Study on Microstructure and Mechanical Properties of WC-10CoCrFeMnNi High-Entropy Cemented Carbide AITranslate

School of Materials and Energy,Guangdong University of Technology;School of Materials and Energy,Guangdong University of Technology;School of Materials and Energy,Guangdong University of Technology;School of Materials and Energy,Guangdong University of Technology;School of Materials and Energy,Guangdong University of Technology;School of Materials and Energy,Guangdong University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

CoCrFeMnNi high-entropy alloy powder with equal molar ratio was prepared by mechanical alloying,and WC-10CoCrFeMnNi cemented carbide was prepared by spark plasma sintering.The microstructure and properties of high-entropy alloy powder and cemented carbide were studied by X-ray diffractometer,scanning electron microscope,energy dispersive spectrometer,Vickers hardness tester,and laser particle size analyzer.The results show that the nanocrystalline CoCrFeMnNi high-entropy alloy powder,with BCC as the main phase and FCC as the secondary phase,can be obtained by 80 h of ball milling.The ave-rage particle size is 1.4μm,and the particle size distribution is relatively centralized.The cemented carbide,using CoCrFeMnNi high-entropy alloy as the binder phase,exhibits excellent mechanical properties.And the cemented carbide sintered at 1250℃has better comprehensive mechanical properties,with a Vickers hardness of(1452±18.95)HV30and a fracture toughness of(8.57±0.32)MPa·m1/2.

KeyWords AITranslate

cemented carbide high-entropy alloy mechanical alloying spark plasma sintering mechanical property

1羊求民,羊建高,苏伟,陈丽勇,陈颢,郭圣达.纳米/超细晶WC-Co类硬质合金的研究进展[J].稀有金属与硬质合金,2018,46(1):76-83. 被引量:22

2张卫兵,刘向中,陈振华,陈鼎,彭程.WC-Co硬质合金最新进展[J].稀有金属,2015,39(2):178-186. 被引量:67

3徐涛.硬质合金高端产品及新材料发展趋势分析[J].硬质合金,2011,28(6):395-402. 被引量:41

4李萌,弓满锋,张程煜,莫德云,李玫,韩栋,张洪军.超细、纳米晶WC-Co硬质合金烧结技术的研究现状[J].材料导报,2020,34(15):15138-15144. 被引量:11

5潘志君,张恒,刘宁,王颖,韩见.全球钴供应市场结构及定价权分析[J].中国矿业,2017,26(8):18-21. 被引量:15

6周盼龙,肖代红,周鹏飞,余永新,袁珉慧.热压法制备超细晶WC-Al_xCrFeCoNi复合材料及其组织与性能[J].粉末冶金材料科学与工程,2019,24(2):100-105. 被引量:8

1万小虎.钴粉粒度和成分对亚微米晶WC-10Co硬质合金组织和性能的影响[J].稀有金属与硬质合金,2023,51(6):72-77.

2刘岩岩,张鹏,熊德树,张柯.碳纳米管增强硬质合金的制备及性能研究[J].有色金属材料与工程,2024,45(2):9-16.

3黄瑞民,王斌,查春梅,崔艳宏,王伟.ZnO改性石墨烯-镁基复合材料微观组织与性能[J].特种铸造及有色合金,2024,44(3):344-348.

4陈睿铎,崔国栋,陈大志,张程菘.金属粉体材料表面改性技术及应用研究进展[J].钢铁研究学报,2023,35(5):504-520. 被引量:1

5王迪,杨剑.激光散射法测定右美托咪定的粒度分布[J].食品与药品,2024,26(2).

6黄峰,黄维蓉,杨波.黏层用C_(9)石油树脂/SBR复合改性乳化沥青性能研究[J].应用化工,2024,53(3):550-554.

7祁进坤,岳永文,胡剑,王树立,赵钢,寇晓磊,齐国强,赵京辉,任淑彬.EIGA和PREP制备M62轴承钢粉末[J].粉末冶金技术,2024,42(2):144-152.

8张晨沛,杨长江,赵吕兴,李灿,李启坤,常军.碳烟颗粒掺杂铅基复合阳极的制备及电化学性能研究[J].稀有金属材料与工程,2024,53(2):483-489.

Basic Information:

DOI:

Chinese Library Classification Number:TG146.41[金属学及工艺—金属材料]

Citation Information:

CoCrFeMnNi high-entropy alloy powder with equal molar ratio was prepared by mechanical alloying,and WC-10CoCrFeMnNi cemented carbide was prepared by spark plasma sintering.The microstructure and properties of high-entropy alloy powder and cemented carbide were studied by X-ray diffractometer,scanning electron microscope,energy dispersive spectrometer,Vickers hardness tester,and laser particle size analyzer.The results show that the nanocrystalline CoCrFeMnNi high-entropy alloy powder,with BCC as the main phase and FCC as the secondary phase,can be obtained by 80 h of ball milling.The ave-rage particle size is 1.4μm,and the particle size distribution is relatively centralized.The cemented carbide,using CoCrFeMnNi high-entropy alloy as the binder phase,exhibits excellent mechanical properties.And the cemented carbide sintered at 1250℃has better comprehensive mechanical properties,with a Vickers hardness of(1452±18.95)HV30and a fracture toughness of(8.57±0.32)MPa·m1/2.

quote

GB/T 7714-2015 [1] WANG Ke-wei, DONG Yong, ZHAO Zhen-dong, et al. Study on Microstructure and Mechanical Properties of WC-10CoCrFeMnNi High-Entropy Cemented Carbide[J]. Rare Metals and Cemented Carbides, 2024(2): 89-94.
MLA [1] WANG Ke-wei, et al., "Study on Microstructure and Mechanical Properties of WC-10CoCrFeMnNi High-Entropy Cemented Carbide." Rare Metals and Cemented Carbides, no. 2, 2024, pp. 89-94.
APA [1] WANG Ke-wei, DONG Yong, ZHAO Zhen-dong, ZENG Zhuo-jian, HU Yong-jun, & ZHANG Zheng-rong. (2024). Study on Microstructure and Mechanical Properties of WC-10CoCrFeMnNi High-Entropy Cemented Carbide. Rare Metals and Cemented Carbides(2), 89-94.
IEEE [1] WANG Ke-wei, DONG Yong, ZHAO Zhen-dong, ZENG Zhuo-jian, HU Yong-jun, and ZHANG Zheng-rong, "Study on Microstructure and Mechanical Properties of WC-10CoCrFeMnNi High-Entropy Cemented Carbide," Rare Metals and Cemented Carbides, no. 2, pp. 89-94, 2024. keywords: {cemented carbide;high-entropy alloy;mechanical alloying;spark plasma sintering;mechanical property}