Experimental Study on Improvement of Purification Process of Crude Na_2WO_4 Solution AITranslate

Chenzhou Diamond Tungsten Products Co., Ltd.;Chenzhou Diamond Tungsten Products Co., Ltd.;Chenzhou Diamond Tungsten Products Co., Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The traditional magnesium salt purification process is difficult to purify crude sodium tungstate solution with high As content (above 0.2 g/L), so MgSO4-FeCl3 mixed method is put forward to purify the solution. Experimental results show that crude sodium tungstate solution with 0. 240.8 g/L As can be effectively purified by adopting 5 times the theoretical amount of MgSO4 solution at first and then adding 0.5 times the theoretical amount of FeCl3 solution under the conditions of 70℃ and pH9~10.

KeyWords AITranslate

crude Na2WO4 solution with high As purification for As removal MgSO4 FeCI3 mixed method

1和晓才.钨酸钠溶液中除硅、磷、砷工艺[J].云南冶金,2005,34(1):30-32. 被引量:10

2邓天天,李义连,陈锴,武荣华,梁艳燕.FeCl_3絮凝除As效率影响因素的初步研究[J].环境化学,2011,30(2):524-529. 被引量:10

3镫屋三雄,佐藤佑辅,见上宽信,等.含砷物质碱处理方法[P].中国专利:101784489A,2010-07-21.

4E.Krause,聂国林.砷酸铁化合物的溶解度和稳定性[J].湿法冶金,1990(2):21-35. 被引量:16

1翁达,李伟,卢寿慈.粉煤灰残炭吸附-电化学复合法净化印染废水的研究[J].武汉钢铁学院学报,1991,14(4):393-399.

2易津湘.城市污水生物脱氮除磷技术[J].科技创新导报,2008,5(11):4-4. 被引量:4

3张文恒,李广平.含氟废水的处理及氟化盐的回收利用[J].有色冶炼,2002,31(6):32-33. 被引量:1

4洪兆鸣,殷旭东,吴敏华,陈宁.混凝-超声处理垃圾渗滤液研究[J].广东化工,2009,36(5):101-103. 被引量:1

5杨娟.磁电场复合法净化烹饪油烟的研究[J].黑龙江科技信息,2011(34):53-53.

6李龙,姚凤霞.湿法炼锌净液渣综合回收生产实践[J].中国有色冶金,2012,41(5):50-54. 被引量:2

7胡粤辉,凌维靖.废干电池热解物料酸溶及溶液净化试验[J].广州环境科学,2005,20(4):27-29.

8龚川南,张秀,赵秀兰,林于廉,陈玉成.混凝-UV/Fe(Ⅲ)工艺处理高浓度垃圾渗滤液的研究[J].西南大学学报:自然科学版,2015,37(11):151-154.

9孔爱平,王九思,刘剑,姜艳玲,夏德强,王学新.复合絮凝剂聚合氯化铝铁的制备及其对黄河水的絮凝作用[J].石化技术与应用,2008,26(6):574-576. 被引量:13

10涂勇,王小将,封悦科.浅析攀枝花市酸雨污染特征及成因[J].四川环境,2004,23(5):36-39. 被引量:7

Basic Information:

DOI:

Chinese Library Classification Number:X756[环境科学与工程—环境工程]

Citation Information:

The traditional magnesium salt purification process is difficult to purify crude sodium tungstate solution with high As content (above 0.2 g/L), so MgSO4-FeCl3 mixed method is put forward to purify the solution. Experimental results show that crude sodium tungstate solution with 0. 240.8 g/L As can be effectively purified by adopting 5 times the theoretical amount of MgSO4 solution at first and then adding 0.5 times the theoretical amount of FeCl3 solution under the conditions of 70℃ and pH9~10.

quote

GB/T 7714-2015 [1] LONG Yang, ZHANG Yang, LEI Yin-chun. Experimental Study on Improvement of Purification Process of Crude Na_2WO_4 Solution[J]. Rare Metals and Cemented Carbides, 2014(6): 4-7.
MLA [1] LONG Yang, et al., "Experimental Study on Improvement of Purification Process of Crude Na_2WO_4 Solution." Rare Metals and Cemented Carbides, no. 6, 2014, pp. 4-7.
APA [1] LONG Yang, ZHANG Yang, & LEI Yin-chun. (2014). Experimental Study on Improvement of Purification Process of Crude Na_2WO_4 Solution. Rare Metals and Cemented Carbides(6), 4-7.
IEEE [1] LONG Yang, ZHANG Yang, and LEI Yin-chun, "Experimental Study on Improvement of Purification Process of Crude Na_2WO_4 Solution," Rare Metals and Cemented Carbides, no. 6, pp. 4-7, 2014. keywords: {crude Na2WO4 solution with high As;purification for As removal;MgSO4 FeCI3 mixed method}