Oxidative Degradation of Thermosets Based on Thioketal Cleavable Linkages in Aqueous Environment AITranslate

Shenzhen Institute of Advanced Technology; Southern University of Science and Technology;Shenzhen Institute of Advanced Technology; Zagazig University; Southern University of Science and Technology;Shenzhen Institute of Advanced Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Thermosets are rigid, infusible, and unmolded materials containing three-dimensional (3D) cross-linked structures. They are considered a fundamental pillar in the international economy, which are produced by 65 million tons annually. The responsive cross-linking moieties provide the thermosets characterized with outstanding physicochemical properties such as stiffness, degradability, and chemical and thermal resistance. We prepared degradable thermoset materials using thioketal (TK) cross-linkers, which underwent main-chain or side change degradation in the presence of hydrogen peroxide in water. TK cross-linkers at different concentrations (5, 10, and 20% wt %) were polymerized with 2-hydroxyethyl acrylate (HEA) or with 2-hydroxyethyl methacrylate (HEMA) and 1-vinyl-2-pyrrolidone (PD) to produce cross-linked poly(HEA) and poly(HEMA-PD) by free radical polymerization, respectively. The resultant polymer materials completely degraded in hydrogen peroxide/water (3–30%, vol). Using isophorone diisocyanate, we also produced degradable polyurethane based on TK-bearing diol. We prepared a 3D degradable thermoset using the Direct-Ink-Writing (DIW) 3D printing technology, which was charged by diethylene glycol diacrylate (15%, wt %) and a prepolymer (isophorone diisocyanate terminated by acrylate moieties) containing diol-thioketal linkage (15%, wt %). Finally, we found that TK-poly(HEA) underwent microbial degradation by Lactobacillus jensenii at 37 °C, which indicates a benign eco-friendly effect.

KeyWords AITranslate

thermosets thioketal biodegradation hydrogen peroxide polyurethane
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01357

Chinese Library Classification Number:

Citation Information:

Thermosets are rigid, infusible, and unmolded materials containing three-dimensional (3D) cross-linked structures. They are considered a fundamental pillar in the international economy, which are produced by 65 million tons annually. The responsive cross-linking moieties provide the thermosets characterized with outstanding physicochemical properties such as stiffness, degradability, and chemical and thermal resistance. We prepared degradable thermoset materials using thioketal (TK) cross-linkers, which underwent main-chain or side change degradation in the presence of hydrogen peroxide in water. TK cross-linkers at different concentrations (5, 10, and 20% wt %) were polymerized with 2-hydroxyethyl acrylate (HEA) or with 2-hydroxyethyl methacrylate (HEMA) and 1-vinyl-2-pyrrolidone (PD) to produce cross-linked poly(HEA) and poly(HEMA-PD) by free radical polymerization, respectively. The resultant polymer materials completely degraded in hydrogen peroxide/water (3–30%, vol). Using isophorone diisocyanate, we also produced degradable polyurethane based on TK-bearing diol. We prepared a 3D degradable thermoset using the Direct-Ink-Writing (DIW) 3D printing technology, which was charged by diethylene glycol diacrylate (15%, wt %) and a prepolymer (isophorone diisocyanate terminated by acrylate moieties) containing diol-thioketal linkage (15%, wt %). Finally, we found that TK-poly(HEA) underwent microbial degradation by Lactobacillus jensenii at 37 °C, which indicates a benign eco-friendly effect.

quote

GB/T 7714-2015 [1] Mohamed Abdelrahim, Jun Zhang, Quan Gao, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c01357.
MLA [1] Mohamed Abdelrahim, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c01357.
APA [1] Mohamed Abdelrahim, Jun Zhang, Quan Gao, Wael A. Zordok, Ji Liu, & Jin Geng. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c01357
IEEE [1] Mohamed Abdelrahim, Jun Zhang, Quan Gao, Wael A. Zordok, Ji Liu, and Jin Geng, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c01357. keywords: {thermosets;thioketal;biodegradation;hydrogen peroxide;polyurethane}