰中稀散金属锗的富集回收技术研究进展[J].稀有金属与硬质合金,2022,50(6):27-32.
5张致远,滕道光,曹亦俊,李鹏.煤系锗的赋存与分离研究进展[J].矿产保护与利用,2022,42(6):10-20.
6武飞乐,李世春.粉煤灰中铝、镓、锂回收技术研究进展[J].中国有色冶金,2023,52(2):116-125.
1李航宇,阎蕊珍,闫亚杰,邢智岩.粉煤灰取代水泥对再生混凝土砖性能的影响[J].新型建筑材料,2020,0(2):92-94. 被引量:10
2汤倩.粉煤灰利用研究现状及其在环境保护中的应用[J].中国资源综合利用,2020,38(5):41-43. 被引量:11
3刘丽霞,宋波,彭军,安胜利.SiO2对锗尘高温富集-盐酸浸出蒸馏中Ge提取的影响[J].稀有金属与硬质合金,2020,48(4):6-11. 被引量:2
4张志华,雷旭阳,王明友.固体废弃物粉煤灰资源化利用技术[J].辽宁化工,2020,49(9):1142-1144. 被引量:8
5王晓龙,刘蓉,王琪,李旭,刘练波,郜时旺.电厂烟气低浓度CO2的粉煤灰直接液相矿化技术[J].热力发电,2021,50(1):104-109. 被引量:5
6孙敏,唐莹,郝亚婷,季宏兵.红枫湖水源地附近粉煤灰堆积场重金属存在形态及静态淋溶规律[J].环境化学,2021,40(3):678-686. 被引量:3
7徐硕,杨金林,马少健.粉煤灰综合利用研究进展[J].矿产保护与利用,2021,41(3):104-111. 被引量:21
8牛永红,康旭峰,李义科,王文才.粉煤灰/废砖基多孔建筑材料及其性能[J].非金属矿,2021,44(4):4-7. 被引量:3
9朱士飞,吴蒙,张谷春,柯妍.粉煤灰提取氧化铝研究进展[J].中国煤炭地质,2021,33(12):83-86. 被引量:3
10唐潇,徐仁博,张发捷,马云龙,赵宏,王乐乐,孙路石,于洁.SCR脱硝氨转化、吸附及飞灰氨脱除技术研究现状[J].洁净煤技术,2022,28(4):75-85. 被引量:4
1李晓华,南小康,封建民.咸阳市耕地与基本农田保护状态研究[J].安徽农业科学,2017,45(33):211-212. 被引量:1
2杨敏,蒋红樱,何振坤,曾怡,白彝华.肠内营养对老年尿毒症透析患者免疫功能及氧化应激状态研究[J].重庆医学,2017,46(32):4566-4569. 被引量:9
3麦伟虎.早产视网膜病变患儿早期屈光状态研究[J].中国现代医学杂志,2017,27(28):82-85. 被引量:2
4张鑫.跃进煤矿南部逆冲推覆构造的推断及影响[J].内蒙古煤炭经济,2017(22):156-156.
5李铁铮.高校教师队伍的亚健康状态研究——以沈阳工程学院为例[J].沈阳工程学院学报:社会科学版,2017,13(4):502-505. 被引量:4
6周军,樊湘芳,丰振东,胡汝骞,胡绍杰.过渡层对TiAlSiN涂层性能的影响[J].真空科学与技术学报,2017,37(10):978-983. 被引量:3
7顾静,夏德宏,齐照东,敖雯青.高温碳热还原条件下钛铁矿物相变化的实验研究[J].稀有金属与硬质合金,2017,45(5):17-21. 被引量:2
8张宇寒,胡煜昭,任涛,董传奇,何岸北,刘昌伟,冯勇.塔西花园砂岩型铜矿床氧化铜矿物研究[J].矿物学报,2017,37(5):625-629. 被引量:6
9任创业.马达加斯加Dabolava金矿地质特征[J].华北国土资源,2017(5):37-38.
10高知睿,赵元艺,曹冲,常玉虎.德兴铜矿堆浸场矿石矿物学、Cu伴生元素地球化学特征及意义[J].岩石矿物学杂志,2017,36(6):785-799. 被引量:3
Basic Information:
DOI:
Chinese Library Classification Number:TQ536.3[化学工程—煤化学工程]
Citation Information:
The germanium content in the coal ash containing germanium was measured with titration meth- od,and other chemical components were tested by ICP. The phase composition of the coal ash containing germanium was studied by ore microscope,XRD and SEM-EDS. The results show that the content of SiO2 and iron oxide are the highest, followed by Al2O3 ,CaO and MgO, the carbon content greatly fluctuates, and arsenic content is also high. Before carbon removal,germanium dispersedly exists in various phases of the coal ash containing germanium. Germanium content is relatively higher in the phases with high SiO2 and iron oxide content, and lower in carbon particles. After carbon removal, germanium-rich phase appears in coal ash containing germanium, mainly existing in the form of Mg3 Fe3 GeO3 complex oxide and inlaid in oxides such as SiO2 and CaO.
quote
| GB/T 7714-2015 | [1] LIU Li-xia, LI Wen-ting, PENG Jun, et al. Study on Occurrence State of Germanium in the Coal Ash[J]. Rare Metals and Cemented Carbides, 2017(5): 27-30. |
| MLA | [1] LIU Li-xia, et al., "Study on Occurrence State of Germanium in the Coal Ash." Rare Metals and Cemented Carbides, no. 5, 2017, pp. 27-30. |
| APA | [1] LIU Li-xia, LI Wen-ting, PENG Jun, ZHANG Lei, AN Sheng-li, XUE Ying-dong, LIU Wei, & LI Xiao-ming. (2017). Study on Occurrence State of Germanium in the Coal Ash. Rare Metals and Cemented Carbides(5), 27-30. |
| IEEE | [1] LIU Li-xia, LI Wen-ting, PENG Jun, ZHANG Lei, AN Sheng-li, XUE Ying-dong, LIU Wei, and LI Xiao-ming, "Study on Occurrence State of Germanium in the Coal Ash," Rare Metals and Cemented Carbides, no. 5, pp. 27-30, 2017. keywords: {coal ash;germanium, mineral phase;phase analysis;occurrence state} |