Study on Surface Boronizing Modification of Ti-55531 Alloy with Lamellar Microstructure AITranslate
Abstract AITranslate
The effects of boronizing treatment at different temperatures on the surface microstructure, composition, hardness distribution and residual stress of Ti-55531 lamellar alloy were systematically studied.The results show that the boronized layer of Ti-55531 alloy is composed of three parts: the outer surface layer of bright white product, the transition layer of whisker-like microstructure and the original lamellar matrix.The content of the element B in the boronized layer decreases gradually from the surface to the inside.After boronizing, there is a gradient layer of Ti-B compounds in the surface layer of the alloy, which significantly increases the microhardness of the alloy, and the hardness decreases gradually from the surface layer to the core.Furthermore, the surface of the alloy after boronizing presents a state of residual compressive stress, and its value increases with boronizing temperature increasing.These results of the study can lay a foundation for further study on the effect of boronizing treatment on the wear resistance and fatigue properties of Ti-55531 alloy.
KeyWords AITranslate
1屠振密,朱永明,李宁,胡会利,曹立新.钛及钛合金表面处理技术的应用及发展[J].表面技术,2009,38(6):76-78. 被引量:42
2张卫,解念锁.钛及钛合金的发展与应用研究[J].科技创新导报,2011,8(7):71-71. 被引量:5
3韩杰阁,陈蔚泽,张浩,黄安国.钛合金表面耐磨性能及抗氧化性能的研究现状[J].电焊机,2017,47(3):73-78. 被引量:11
4冷崇燕,张旭,周荣,张荟星,吴先映.Ta离子注入Ti6Al4V合金耐磨性研究[J].稀有金属材料与工程,2008,37(3):556-560. 被引量:19
5蒋昌宇,张罡.TC4钛合金低磷化学镀工艺研究[J].沈阳理工大学学报,2010,29(6):59-62. 被引量:5
6李凤华,王丽娜,衣晓红,樊占国.钛及钛合金渗硼的研究现状与反应机理[J].材料与冶金学报,2013,12(3):212-217. 被引量:10
7付颖,张艳,包星宇,张伟,王福会,辛丽.钛合金表面耐磨涂层研究进展[J].中国腐蚀与防护学报,2018,38(2):117-123. 被引量:17
8魏祥飞,张平则,魏东博,周鹏,张扬,陈小虎,王琼,王若男.多弧离子镀Cr涂层对γ-TiAl合金高温氧化性能的影响[J].稀有金属材料与工程,2014,43(3):707-711. 被引量:8
9姬寿长,李京龙,李争显,杨海彧,畅晨阳,刘林涛.TC21钛合金表面处理技术的研究现状[J].热加工工艺,2021,50(4):17-20. 被引量:4
10潘婷,樊新民,周旸.钛及钛合金渗硼技术的发展[J].热处理,2014,29(2):27-33. 被引量:6
1刘建儒,王战清,马录.一种薄壁滑套的热处理变形控制[J].热处理技术与装备,2022,43(3):18-20.
2李阳,张建伟,朱鹏凯,杨扬.碳含量及冷却速率对钢件淬火残余应力的影响[J].金属热处理,2022,47(6):192-195.
3高钰涵,齐荣钊(指导).月下即景[J].新作文:冰心少年文学,2022(6):46-46.
4韩颢源,杨涛,邱娟,杨刚,余万华,翟月雯,周乐育.固溶处理对TC4合金组织和硬度的影响[J].金属热处理,2022,47(6):93-98. 被引量:3
5芦博昕,杨芳,周洋,陈存广,隋延力,郭志猛.粉末冶金高性能双态组织钛合金的制备[J].稀有金属材料与工程,2022,51(4):1152-1157.
6罗高丽,张凌峰,熊毅,张保丰,陈雪鹏.激光冲击强化对Ti-6Al-3Nb-2Zr-1Mo钛合金组织与性能的影响[J].中国激光,2022,49(8):209-220. 被引量:3
7汤彩碟,张甫生,杨金来,吴良如,郑炯.机械球磨处理对方竹笋全粉理化特性及微观结构的影响[J].食品与发酵工业,2022,48(12):175-182. 被引量:3
8蔡锋,刘曼,徐光.表面高硬度和耐腐蚀性高强贝氏体钢制备新工艺[J].钢铁,2022,57(6):143-149.
9陈正阁,武永丽,薛全喜,熊毅,王淏.激光冲击强化对片层TC11钛合金组织和性能的影响[J].表面技术,2022,51(7):343-352. 被引量:3
10樊永霞,张学哲,贾亮.β热处理对SEBM Ti-6Al-4V Diamond点阵材料显微组织和力学性能的影响[J].钛工业进展,2022,39(3):17-21.
Basic Information:
DOI:
Chinese Library Classification Number:TG166.5[金属学及工艺—热处理]
Citation Information:
The effects of boronizing treatment at different temperatures on the surface microstructure, composition, hardness distribution and residual stress of Ti-55531 lamellar alloy were systematically studied.The results show that the boronized layer of Ti-55531 alloy is composed of three parts: the outer surface layer of bright white product, the transition layer of whisker-like microstructure and the original lamellar matrix.The content of the element B in the boronized layer decreases gradually from the surface to the inside.After boronizing, there is a gradient layer of Ti-B compounds in the surface layer of the alloy, which significantly increases the microhardness of the alloy, and the hardness decreases gradually from the surface layer to the core.Furthermore, the surface of the alloy after boronizing presents a state of residual compressive stress, and its value increases with boronizing temperature increasing.These results of the study can lay a foundation for further study on the effect of boronizing treatment on the wear resistance and fatigue properties of Ti-55531 alloy.
quote
| GB/T 7714-2015 | [1] CHEN Xiao-xiao, HUANG Chao-wen, XU Zi-lu, et al. Study on Surface Boronizing Modification of Ti-55531 Alloy with Lamellar Microstructure[J]. Rare Metals and Cemented Carbides, 2022(3): 65-71. |
| MLA | [1] CHEN Xiao-xiao, et al., "Study on Surface Boronizing Modification of Ti-55531 Alloy with Lamellar Microstructure." Rare Metals and Cemented Carbides, no. 3, 2022, pp. 65-71. |
| APA | [1] CHEN Xiao-xiao, HUANG Chao-wen, XU Zi-lu, XU Qun-li, ZHAO Ai, & SHI Yun-mei. (2022). Study on Surface Boronizing Modification of Ti-55531 Alloy with Lamellar Microstructure. Rare Metals and Cemented Carbides(3), 65-71. |
| IEEE | [1] CHEN Xiao-xiao, HUANG Chao-wen, XU Zi-lu, XU Qun-li, ZHAO Ai, and SHI Yun-mei, "Study on Surface Boronizing Modification of Ti-55531 Alloy with Lamellar Microstructure," Rare Metals and Cemented Carbides, no. 3, pp. 65-71, 2022. keywords: {Ti-55531;titanium alloy;boronizing;heat treatment;microstructure;mechanical property} |