Vanadium Extraction from Carbonaceous Shale by Microwave Pretreatment and Impurity Removal from its Leaching Solution AITranslate
Abstract AITranslate
Carbonaceous shale from Henan Province was leached with sulfuric acid after pretreated with microwave,and then impurity removal from the leaching solution was carried out.The results show that the leaching rate of vanadium is up to 85% and increases by nearly 15% when carbonaceous shale is heated with microwave for 20 min.The aluminum removing rate can reach 82.31% by adjusting the leaching solution pH to 2.0.The silicon removing rate can reach 84.55% by adding 1.2 times theoretical amount MgCl2 into the leaching solution.
KeyWords AITranslate
1漆明鉴.从石煤中提钒现状及前景[J].湿法冶金,1999,18(4):1-10. 被引量:128
2宾智勇.石煤提钒研究进展与五氧化二钒的市场状况[J].湖南有色金属,2006,22(1):16-20. 被引量:126
3熊卫江,曾清全,梁礼渭.微波在冶金中的应用研究[J].世界有色金属,2010(2):51-53. 被引量:11
4金钦汉.微波化学[M].北京:科学出版社,2001.5.
5鲁兆伶.用酸法从石煤中提取五氧化二钒的试验研究与工业实践[J].湿法冶金,2002,21(4):175-183. 被引量:139
6徐耀兵,王勤辉,施正伦,方梦祥,高翔,骆仲泱.含钒灰渣酸浸液结晶铵明矾的工艺条件[J].过程工程学报,2009,9(5):927-931. 被引量:10
1马红周,王耀宁,燕超,何晓梅,毋海峰.从高冰镍浸出渣中浸出铜[J].湿法冶金,2015,34(6):492-495. 被引量:2
2周嘉郁,张一敏,包申旭,段继华.电容去离子技术分离石煤酸浸液中的钒和铝[J].有色金属:冶炼部分,2016(8):43-47.
3李红湘,颜文斌,蔡俊,华骏,高峰.助浸剂亚硝酸钠对石煤中钒浸出率的影响[J].稀有金属与硬质合金,2019,47(4):13-19. 被引量:7
1李康强,李鑫培,陈晋,和飞,林顺达,郭胜惠,陈菓.微波加热技术在冶金渣资源化利用中的应用[J].矿产保护与利用,2019,39(3):133-139. 被引量:3
2史博洋,王皓莹,刘宇.火试金减杂-电感耦合等离子体原子发射光谱(ICP-AES)法测定高冰镍中的金、银、铂、钯[J].中国无机分析化学,2021,11(4):63-66. 被引量:12
3胡洋,何东升,张琦,张可成,朱志伟.电场强化石煤浸出提钒试验研究[J].金属矿山,2021(9):102-106.
4张卫国,杨建业,李军,李焕同,车晓阳.基于化学浸取法的石煤中稀有金属元素赋存状态[J].煤炭学报,2021,46(10):3255-3267. 被引量:1
5李崇,陈延信,赵博,姚艳飞.石煤提钒及尾渣综合利用研究现状[J].化学世界,2021,62(12):717-725. 被引量:3
6窦向丽,张旺强,黑文龙,殷陶刚.敞开酸溶-电感耦合等离子体发射光谱法测定石煤钒矿中钒铁铝磷[J].岩矿测试,2022,41(4):673-679.
7李崇,陈延信,赵博,酒少武,姚艳飞.助浸剂强化浸出低品位石煤钒矿[J].材料科学与工程学报,2022,40(5):865-871.
8刘东,李峰,阎赞.商洛石煤钒矿的钠化焙烧研究[J].商洛学院学报,2023,37(2):71-75.
9赖永传,杨鑫龙,孙建之,尚鹤,莫晓兰,温建康.石煤含氟酸浸液中V(Ⅴ)-Fe(Ⅲ)-F-H_(2)O系钒铁分离热力学研究[J].中南大学学报:自然科学版,2023,54(5):1703-1712.
1夏李斌,谢法正,王瑞祥.P507-Cyanex272协同萃取分离回收废旧镍氢电池中镍钴金属新工艺研究[J].中国有色冶金,2011,40(1):67-69. 被引量:15
2王彤.黄铜水平连铸渣中的金属回收[J].甘肃冶金,2012,34(6):7-8.
3夏李斌,蔡伟松.废旧镍氢电池浸出液除杂工艺研究[J].有色金属科学与工程,2011,2(1):32-34.
4肖超,肖连生,成宝海,曹佐英.石煤钒矿碱性浸出液提取钒新工艺[J].稀有金属与硬质合金,2011,39(1):4-7. 被引量:10
5聂荣辉,高亚瑞,齐欣.探究铝电解用炭阳极的综合性能[J].科技风,2013(16):189-189. 被引量:1
6稀土二钼酸铵制备工艺[J].中国钼业,2007,31(3):22-22.
7唐秋香,唐有根,缪新.从熟化石煤水浸液中溶剂萃取——沉淀钒[J].湿法冶金,2014,33(6):457-459. 被引量:2
8陈斌,李小斌,陈谦德.拜耳法赤泥的湿法处理——从高苛性比铝酸钠溶液中回收氧化铝[J].稀有金属与硬质合金,1993,21(S1):425-428.
9朱金勇,杨巧芳,闫晓军,娄世斌.拜尔法种分母液沉铝试验研究[J].矿冶工程,2002,22(4):64-65. 被引量:3
10张曦,邹晓勇.含钒液体除硅过程的研究[J].金属材料与冶金工程,2007,35(6):19-22.
Basic Information:
DOI:
Chinese Library Classification Number:TF841.3[冶金工程—有色金属冶金]
Citation Information:
Carbonaceous shale from Henan Province was leached with sulfuric acid after pretreated with microwave,and then impurity removal from the leaching solution was carried out.The results show that the leaching rate of vanadium is up to 85% and increases by nearly 15% when carbonaceous shale is heated with microwave for 20 min.The aluminum removing rate can reach 82.31% by adjusting the leaching solution pH to 2.0.The silicon removing rate can reach 84.55% by adding 1.2 times theoretical amount MgCl2 into the leaching solution.
quote
| GB/T 7714-2015 | [1] CHEN Hui, ZHANG Yan-yan, LI Jian-wen, et al. Vanadium Extraction from Carbonaceous Shale by Microwave Pretreatment and Impurity Removal from its Leaching Solution[J]. Rare Metals and Cemented Carbides, 2011(2): 1-5. |
| MLA | [1] CHEN Hui, et al., "Vanadium Extraction from Carbonaceous Shale by Microwave Pretreatment and Impurity Removal from its Leaching Solution." Rare Metals and Cemented Carbides, no. 2, 2011, pp. 1-5. |
| APA | [1] CHEN Hui, ZHANG Yan-yan, LI Jian-wen, & SI Shi-hui. (2011). Vanadium Extraction from Carbonaceous Shale by Microwave Pretreatment and Impurity Removal from its Leaching Solution. Rare Metals and Cemented Carbides(2), 1-5. |
| IEEE | [1] CHEN Hui, ZHANG Yan-yan, LI Jian-wen, and SI Shi-hui, "Vanadium Extraction from Carbonaceous Shale by Microwave Pretreatment and Impurity Removal from its Leaching Solution," Rare Metals and Cemented Carbides, no. 2, pp. 1-5, 2011. keywords: {vanadium extraction;carbonaceous shale;microwave pretreatment;sulfuric acid leaching;impurity removal} |