Study on the Micro Defect of DGJW40 Steel bonded Carbide Made by a New Process AITranslate
Abstract AITranslate
Study of the micro defects of DGJW40 steel bonded WC carbide made by a new process showed that this process was better than the existing compacting sintering methods in respect of the alloy's compactness,hole cleanliness,free carbon content and segregation of hard phase in the alloy.
KeyWords AITranslate
1唐文英.钢结硬质合金金相检验法[J].理化检验:物理分册,1982,(1):43-43.
2马营生.精密合金及粉末冶金材料[M].北京:机械工业出版社,1982.92.
3安振琳.工具钢金相图谱[M].北京:机械工业出版社,1979.218.
1梁和.新闻报道理念浅探[J].中国广播电视学刊,2002(12):79-79. 被引量:1
1吴昊.从法制与道德看新闻价值的应有之义[J].新闻世界,2015,0(1):144-145.
1郭钊.钢中气体对特殊钢陛能的影响分析[J].科学与财富,2010(4):11-12.
2尤显卿,王基才,任昊.新型钢结硬质合金DGJW20的显微缺陷分析[J].新技术新工艺,2004(2):53-55.
3黄新,孙亚丽,颜杰,唐凯,刘清才,何宪峰,李伟.两步碳化法生产优质粗颗粒WC粉末[J].中国钨业,2007,22(6):39-42. 被引量:4
4陈荣欢,朱祖民,职建军,冯长宝.宝钢超低碳钢保护渣的开发[J].炼钢,2007,23(2):14-17. 被引量:6
5宋安国.亚微米级碳化钨的生产工艺[J].中国钨业,1994,0(5):19-20.
6宋佳霖,易正明,彭其春,盛喜松,邓品团.RH精炼终点-中间包浇铸过程超低碳钢水增碳的影响因素[J].特殊钢,2013,34(5):32-33. 被引量:1
7赵秦生,陈绍衣.关于碳化钨质量的评述与建议[J].中国钨业,1990(11):6-10. 被引量:1
8周玉昌.配碳比对TiO2真空碳热还原的影响[J].钢铁钒钛,2012,33(6):6-10. 被引量:5
9高翔,袁勇,张德金,李威,蔺瑞冬,崔建民,罗丰华.复压复烧对预合金钢粉烧结材料性能的影响[J].中南大学学报:自然科学版,2011,42(9):2628-2634. 被引量:5
10李劲风,张昭,张鉴清,郑子樵,徐协文.燃烧合成(W,Ti)C在硬质合金中的应用[J].粉末冶金技术,2001,19(5):283-285. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TF125.32[冶金工程—粉末冶金]
Citation Information:
Study of the micro defects of DGJW40 steel bonded WC carbide made by a new process showed that this process was better than the existing compacting sintering methods in respect of the alloy's compactness,hole cleanliness,free carbon content and segregation of hard phase in the alloy.
quote
| GB/T 7714-2015 | [1] DU Xiao-dong, YOU Xian-qing, ZHENG Yu-chun. Study on the Micro Defect of DGJW40 Steel bonded Carbide Made by a New Process[J]. Rare Metals and Cemented Carbides, 2000(1): 22-25. |
| MLA | [1] DU Xiao-dong, et al., "Study on the Micro Defect of DGJW40 Steel bonded Carbide Made by a New Process." Rare Metals and Cemented Carbides, no. 1, 2000, pp. 22-25. |
| APA | [1] DU Xiao-dong, YOU Xian-qing, & ZHENG Yu-chun. (2000). Study on the Micro Defect of DGJW40 Steel bonded Carbide Made by a New Process. Rare Metals and Cemented Carbides(1), 22-25. |
| IEEE | [1] DU Xiao-dong, YOU Xian-qing, and ZHENG Yu-chun, "Study on the Micro Defect of DGJW40 Steel bonded Carbide Made by a New Process," Rare Metals and Cemented Carbides, no. 1, pp. 22-25, 2000. keywords: {steel bonded hard alloy;micro defect;WC} |