Abstract AITranslate

Color-tunable light-emitting diodes (LEDs) offer a broad spectrum of applications, encompassing augmented and virtual reality displays, indoor lighting, and architectural lighting. Achieving high efficiency and brightness, stable emission, and full-color emission is highly desirable in color-tunable LEDs. However, conventional mass transfer processes have made realizing this technology challenging, because they require extracting red, green, and blue LED chips from different epitaxial wafers. In this spotlight article, we review the progress made toward achieving color-tunable LEDs based on rare earth doped wide bandgap Ga2O3 semiconductors. We have systematically studied the structural and optical characteristics of rare earth (Eu, Er, and Tm) doped Ga2O3 films grown by pulsed laser deposition and observed strong emissions in the red, green, and blue spectral regions from Eu, Er, and Tm doped Ga2O3 films, respectively. We have demonstrated the development of red, green, and blue LEDs based on these Eu, Er, and Tm doped Ga2O3 films and achieved color-tunable LEDs using Eu, Er, and Tm codoped Ga2O3 films. These results demonstrate the great potential of rare earth doped Ga2O3 films for use in color-tunable LED applications.

KeyWords AITranslate

wide bandgap gallium oxide rare earth colortunable light emitting diodes
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c00587

Chinese Library Classification Number:

Citation Information:

Color-tunable light-emitting diodes (LEDs) offer a broad spectrum of applications, encompassing augmented and virtual reality displays, indoor lighting, and architectural lighting. Achieving high efficiency and brightness, stable emission, and full-color emission is highly desirable in color-tunable LEDs. However, conventional mass transfer processes have made realizing this technology challenging, because they require extracting red, green, and blue LED chips from different epitaxial wafers. In this spotlight article, we review the progress made toward achieving color-tunable LEDs based on rare earth doped wide bandgap Ga2O3 semiconductors. We have systematically studied the structural and optical characteristics of rare earth (Eu, Er, and Tm) doped Ga2O3 films grown by pulsed laser deposition and observed strong emissions in the red, green, and blue spectral regions from Eu, Er, and Tm doped Ga2O3 films, respectively. We have demonstrated the development of red, green, and blue LEDs based on these Eu, Er, and Tm doped Ga2O3 films and achieved color-tunable LEDs using Eu, Er, and Tm codoped Ga2O3 films. These results demonstrate the great potential of rare earth doped Ga2O3 films for use in color-tunable LED applications.

quote

GB/T 7714-2015 [1] Qixin Guo, Katsuhiko Saito, Tooru Tanaka. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00587.
MLA [1] Qixin Guo, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00587.
APA [1] Qixin Guo, Katsuhiko Saito, & Tooru Tanaka. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00587
IEEE [1] Qixin Guo, Katsuhiko Saito, and Tooru Tanaka, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00587. keywords: {wide bandgap gallium oxide rare earth colortunable light emitting diodes}